journal article·2025-09Open access

Superior stress relaxation resistance of 2.2 GPa martensitic steels and the effect of vanadium

Siming Huang, Jianping Ouyang, Liejun Li, Songjun Chen, Xianqiang Xing, Zhuoran Li, Haixiao Ye, Zhengwu Peng, Zhichao Luo

Abstract

For ultra-high-strength steels subjected to sustained loading, stress relaxation resistance is a core indicator determining their long-term service reliability. This work investigates the stress relaxation behaviors of two 2.2 GPa-grade martensitic steels (with and without V addition). Both steels were fabricated by flash heating and tempering treatments and exhibited high density dislocations in ultrafine-grained microstructure. Stress-relaxation testing results across various temperatures demonstrate superior relaxation resistance for these two steels. The thermal activation energy (ΔG 0 ) of dislocations at an extremely high stress of 1750 MPa of V-free and V-alloyed steel is 11.8 eV and 14.8 eV, respectively. The synergistic combination of high mechanical strength and stress relaxation resistance in the present martensitic steels is superior to that of other metallic materials reported in previous studies. Furthermore, the higher activation energy and relaxation resistance of V-alloyed steel is primarily associated with the increased density of dislocation obstacles from grain boundaries and nanoprecipitates.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Microstructure and Mechanical Properties of Steels · Hydrogen embrittlement and corrosion behaviors in metals · Metal Alloys Wear and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (45)

Show source-provided references
1. Chemical boundary engineering: a new route toward lean, ultrastrong yet ductile steels10.1126/sciadv.aay1430 ↗
2. High dislocation density-induced large ductility in deformed and partitioned steels10.1126/science.aan0177 ↗
3. Ductile 2-GPa steels with hierarchical substructure10.1126/science.add7857 ↗
4. Size and stress dependences in the tensile stress relaxation of thin copper wires at room temperature10.1016/j.ijplas.2018.09.001 ↗
5. Strength, strain-rate sensitivity and ductility of copper with nanoscale twins10.1016/j.actamat.2006.06.062 ↗
6. Tempering stress relaxation behavior and microstructure evolution of 300 M steel10.1016/j.matchar.2023.112688 ↗
7. Analysis of strain hardening behavior of a high-Mn TWIP steel using electron microscopy and cyclic stress relaxation
8. Activation of different twinning mechanisms and their contributions to mechanical behavior of a face-centered cubic Co-based high-entropy alloy
9. Time, stress, and temperature-dependent deformation in nanostructured copper: stress relaxation tests and simulations10.1016/j.actamat.2016.02.021 ↗
10. High temperature stress relaxation behavior of high Si, Mo-doped austenitic stainless steels10.1016/j.msea.2024.147330 ↗
11. Mechanism of Cr enhancement on stress relaxation resistance in Cu–Ni–Co–Si–Mg alloys
12. Strength-ductility-toughness balance in flash-tempered martensitic steel: role of dislocation-precipitate interactions10.1016/j.matchar.2025.114847 ↗
13. Kinetic transitions and Mn partitioning during austenite growth from a mixture of partitioned cementite and ferrite: role of heating rate10.1016/j.jmst.2020.01.051 ↗
14. Abnormal expansion during the ferro-to para-magnetic transition in pure iron10.1016/j.jmmm.2014.10.092 ↗
15. Effect of vanadium microalloying on phase transformation and strengthening mechanism of 1000 MPa low carbon bainitic steel10.1016/j.msea.2023.145578 ↗
16. Strengthening mechanisms of Nb and V microalloying high strength hot-stamped steel10.1016/j.msea.2020.140115 ↗
17. Harjo · 2011 · 443
18. Dual nanoprecipitation and nanoscale chemical heterogeneity in a secondary hardening steel for ultrahigh strength and large uniform elongation10.1016/j.jmst.2023.10.048 ↗
19. Formation of eta carbide in ferrous martensite by room temperature aging10.1016/j.actamat.2018.07.071 ↗
20. Strength improvement over 2 GPa and austenite grain ultra-refinement in a low carbon martensite steel achieved by ultra-rapid heating and quenching10.1016/j.msea.2023.145538 ↗
21. Tempering of lath martensite in low and medium carbon steels: assessment and challenges10.1002/srin.201700038 ↗
22. Dislocations, grain size and planar faults in nanostructured copper determined by high resolution X-ray diffraction and a new procedure of peak profile analysis10.1016/S1359-6454(98)00001-9 ↗
23. Strain rate dependence of strengthening mechanisms in ultrahigh strength lath martensite10.1016/j.ijplas.2022.103495 ↗
24. The effect of dislocation contrast on x-ray line broadening: a new approach to line profile analysis10.1063/1.117951 ↗
25. The contrast factors of dislocations in cubic crystals: the dislocation model of strain anisotropy in practice10.1107/S0021889899009334 ↗
26. Work hardening, dislocation structure, and load partitioning in lath martensite determined by in situ neutron diffraction line profile analysis10.1007/s11661-017-4172-0 ↗
27. Improving the ductility of ultrahigh strength lath martensite through heterogeneous carbon distribution10.1016/j.jmrt.2023.11.229 ↗
28. X-ray diffraction peak profile analysis aiming at better understanding of the deformation process and deformed structure of a martensitic steel10.1016/j.tsf.2008.04.019 ↗
29. Comparison of the dislocation density in martensitic steels evaluated by some X-ray diffraction methods10.2355/isijinternational.50.875 ↗
30. Optimising the strength-ductility-toughness combination in ultra-high strength quenching and partitioning steels by tailoring martensite matrix and retained austenite10.1016/j.ijplas.2020.102851 ↗
31. Modelling strength and ductility of ultrafine grained BCC and FCC alloys using irreversible thermodynamics10.1179/174328408X353750 ↗
32. Achieving springback-free age forming via dislocation-enhanced stress relaxation in Al alloy10.1016/j.jmst.2024.11.011 ↗
33. A low-alloy high-carbon martensite steel with 2.6 GPa tensile strength and good ductility10.1016/j.actamat.2018.07.060 ↗
34. Optimizing dislocation strengthening in high-strength medium-carbon steel via fast induction heating quenching & tempering10.1016/j.jmrt.2023.05.260 ↗
35. Stress relaxation in crystals10.1002/pssb.2220930102 ↗
36. Temperature-dependent strain rate sensitivity and activation volume of nanocrystalline Ni10.1016/j.actamat.2006.02.013 ↗
37. Stress relaxation and the structure size-dependence of plastic deformation in nanotwinned copper10.1016/j.actamat.2009.07.018 ↗
38. Stress relaxation, internal stress, and work hardening in some bcc metals and alloys10.1007/BF02643451 ↗
39. Activation processes of stress relaxation during hold time in 1Cr–Mo–V steel10.1016/S0921-5093(98)01086-7 ↗
40. The influence of temperature and strain rate on the flow stress of α-iron single crystals10.1080/14786436208212178 ↗
41. Deformation mechanism transition caused by strain rate in a pulse electric brush-plated nanocrystalline Cu10.1063/1.2973200 ↗
42. Thermal activation under shear10.1080/01418610108214448 ↗
43. Direct observation of individual dislocation interaction processes with grain boundaries10.1126/sciadv.1501926 ↗
44. A high-entropy alloy with dislocation-precipitate skeleton for ultrastrength and ductility10.1016/j.actamat.2022.117975 ↗
45. Unraveling the effects of strain‒induced precipitation on continuous cooling ferrite transformation in titanium‒molybdenum microalloyed steel10.1016/j.jmrt.2024.09.130 ↗