Microstructural characteristics and wear resistance of nano-sized TiC reinforced Ti6Al4V composites fabricated by selective laser melting
Source abstract
Abstract
In this study, TiC/Ti6Al4V composites with varying TiC contents (0 wt%, 1 wt%, 3 wt%, and 10 wt%) were fabricated via selective laser melting. Post-build annealing was performed immediately after the SLM process. The microstructure of the annealed composites was characterized, and reciprocating sliding friction tests were conducted to evaluate the tribological behavior under different loads (2 N, 10 N, 20 N, 30 N and 50 N) at room temperature. The results showed that the relative density of the composites decreases with increasing TiC content at a given energy density. The initially incorporated nano-sized TiC particles melted and were subsequently synthesized in situ during the SLM process. The solidification pathway and phase formation are influenced by the initial TiC content, resulting in distinct microstructural characteristics. For the 1 wt% TiC composite, there is no eutectic reaction occurs during the solidification process. The composition of the 3 wt% and 10 wt% composites placed them within the hypereutectic region, and both the primary and eutecticed TiC phase formed during solidification. The addition of TiC also resulted in a reduction in both the width and length of α laths, accompanied by an increase in the amount of irregularly blocky α phase. The average friction coefficient exhibited a non-monotonic trend with increasing load for a given TiC content, initially decreasing before rising again. The addition of nano-sized TiC particles did not lead to a discernible improvement in the wear resistance of the SLM-ed Ti6Al4V alloy, and even leads to deterioration in wear resistance under some test conditions.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Titanium Alloys Microstructure and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (39)
Show source-provided references
1. Material-structure-performance integrated laser-metal additive manufacturing10.1126/science.abg1487 ↗
2. Additive manufacturing modification by artificial intelligence, machine learning, and deep learning: a review
3. On the current research progress of metallic materials fabricated by laser powder bed fusion process: a review10.1016/j.jmrt.2022.07.085 ↗
4. Enhancing geometric integrity and surface hardness of SLM-printed Ti-6Al-4V components with support structures and laser nitriding10.1016/j.surfcoat.2024.131378 ↗
5. Strength-ductility synergy of selective laser melted Al-Mg-Sc-Zr alloy with a heterogeneous grain structure
6. Effect of heat treatment on microstructure evolution and mechanical properties of selective laser melted inconel 718 alloy10.1007/s11665-019-04309-3 ↗
7. Texture control of 316L parts by modulation of the melt pool morphology in selective laser melting10.1016/j.jmatprotec.2018.08.049 ↗
8. Study of the microstructure and mechanical properties of Cu-Sn alloys formed by selective laser melting with different Sn contents10.1016/j.jmrt.2023.04.198 ↗
9. Selective laser melting of aluminum and titanium matrix composites: recent progress and potential applications in the aerospace industry10.3390/aerospace7060077 ↗
10. Effect of powder particle shape on the properties of in situ Ti–TiB composite materials produced by selective laser melting10.1016/j.jmst.2015.08.007 ↗
11. Influence of laser power on microstructure and performance of SiC/Ti composite fabricated through selective laser melting10.1016/j.jmrt.2024.12.044 ↗
12. Investigation on the microstructure, room and high temperature mechanical behaviors and strengthening mechanisms of the (TiB+TiC)/TC4 composites10.1016/j.jallcom.2017.08.017 ↗
13. Duplex strengthening via SiC addition and in-situ precipitation in additively manufactured composite materials10.1016/j.compositesb.2022.109820 ↗
14. Interfacial structure and wear properties of selective laser melted Ti/(TiC+TiN) composites with high content of reinforcements10.1016/j.jallcom.2021.159436 ↗
15. Parameters and microstructure evolution of TiC/TC4 composites formed by selective laser melting
16. Microstructure evolution and strengthening mechanism of TiC/Ti6Al4V composites fabricated by selective laser melting during isothermal deformation10.1080/17452759.2024.2374466 ↗
17. Comparative study on process-structure-property relationships of TiC/Ti6Al4V and Ti6Al4V by selective laser melting10.1016/j.ijmecsci.2022.107963 ↗
18. In situ TiC reinforced Ti6Al4V matrix composites manufactured via selective laser melting10.1108/RPJ-01-2023-0027 ↗
19. Effect of in situ synthesis TiC on the microstructure of graphene/Ti6Al4V composite fabricated by selective laser melting10.1016/j.matlet.2021.130715 ↗
20. Nanocrystalline TiC reinforced Ti matrix bulk-form nanocomposites by selective Laser Melting (SLM): densification, growth mechanism and wear behavior10.1016/j.compscitech.2011.07.010 ↗
21. Microstructural evolution, mechanical and tribological properties of TiC/Ti6Al4V composites with unique microstructure prepared by SLM10.1016/j.msea.2021.141187 ↗
22. Selective laser melting of TiC/Ti bulk nanocomposites: influence of nanoscale reinforcement10.1016/j.scriptamat.2012.04.013 ↗
23. An overview of residual stresses in metal powder bed fusion
24. Research progress on microstructure, defects, surface and configuration of additive manufactured typical aviation metals
25. Effect of heat treatment on the corrosion resistance behavior of selective laser melted Ti6Al4V ELI10.1016/j.surfcoat.2020.125955 ↗
26. Corrosion and tensile behaviors of Ti-4Al-2V-1Mo-1Fe and Ti-6Al-4V titanium alloys10.3390/met9111213 ↗
27. Microstructure and mechanical properties of in situ casting TiC/Ti6Al4V composites through adding multi-walled carbon nanotubes10.1016/j.jallcom.2015.03.044 ↗
28. Numerical simulation of temperature distribution and TiC growth kinetics for high power laser clad TiC/NiCrBSiC composite coatings10.1016/j.optlastec.2011.09.030 ↗
29. Effect of TiC particle size on the microstructure and tensile properties of TiCp/Ti6Al4V composites fabricated by laser melting deposition10.1016/j.optlastec.2018.03.009 ↗
30. Microstructure and mechanical properties of functionally graded TiCp/Ti6Al4V composite fabricated by laser melting deposition10.1016/j.ceramint.2017.09.054 ↗
31. Microstructure and tensile properties of TiCp/Ti6Al4V composites by laser melting deposition with different dissolving degrees of TiC10.1016/j.ceramint.2022.08.052 ↗
32. Study on microstructure and tribological properties of nano/micron TiC/TC4 composites fabricated by laser melting deposition10.1016/j.jmapro.2022.07.068 ↗
33. The friction and wear behaviour of in-situ titanium carbide reinforced composite layers manufactured on ductile cast iron by laser surface alloying10.1016/j.surfcoat.2020.126634 ↗
34. Microstructure and properties of (diamond+TiC) reinforced Ti6Al4V titanium matrix composites manufactured by directed energy deposition10.1016/j.jmrt.2023.12.227 ↗
35. Laser metal deposition of functionally graded Ti6Al4V/TiC10.1016/j.matdes.2015.06.135 ↗
36. Wear behavior of alumina abrasive belt and its effect on surface integrity of titanium alloy during conventional and creep-feed grinding
37. Investigation of friction and wear behavior of titanium alloy-diamond based on the morphology evolution of single abrasive clusters
38. Microstructure and mechanical properties of (TiB+TiC)/Ti composites fabricated in situ via selective laser melting of Ti and B4C powders
39. Microstructure and friction/wear behavior of (TiB + TiC) particulate-reinforced titanium matrix composites10.1016/j.wear.2014.05.013 ↗