Effect of pulsed current-assisted CMT welding parameters on friction and wear properties and electrochemical corrosion performance of heterogeneous structure composites

Tianlong Gao, Can Peng, Rongtao Zhu, Chuang Li, Longhan Duan, Hawke Suen, Bo Yuan, Liang Zhang, Zhiwen Xie

Abstract

The interfacial integrity of Babbitt alloy bushings is critical to the service life of sliding bearings operating under extreme conditions, including cyclic shock loads, seawater ingress, and prolonged boundary lubrication. Conventional bonding techniques often result in interfacial voids and thermal stress cracking, limiting performance. To address these issues, a novel joining process combining low-heat-input cold metal transfer (CMT) with pulsed current has been developed for Babbitt alloy bushings. The pulsed current generates electromagnetic forces (Lorentz force) that stir the molten pool, promoting heterogeneous nucleation, refining grain structure, and reducing defects. Reflecting real-world bearing applications, this study focuses on the friction-wear performance and localized corrosion behavior in a simulated marine environment at 30 °C / 168 hours. The results demonstrate that pulse-assisted CMT welding parameters significantly influence the tribological and electrochemical properties of the Babbitt alloy. The sample produced with 10-pulse series exhibited the lowest friction coefficient (0.27) and the lowest wear rate (2.95×10 -6 mm 3 /(N·m)). Meanwhile, the 13-pulse sample showed superior corrosion resistance, presenting the highest electrochemical impedance, the most positive self-corrosion potential, and the lowest corrosion rate (1.96×10 -7 A·cm -2 ). This work provides metallurgical strategies aimed at improving the reliability of next-generation offshore wind turbine bearings.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced machining processes and optimization · Advanced materials and composites · Metal Alloys Wear and Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (51)

Show source-provided references
1. Developments in internal combustion engines and implications for combustion science and future transport fuels10.1016/j.proci.2014.10.002 ↗
2. Failure analysis of a wear ring impeller10.1016/j.engfailanal.2022.106415 ↗
3. Lifetime extension of offshore support structures of wind turbines: a review10.1016/j.rser.2025.115788 ↗
4. Ultrasonic nanocrystal surface modification of CuSn12Ni2 alloy and its tribological behavior under starved oil lubrication10.1016/j.jallcom.2025.181284 ↗
5. Direct elimination of Fe-oxides assists the preparation of Cu/1010 steel bimetal laminated composites with oxides-free interface10.1016/j.matchar.2025.115386 ↗
6. Interfacial microstructure and hardness of Sn-Based Babbitt/C93700 cu-pb-sn bimetallic materials
7. High-strength and wear-resistant Babbitt alloy coatings prepared through in-situ alloying10.1016/j.surfcoat.2024.131416 ↗
8. Effect of surface modification on friction characteristics of sliding bearings: a review10.1016/j.triboint.2022.107937 ↗
9. Experimental and simulation study of Babbitt Alloy/Steel composite in swing Cold Metal Transfer (CMT) welding under different heat input10.1007/s11837-024-06424-6 ↗
10. Advancements in corrosion studies and protective measures for copper and copper-based alloys in varied environmental conditions10.1016/j.rineng.2025.105257 ↗
11. Enhancing tribological properties via double-pass friction stir processing of novel Mg-Y-Nd-Zr/Ti/Al/Sn metal matrix composite
12. Differentiated SnSb grain size distribution for improved tribological properties of Babbitt alloy10.1108/ILT-09-2022-0259 ↗
13. Wear behavior of graphite self-lubricating Babbitt alloy composite coating on 20 steel prepared by laser cladding10.1016/j.engfailanal.2022.106698 ↗
14. High performance tin-based Babbitt coatings deposited by high-pressure cold spraying10.1016/j.surfcoat.2023.130048 ↗
15. Investigating the effect of PWHT on microstructural features and fatigue crack growth behavior of friction stir welded AA2024-T6 aluminum alloy joints10.1016/j.finmec.2022.100107 ↗
16. Evaluation of nickel shot peening process on strength of friction stir welded AA2014-T6 aluminum alloy joints
17. Mechanisms of fatigue crack initiation and propagation in 6005A CMT welded joint10.1016/j.jallcom.2017.12.374 ↗
18. CMT welding-brazing of al/steel dissimilar materials using cycle-step mode10.1016/j.jmrt.2022.03.043 ↗
19. Effect of Swing-CMT welding parameters on friction and wear properties and electrochemical corrosion performance of Babbitt alloy ZChSnSb11-610.1016/j.jmrt.2025.02.097 ↗
20. Influence of arc mode on the microstructure and mechanical properties of 5356 aluminum alloy fabricated by wire arc additive manufacturing10.1016/j.jmrt.2022.08.005 ↗
21. Pulse profile and metal transfer in pulsed gas metal arc welding: droplet formation, detachment and velocity10.1080/13621718.2017.1288889 ↗
22. Microstructure evolution and strengthening mechanism of pulsed current diffusion bonding TiAl/Ti2AlNb joints with in-situ rapid hot deformation10.1016/j.jmatprotec.2024.118515 ↗
23. Effect of pulse frequency on the microstructure and corrosion behavior of Ti-6Al-4V alloy fabricated by pulse arc remelting method10.1016/j.surfcoat.2025.132159 ↗
24. Effect of pulse current treatment on interface structure and mechanical behavior of TA1/304 clad plates10.1016/j.msea.2022.143583 ↗
25. Microscopic characteristics and properties of co-based coating by pulse current-assisted laser cladding on high carbon steel10.1016/j.surfcoat.2024.131367 ↗
26. Insight into microstructure evolution and mechanical properties of 5 wt% SiC/Al composites by high frequency pulse current treatment10.1016/j.vacuum.2023.112262 ↗
27. The study of grain transport effects on grain refinement under pulsed magnetic fields
28. A review on distortion and residual stress in additive manufacturing
29. Investigation of tribological behavior and failure mechanisms of PEEK-based composites, Babbitt alloy, and CuSn10Pb10 bimetal for wind turbine main shaft sliding bearings under simulated operational conditions10.1016/j.triboint.2025.110522 ↗
30. Friction stir welding parameters optimization for tailored welded blank sheets of AA1100 with AA6061 dissimilar alloy using response surface methodology
31. Effects of Ag micro-addition on structure and mechanical properties of Sn-11Sb-6Cu Babbitt10.1016/j.msea.2018.03.034 ↗
32. Microstructure and mechanical properties of TiC reinforced TZM composites prepared by spark plasma sintering10.1016/j.ijrmhm.2023.106345 ↗
33. Steel shot peening effects on friction stir welded AA2014-T6 aluminum alloys10.1515/mt-2021-2173 ↗
34. Adhesion transfer in sliding a steel ball against an aluminum alloy10.1016/j.triboint.2017.05.039 ↗
35. Effects of WC particles on microstructure and mechanical properties of 316L steel obtained by laser melting deposition10.1016/j.ceramint.2022.03.324 ↗
36. On the localized corrosion of AA5083 in a simulated dynamic seawater/air interface—Part 3: effects of sensitization10.1016/j.corsci.2024.111821 ↗
37. Analytical transfer function for the blocked-diffusion warburg impedance with frequency dispersion. Simulation of the impedance spectrum and voltage response of a lithium-ion battery10.1016/j.fub.2025.100051 ↗
38. The genesis of friction10.1016/0043-1648(81)90315-X ↗
39. Microstructure evolution and underlying thermal behavior of high-content TiC reinforced titanium matrix composites fabricated by laser directed energy deposition10.1016/j.jmrt.2023.01.226 ↗
40. Effect of deposition current on microstructure and tribological properties of tin-based Babbitt alloy on magnesium alloy deposited by TIG process10.1016/j.surfcoat.2024.131702 ↗
41. Correction to: effect of heat treatment on the structure and properties of laser welded joints of Aluminum alloy AA2024
42. Wear reducing effects and temperature dependence of tribolayer formation in harsh environment10.1016/j.triboint.2013.03.003 ↗
43. Selective laser melting of WC reinforced maraging steel 300: microstructure characterization and tribological performance10.1016/j.surfcoat.2018.11.033 ↗
44. Fracture toughness and wear resistance of heat-treated H13 tool steel processed by laser powder bed fusion
45. Achieving excellent corrosion resistance properties of 7075 Al alloy via ultrasonic surface rolling treatment10.1016/j.jallcom.2022.165009 ↗
46. Three-dimensional Sn rich Cu6Sn5 negative electrodes for Li ion batteries10.1016/j.ijhydene.2016.03.097 ↗
47. Electrochemical corrosion behavior of nanocrystalline Materials—A review10.1016/S1005-0302(10)60001-1 ↗
48. Microstructure, corrosion behaviour and microhardness of a directionally solidified Sn–Cu solder alloy10.1016/j.electacta.2011.07.114 ↗
49. Electrochemical behavior of a lead-free Sn–Cu solder alloy in NaCl solution10.1016/j.corsci.2013.11.010 ↗
50. On the localized corrosion of AA5083 in a simulated dynamic seawater/air interface—Part 1: corrosion initiation mechanism10.1016/j.corsci.2023.110985 ↗
51. Revealing the relationship between grain size and corrosion rate of metals10.1016/j.scriptamat.2010.08.035 ↗