In situ thermal monitoring optimizes AFSD preheating: Feed strategy controls heat transfer, microstructure, and mechanical properties
Source abstract
Abstract
This study reports the first application of a self-developed in-situ monitoring device to record interfacial thermal profiles during the preheating stage of additive friction stir deposition (AFSD). By combining finite element modeling with experimental validation, the work establishes a quantitative link between feed length, heat generation, and thermal distribution. Based on this understanding, three preheating strategies were designed and compared. Results show that the preheating process evolves through three characteristic stages driven by interfacial friction, and that heat output increases linearly with feed length. Among the evaluated strategies, the stepped growth (SG) approach promoted effective recrystallization and dislocation strengthening, leading to higher hardness and strength while reducing variations between preheating and steady-state regions. These findings provide mechanistic insight into AFSD preheating and suggest a practical route to improve the consistency of multilayer additive manufacturing.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Advanced Welding Techniques Analysis · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (70)
Show source-provided references
1. Friction surface cladding: an exploratory study of a new solid state cladding process10.1016/j.jmatprotec.2015.10.029 ↗
2. Relationship between grain structure evolution and tensile anisotropy in al-zn-mg-cu cylindrical part formed by additive friction stir deposition10.1016/j.msea.2024.147423 ↗
3. Interface stair-like design and repair performance of al-zn-mg-cu aluminum alloy based on additive friction stir deposition10.1016/j.jmatprotec.2025.118758 ↗
4. Additive friction stir deposition: a deformation processing route to metal additive manufacturing10.1080/21663831.2020.1847211 ↗
5. Friction stir additive manufacturing for high structural performance through microstructural control in an Mg based WE43 alloy10.1016/j.matdes.2014.09.082 ↗
6. Potential and challenges for large-scale near-net-shaping of 7xxx aerospace grade aluminum via additive friction stir deposition
7. In situ investigation into temperature evolution and heat generation during additive friction stir deposition: a comparative study of Cu and al-mg-si
8. Effect of rotational speed and feed rate on microstructure and mechanical properties of 6061 aluminum alloy manufactured by additive friction stir deposition10.1007/s00170-023-11527-6 ↗
9. In-situ monitoring of additive friction stir deposition of AA6061: effect of layer thickness on the microstructure and mechanical properties
10. The effect of heat treatment on the microstructure and electrochemical corrosion behavior of multilayer AA6061 alloy fabricated by additive friction stir deposition10.1016/j.apsusc.2023.159167 ↗
11. The effect of solutionizing and artificial aging on the microstructure and mechanical properties in solid-state additive manufacturing of precipitation hardened Al–Mg–Si alloy10.1016/j.msea.2021.141351 ↗
12. Effects on microstructure and mechanical properties of aluminum alloy 6061 processed via underwater additive friction stir deposition10.1016/j.jmapro.2025.01.006 ↗
13. Heterogeneous microstructure development in additive friction-stir deposited al-mg-si alloy
14. Investigating multi-scale heterogeneity in multi-layer additive friction stir deposition of high-strength aluminum alloys10.1016/j.msea.2025.147979 ↗
15. Influence of preheating temperature on the microstructure and mechanical properties of 6061/TA1 composite plates fabricated by AFSD10.3390/ma16176018 ↗
16. Effect of pre-heating on residual stresses and deformation in laser-based directed energy deposition repair: a comparative analysis10.3390/ma17102179 ↗
17. Experimental and numerical investigation in directed energy deposition for component repair10.3390/ma14061409 ↗
18. A pathway towards strengthening and ductilization of additive-manufactured AlSi10Mg through friction stir processing: microstructural evolution and tensile behavior10.1016/j.msea.2024.146367 ↗
19. Enhancing microstructure and mechanical properties of laser powder bed fusion-fabricated AlSi10Mg alloy through tailored friction stir processing and post-heat treatment
20. Overcoming the strength-ductility trade-off in additive manufactured AlSi10Mg plates by friction stir welding at a low rotational speed10.1016/j.jmrt.2023.03.109 ↗
21. Multipass friction stir processing of laser-powder bed fusion AlSi10Mg: microstructure and mechanical properties10.3390/ma16041559 ↗
22. Grain structure formation and texture modification through multi-pass friction stir processing in AlSi10Mg alloy produced by laser powder bed fusion
23. Numerical and experimental study on the thermal process during additive friction stir deposition10.1016/j.cirpj.2023.12.002 ↗
24. A pseudo thermo-mechanical model linking process parameters to microstructural evolution in multilayer additive friction stir deposition of magnesium alloy10.1016/j.matdes.2022.111412 ↗
25. Numerical studies on controlling of process parameters in friction stir welding10.1016/j.jmatprotec.2008.01.044 ↗
26. Observations of the mechanical response and evolution of damage of AA 6061-T6 under different strain rates and temperatures10.1016/j.msea.2014.11.074 ↗
27. Material flow path and extreme thermomechanical processing history during additive friction stir deposition10.1016/j.jmapro.2023.05.095 ↗
28. Thermal prediction of additive friction stir deposition through Bayesian learning- enabled explainable artificial intelligence10.1016/j.jmsy.2023.10.015 ↗
29. Influence of particulate reinforcements on 6061 materials in extrusion modeling10.1016/j.msea.2003.08.006 ↗
30. A pseudo thermo-mechanical model linking process parameters to microstructural evolution in multilayer additive friction stir deposition of magnesium alloy10.1016/j.matdes.2022.111412 ↗
31. Numerical modelling of 3D plastic flow and heat transfer during friction stir welding of stainless steel10.1179/174329306X107692 ↗
32. Experimental and Numerical Study on Friction and Wear Performance of Hot Extrusion Die Materials10.3390/ma15051798 ↗
33. Thermal energy generation and distribution in friction stir welding of aluminum alloys10.1016/j.energy.2014.09.045 ↗
34. Experimental validation of an FSW model with an enhanced friction law: application to a threaded cylindrical pin tool10.3390/met7110491 ↗
35. Fully coupled thermomechanical simulation of friction stir welding of aluminum 6061-T6 alloy T-joint10.1016/j.jmapro.2019.06.030 ↗
36. Experimental investigation of mechanical properties of aluminum alloy at high and low temperatures10.1061/(ASCE)MT.1943-5533.0003002 ↗
37. Tracing plastic deformation path and concurrent grain refinement during additive friction stir deposition10.1016/j.mtla.2021.101159 ↗
38. Microstructures, tensile properties, and strengthening mechanisms of novel Al-Mg alloys with high Mg content10.1016/j.jallcom.2023.169866 ↗
39. In-situ monitoring of additive friction stir deposition of AA6061: effect of rotation speed on the microstructure and mechanical properties10.1016/j.msea.2024.146620 ↗
40. Effect of thermomechanical processing on fatigue behavior in solid-state additive manufacturing of Al-Mg-Si alloy10.3390/met10070947 ↗
41. Evaluation of solute clusters associated with bake-hardening response in isothermal aged al-mg-si alloys using a three-dimensional atom probe10.1007/s11661-014-2548-y ↗
42. The precipitation sequence in Al–Mg–Si alloys10.1016/S1359-6454(98)00059-7 ↗
43. Microstructure evolution of Al6061 alloy made by additive friction stir deposition10.3390/ma15103676 ↗
44. Influence of silicon carbide particulate reinforcement on quasi static and cyclic fatigue fracture behavior of 6061 aluminum alloy composites10.1016/S0921-5093(01)01444-7 ↗
45. Microstructure evolution and recrystallization behavior of hot rolled AA6061 twin-roll casting plate with different manganese contents10.1016/j.jallcom.2022.165618 ↗
46. Development of elastoplastic-damage model of AlFeSi phase for aluminum alloy 606110.3390/met11060954 ↗
47. Preparation of millimeter scale second phase particles in aluminum alloys and determination of their mechanical properties10.1016/j.jallcom.2018.12.395 ↗
48. Influence of texture and grain refinement on the mechanical behavior of AA2219 fabricated by high shear solid state material deposition10.1016/j.msea.2018.03.088 ↗
49. Evaluation of microstructure and mechanical properties of al-zn-mg-cu alloy repaired via additive friction stir deposition10.1115/1.4052816 ↗
50. Electrochemical corrosion behavior of 6061 Al alloy under high rotating speed submerged friction stir processing10.1016/j.corsci.2023.111029 ↗
51. Friction stir welding/processing of metals and alloys: a comprehensive review on microstructural evolution10.1016/j.pmatsci.2020.100752 ↗
52. Age-hardening characteristics of Cu–2.4 Ni–0.6 Si alloy produced by the spray forming process10.1016/j.jmatprotec.2003.12.013 ↗
53. Effect of grain boundaries on t exture formation during dynamic recrystallization of magnesium alloys10.1016/j.actamat.2017.01.063 ↗
54. Interfacial grain structure, texture and tensile behavior of multilayer deformation-based additively manufactured Al 6061 alloy10.1016/j.matchar.2023.112646 ↗
55. Effect of grain boundaries on texture formation during dynamic recrystallization of magnesium alloys10.1016/j.actamat.2017.01.063 ↗
56. Tensile behavior of friction stir welded AA 6061-T4 aluminum alloy joints10.1016/j.matdes.2011.12.022 ↗
57. Mohamed Elbestawi. Friction stir processing of AlSi10Mg parts produced by selective laser melting10.1016/j.jmatprotec.2018.08.030 ↗
58. Enhancing microstructure and mechanical properties of laser powder bed fusion-fabricated AlSi10Mg alloy through tailored friction stir processing and post-heat treatment
59. Precipitation-induced mitigation of recrystallization in ultra-thin, cold-rolled AlScZrMn(Mg) sheets at brazing temperatures: the critical effect of alloy composition and thermal processing route10.1016/j.actamat.2020.01.003 ↗
60. Effect of grain size and dislocation density on thermal stability of Al-Cu-Mg alloy10.1016/j.mtla.2024.102276 ↗
61. Twin recrystallization mechanisms in magnesium-rare earth alloys10.1016/j.actamat.2015.05.044 ↗
62. Effect of ageing on tensile behavior of ultrafine grained Al 6061 alloy10.1016/j.msea.2015.06.036 ↗
63. Elucidating the effect of additive friction stir deposition on the resulting microstructure and mechanical properties of magnesium alloy WE4310.3390/met11111739 ↗
64. Anisotropy and mechanical properties of dissimilar Al additive manufactured structures generated by multi-layer friction surfacing10.1007/s00170-022-10685-3 ↗
65. Effect of rotation speed on microstructure and mechanical anisotropy of Al-5083 alloy builds fabricated by friction extrusion additive manufacturing10.1016/j.msea.2022.144237 ↗
66. Ductile failure behavior of polycrystalline Al 6061-T610.1007/s10704-012-9689-z ↗
67. Improvement of tensile and fracture toughness properties of Al 2014 alloy processed by different rolling method followed by post-ageing treatment10.1007/s12666-021-02198-6 ↗
68. Effect of room temperature rolling followed by annealing on tensile and fracture behaviour of bulk ultrafine-grained Al–Li 8090 alloy10.1007/s13632-019-00570-z ↗
69. Influence of build direction and heat treatment on the microstructure and tensile characteristics of cold metal transfer based wire arc additive manufactured SS 304L10.1016/j.cirpj.2023.08.013 ↗
70. The effect of cryogenic applications on tensile strength of aluminum 2219-T87 T-joint welded by dual laser-beam bilateral synchronous welding10.1016/j.jmapro.2020.05.020 ↗