Assessment of the suitability of an existing L360NB natural gas pipeline for hydrogen transport using the hollow specimen technique

Ahmed Hamed, Monika Beschliesser, Stefan Fink, Gregor Mori

Abstract

Evaluating the efficiency and suitability of the existing natural gas transport and storage infrastructure for hydrogen use is the main key to boost hydrogen implementation. In this research, hollow specimens made of an existing L360NB natural gas pipeline steel, including a girth weld, were investigated up to 1000 bar hydrogen. Slow strain rate and cyclic ripple load tests at different stress levels were performed. The fracture surfaces of slow strain rate tests showed a certain limited hydrogen embrittlement. Cyclic loads up to 7000 cycles at different stresses resulted in no rupture, even at stresses above yield strength. The severe testing conditions say for the applicability of L360 NB pipeline steel for hydrogen transport.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Material Properties and Failure Mechanisms

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (34)

Show source-provided references
1. Tensile testing in high - pressure gaseous hydrogen using the hollow specimen method10.1557/s43577-024-00776-9 ↗
2. Chandler · 1974 · 170
3. Influence of high pressure hydrogen environment on tensile and fatigue properties of stainless steels at low temperatures10.1063/1.4712078 ↗
4. Effect of high-pressure H2 gas on tensile and fatigue properties of stainless steel SUS316L by means of the internal high-pressure H2 gas method10.1016/j.prostr.2019.12.053 ↗
5. Hydrogen environment embrittlement evaluation in fatigue properties of stainless steel SUS304L at cryogenic temperatures10.1063/1.3402310 ↗
6. Comparison of tensile properties of X60 pipeline steel tested in high pressure gaseous hydrogen using tubular and conventional specimen10.1016/j.ijhydene.2022.07.211 ↗
7. In-situ hollow sample setup design for mechanical characterisation of gaseous hydrogen embrittlement of pipeline steels and welds10.3390/met11081242 ↗
8. Evaluating the effect of blended and pure hydrogen in X60 pipeline steel for low-pressure transmission using hollow-specimen slow-strain-rate tensile testing10.3390/met14101132 ↗
9. Hydrogen environment assisted cracking in X70 welding heat-affected zone under a high-pressure hydrogen gas10.1016/j.tafmec.2020.102746 ↗
10. Steiner · 2023
11. 1988
12. Effect of hydrogen in mixed gases on the mechanical properties of steels—theoretical background and review of test results10.3390/met11111847 ↗
13. Comparison of hydrogen embrittlement in three pipeline steels in high pressure gaseous hydrogen environments10.1016/j.corsci.2012.01.028 ↗
14. Effects of hydrogen charging time and pressure on the hydrogen embrittlement susceptibility of X52 pipeline steel material10.1007/s40195-023-01625-5 ↗
15. Experimental and molecular dynamics study of the hydrogen embrittlement behavior of X52 steel: analysis of abnormal hydrogen embrittlement susceptibility10.1016/j.ijhydene.2024.08.183 ↗
16. Investigations on the hydrogen embrittlement tendency of K55 for underground storage applications using hollow probe specimens10.1016/j.matlet.2024.136330 ↗
17. Assessing the hydrogen embrittlement susceptibility of an existing L360NB natural gas pipeline steel for 100 % hydrogen transport10.1016/j.corsci.2024.112648 ↗
18. Evaluation of the impact of gaseous hydrogen on pipeline steels utilizing hollow specimen technique and μCT10.1016/j.ijhydene.2024.02.005 ↗
19. Use of existing steel pipeline infrastructure for gaseous hydrogen storage and transport: a review of factors affecting hydrogen induced degradation10.1016/j.jngse.2022.104534 ↗
20. Absorption of gases by metals
21. Lee · 2016
22. Tensile testing in high pressure gaseous hydrogen using conventional and tubular specimens: austenitic stainless steels10.1016/j.ijhydene.2023.03.248 ↗
23. Investigation of resistance to gaseous hydrogen of a longitudinal weld seam in a X65 pipeline using the hollow specimen technique10.1007/s40194-025-01953-3 ↗
24. Hydrogen in pipeline steels: recent advances in characterization and embrittlement mitigation10.1016/j.jngse.2022.104709 ↗
25. Susceptibility of pipeline girth welds to hydrogen embrittlement and sulphide stress cracking10.1002/maco.201206574 ↗
26. Investigation of hydrogen embrittlement in welded joints of the L360MH pipeline steel for hydrogen transportation10.1016/j.corsci.2025.112940 ↗
27. Distinguishing geometric and metallurgic hydrogen-embrittlement susceptibilities in pre-cracked structures made of interstitial-free steel under monotonic tension10.1016/j.tafmec.2020.102574 ↗
28. Effect of hydrogen and stress concentration on the notch tensile strength of AISI 4135 steel10.1016/j.msea.2005.03.008 ↗
29. Michler
30. Evaluation of the tensile properties of X65 pipeline steel in compressed gaseous hydrogen using hollow specimens10.1016/j.prostr.2024.01.074 ↗
31. Rippled strain rate test for CRA sour service materials selection
32. On the applicability of carbon steels K55 and L80 for underground hydrogen storage10.1016/j.ijhydene.2023.12.123 ↗
33. An evaluation of the ripple-slow strain rate (R-SSR) technique for environmentally assisted cracking (EAC) qualification of modified 13Cr-110 stainless steel
34. Monotonic and cyclic slow strain rate testing of super 13% chromium steel welds under cathodic protection10.5006/1.3278165 ↗