journal article·2025-07Open access

Physically simulated heat-affected zones of 2101 lean duplex stainless steel: microstructure, corrosion behavior, and DICTRA® analysis at different cooling rates

C.L. Kugelmeier, R. Silva, G.S. Vacchi, M.V.G. Rodrigues, S.F. Rodrigues, D.C.C. Magalhães, R. Magnabosco, C.A.D. Rovere

Abstract

The effect of cooling rates on microstructure evolution and pitting corrosion resistance of the Gleeble®-simulated heat-affected zones (HAZs) of UNS S32101 lean duplex stainless steel (LDSS 2101) was studied. Thus, physical simulations of single-pass welding were performed, applying cooling rates of 200, 100, 50, 20, or 10 °C/s to obtain high-temperature HAZs (HT-HAZ) and 5 or 1 °C/s to obtain low-temperature HAZs (LT-HAZ). The findings showed the formation of three primary austenite morphologies in the HT-HAZ. Significantly high-temperature chromium nitrides (Cr 2 N) precipitation was observed at 200, 100, and 50 °C/s cooling rates. The influence of Cr 2 N on LDSS 2101 was related to its amount, distribution (regions where precipitation occurred, such as α/α boundaries and α/γ interfaces), and the cooling rates applied. The degree of sensitization (DOS) remained below 1 % at all cooling rates. This finding is consistent with the anodic polarization tests, which showed similar pitting corrosion resistance for all cooling rates. Furthermore, DICTRA® simulations predicted the Cr 2 N precipitation behavior and Cr redistribution at the ferrite/nitride interface. Simulations showed that faster cooling rates, such as 200 °C/s, lead to local Cr-depletion (down to 7 %), while slower rates allow Cr enrichment at the interface (up to 12 %) but result in broader Cr-depleted zones. These opposing effects influence the stability of the passive film and help explain the similar DOS observed at intermediate cooling rates.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Microstructure and Mechanical Properties of Steels

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (82)

Show source-provided references
1. Effect of thermal aging at 475 °C on the properties of lean duplex stainless steel 210110.1016/j.matchar.2016.03.002 ↗
2. Effect of Ni content on 475 °C embrittlement of directed energy deposited duplex stainless steel using a laser beam and wire feedstock10.1016/j.mtla.2024.102155 ↗
3. Predicting the Ms temperature of lean alloyed ferritic – austenitic stainless steels10.1016/j.jmrt.2025.01.089 ↗
4. New insights into the hardening and pitting corrosion mechanisms of thermally aged duplex stainless steel at 475 °C: a comparative study between 2205 and 2101 steels10.1016/j.jmst.2021.04.046 ↗
5. Thermal aging at 475 °C of newly developed lean duplex stainless steel 2404: mechanical properties and corrosion behavior10.1016/j.corsci.2016.12.014 ↗
6. Effect of brief heat treatments performed between 650 and 850°C on corrosion behaviour of a lean duplex stainless steel10.1016/j.corsci.2015.01.035 ↗
7. Kinetics of sigma phase formation in a duplex stainless steel10.1590/S1516-14392009000300012 ↗
8. Inhibition of the second phase precipitation and improvement of intergranular corrosion resistance by boron segregation at the grain boundary of S31254 superaustenitic stainless steel10.1016/j.corcom.2023.08.006 ↗
9. Effect of welding processes and conditions on the microstructure, mechanical properties and corrosion resistance of duplex stainless steel weldments—a review10.1016/j.jmapro.2016.11.003 ↗
10. Influence of friction stir processing (FSP) on arc directed energy deposited 316 L stainless steel: a corrosion science study10.1016/j.corcom.2023.12.001 ↗
11. Effect of microstructure evolution caused by welding process on pitting behavior of 321 stainless steel10.1016/j.corsci.2024.112591 ↗
12. Microstructure and corrosion behavior of welded joint between 2507 super duplex stainless steel and E690 low alloy steel10.1016/j.corcom.2022.08.005 ↗
13. Effects of cooling time and alloying elements on the microstructure of the Gleeble-simulated heat-affected zone of 22% Cr duplex stainless steels10.1361/105994901770344665 ↗
14. Reduction of austenite-ferrite galvanic activity in the heat-affected zone of a Gleeble-simulated grade 2205 duplex stainless steel weld10.1016/j.corsci.2019.108198 ↗
15. Effect of heat input and role of nitrogen on the phase evolution of 2205 duplex stainless steel weldment10.1016/j.ijpvp.2019.103952 ↗
16. Microstructural characterization and electron backscatter diffraction analysis across the welded interface of duplex stainless steel10.1016/j.apsusc.2017.03.301 ↗
17. Understanding the pitting behavior of laser welds in different austenitic stainless steels: from the perspective of pitting initiation10.1016/j.corsci.2023.111483 ↗
18. Investigation on microstructure and impact toughness of different zones in duplex stainless steel welding joint10.1007/s11665-016-2441-5 ↗
19. Y. The microstructure and pitting resistance of 2002 lean duplex stainless steel after the simulated welding thermal cycle process
20. Effect of aging on the corrosion resistance of 2101 lean duplex stainless steel10.1016/j.matchar.2009.08.009 ↗
21. Effect of ageing on precipitation and impact energy of 2101 economical duplex stainless steel10.1016/j.matchar.2008.07.002 ↗
22. Microstructural and ultrasonic characterization of 2101 lean duplex stainless steel welded joint10.1016/j.apacoust.2016.10.018 ↗
23. Characterization of the soft zone in dissimilar welds joint of 2.25Cr-1Mo and lean duplex LDX 2101 steel10.1016/j.fusengdes.2020.112147 ↗
24. Study of heat input effects on the microstructure of lean duplex 2101 shielded metal arc weld and its effect on mechanical properties, corrosion, and scratch behavior10.1007/s13632-023-01001-w ↗
25. Microstructural behavior and corrosion analysis of lean duplex stainless steel 2101 under the influence of variable heat inputs using gas tungsten arc welding
26. Effect of nitrogen-containing shielding and backing gas on the pitting corrosion resistance of welded lean duplex stainless steel LDX 210110.1007/s40194-013-0046-2 ↗
27. Microstructure evolution and pitting corrosion resistance of the Gleeble-simulated heat-affected zone of a newly developed lean duplex stainless steel 200210.1016/j.jallcom.2015.10.218 ↗
28. Gleeble® simulation of the heat-affected zones in lean duplex stainless steel 2404: understanding the effect of cooling rates on microstructure evolution and pitting corrosion resistance10.1016/j.jmrt.2024.11.118 ↗
29. Microstructural characterization of simulated heat affected zone in a nitrogen-containing 2205 duplex stainless steel10.1016/S0921-5093(02)00065-5 ↗
30. Microstructure evolution and pitting corrosion behavior of UNS S32750 super duplex stainless steel welds after short-time heat treatment10.1016/j.corsci.2017.02.006 ↗
31. 2023
32. 2015
33. Effect of 475°C embrittlement on duplex stainless steels localized corrosion resistance10.1016/j.corsci.2004.06.012 ↗
34. Mechanisms of intergranular corrosion and self-healing in high temperature aged lean duplex stainless steel 240410.1038/s41529-024-00541-y ↗
35. 2014
36. The determination of pitting potentials
37. A comprehensive study of the pitting corrosion mechanism of lean duplex stainless steel grade 2404 aged at 475 °C10.1016/j.corsci.2021.109738 ↗
38. Effect of solubilization heat treatment on microstructure and corrosion resistance of joints welded with the autogenous TIG process duplex stainless steel10.1016/j.jmrt.2023.08.014 ↗
39. Physical and kinetic simulation of nitrogen loss in high temperature heat affected zone of duplex stainless steels10.1016/j.mtla.2019.100325 ↗
40. Influence of cooling rate on microstructure evolution and pitting corrosion resistance in the simulated heat-affected zone of 2304 duplex stainless steels10.1016/j.corsci.2012.01.018 ↗
41. M23C6 carbides and Cr2N nitrides in aged duplex stainless steel: a SEM, TEM and FIB tomography investigation10.1016/j.micron.2016.01.007 ↗
42. Multi-pass arc welding techniques of 12 mm thick super-duplex stainless steel10.1016/j.jmatprotec.2019.03.031 ↗
43. Time-temperature-precipitation and property diagrams for super duplex stainless steel weld metals10.1007/s40194-018-0548-z ↗
44. Microstructure and corrosion behavior of S32101 stainless steel underwater dry and wet welded joints10.1016/j.jmatprotec.2018.02.018 ↗
45. Secondary austenite formation and its relation to pitting corrosion in duplex stainless steel weld metal10.1179/mst.1995.11.3.276 ↗
46. Effect of solution treatment temperature on the precipitation kinetic of σ-phase in 2205 duplex stainless steel welds10.1016/j.msea.2008.06.024 ↗
47. On the pitting resistance of friction stir welded UNS S82441 lean duplex stainless steel10.1016/j.jmrt.2019.05.010 ↗
48. Evolution of phase ratio and its effect on residual stress for 2205 duplex stainless steel multipass welded joints by thermo-metallurgical-mechanical model10.1016/j.ijpvp.2024.105283 ↗
49. Investigation on microstructure evolution and properties of duplex stainless steel joint multi-pass welded by using different methods10.1016/j.matdes.2016.07.110 ↗
50. Mechanism of δ → δ + γ phase transformation and hardening behavior of duplex stainless steel via sub-rapid solidification process10.1016/j.matchar.2020.110679 ↗
51. Investigations on reformed austenite in the microstructure of dissimilar super duplex/pipeline steel weld10.1016/j.matlet.2020.129109 ↗
52. The effect of phase transformation route on the intergranular corrosion susceptibility of 2205 duplex stainless steel10.1016/j.matlet.2018.11.143 ↗
53. Corrosion studies using potentiodynamic and EIS electrochemical techniques of welded lean duplex stainless steel UNS S8244110.1016/j.apsusc.2016.01.260 ↗
54. Unlocking the influence of microstructural evolution on hardness and pitting corrosion in duplex stainless welded joints10.1016/j.corsci.2022.110532 ↗
55. Influence of microstructure and elemental partitioning on pitting corrosion resistance of duplex stainless steel welding joints10.1016/j.apsusc.2016.10.047 ↗
56. The evolution of microstructure and intergranular corrosion resistance of duplex stainless steel joint in multi-pass welding10.1016/j.jmatprotec.2019.116471 ↗
57. Study of corrosion behavior of a 22% Cr duplex stainless steel: influence of nano-sized chromium nitrides and exposure temperature10.1016/j.electacta.2013.09.056 ↗
58. Microstructural and electrochemical behavior of 2205 duplex stainless steel weldments10.1016/j.surfin.2017.09.007 ↗
59. Study of the effect of sigma phase precipitation on the sliding wear and corrosion behaviour of duplex stainless steel AISI 220510.1016/j.wear.2017.12.019 ↗
60. Identification of sigma and chi phases in duplex stainless steels10.1016/j.matchar.2015.12.004 ↗
61. Precipitation of sigma phase in duplex stainless steel and recent development on its detection by electrochemical potentiokinetic reactivation: a review10.1016/j.corcom.2021.08.001 ↗
62. Precipitation and phase transformations in 2101 lean duplex stainless steel during isothermal aging10.1007/s11661-015-3215-7 ↗
63. Effects of solution treatment and continuous cooling on phase σ-precipitation in a 2205 duplex stainless steel
64. Pitting corrosion of metals10.1149/1.1838615 ↗
65. Microstructural evolution and localized corrosion behavior of friction stir welded super duplex UNS S32760 in chloride-containing environments10.1016/j.jmrt.2025.03.042 ↗
66. Unraveling the Cr2N precipitation and its negative effect on the corrosion resistance of friction stir welded UNS S32760 super duplex stainless steel
67. Effect of nitrogen on precipitation behavior of hyper duplex stainless steel S3270710.1016/j.matchar.2021.111096 ↗
68. Study of nobility of chromium nitrides in isothermally aged duplex stainless steels by using SKPFM and SEM/EDS10.1016/j.corsci.2009.08.057 ↗
69. Corrosion behavior of radial friction welded supermartensitic stainless steel pipes10.1016/j.matdes.2014.09.003 ↗
70. Low temperature embrittlement of duplex stainless steel: correlation between mechanical and electrochemical behavior10.1016/j.msea.2010.02.069 ↗
71. Sedriks · 1996
72. The influence of microstructural evolution on selective corrosion in duplex stainless steel flux-cored arc welded joints10.1016/j.corsci.2016.12.007 ↗
73. Evaluation of microstructural effects on the degree of sensitization (DOS) of a UNS S31803 duplex stainless steel aged at 475 °C10.5006/1701 ↗
74. Influence of microstructure on the corrosion resistance of the duplex stainless steel UNS S3180310.1016/j.matchar.2007.09.002 ↗
75. Nitrides precipitation and preferential pitting corrosion of ferrite phase in UNS S39274 superduplex stainless steel10.1007/s13632-020-00685-8 ↗
76. Secondary austenite and chromium nitride precipitation in simulated heat affected zones of duplex stainless steels10.1179/136217104225021715 ↗
77. Effect of a brief post-weld heat treatment on the microstructure evolution and pitting corrosion of laser beam welded UNS S31803 duplex stainless steel10.1016/j.corsci.2012.08.054 ↗
78. Investigation of the sensitization and intergranular corrosion of tube-to-tubesheet welds of hyper duplex stainless steel using an electrochemical reactivation method10.1016/j.corsci.2014.06.005 ↗
79. Initiation mechanism of pitting corrosion in weld heat affected zone of duplex stainless steel10.1016/j.corsci.2022.110278 ↗
80. Influence of heat input on microstructure, hardness and pitting corrosion of weld metal in duplex stainless steel welded by keyhole-TIG10.1016/j.matchar.2021.111052 ↗
81. Evolution of current transients and morphology of metastable and stable pitting on stainless steel near the critical pitting temperature10.1016/j.corsci.2005.03.002 ↗
82. Mechanism of improving corrosion resistance in heat affected zone of duplex stainless steel by tantalum addition10.1016/j.corsci.2023.111748 ↗