journal article·2025-11Open access

Design and magnetic properties of gradient Fe(Si)/Fe structure soft magnetic composites

Xiaoyu Wang, Ziru Zheng, Kun Peng

Abstract

Soft magnetic composites (SMCs) play a key role in the electric energy conversion, developing higher magnetization and lower loss SMCs is a strategy for modern power system and electric devices. In this paper, a gradient Fe(Si)/Fe particles is prepared by a Si diffusion method, the high electronic resistivity gradient Fe(Si) reduced the intraparticle eddy current loss and total loss, which can be explained by the cause and influence factor of eddy current loss. The optimized magnetic properties of Fe(Si)/Fe composites can be obtained by Si diffusion for 60 min to form a several micrometer thickness Fe(Si) shell on Fe particles surface, it has a high permeability (77) and magnetization (216.7emu/g) which was about 97 % of pure Fe (219.2 emu/g), the total loss at 50 KHz, 20 mT was 110.56 mW/cm 3 , which was much lower pure Fe cores and slightly higher than that of Fe-6.5 wt%Si alloy, which provide a method for the development of SMCs with high saturation magnetization and low loss.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Metallic Glasses and Amorphous Alloys · Magnetic Properties and Applications · Magnetic Properties of Alloys

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (29)

Show source-provided references
1. Development of soft magnetic composites for low-loss applications10.1016/S0304-8853(01)01252-5 ↗
2. Fe-based amorphous soft magnetic composites with SiO2 insulation coating: a study on coatings thickness, microstructure and magnetic properties10.1016/j.ceramint.2020.02.128 ↗
3. Soft magnetic composite materials (SMCs)10.1016/j.jmatprotec.2007.02.034 ↗
4. Soft magnetic materials for a sustainable and electrified world10.1126/science.aao0195 ↗
5. High permeability and low loss bioinspired soft magnetic composites with nacre-like structure for high frequency applications10.1016/j.actamat.2019.01.035 ↗
6. Particles size dependent magnetic properties of FeSiAl soft magnetic composite with hybrid insulating coating for MHz applications
7. Multimodal iron loss analyses based on magnetization processes for various soft magnetic toroidal cores10.1016/j.jmmm.2024.172222 ↗
8. Crystal-like microstructural Finemet/FeSi compound powder core with excellent soft magnetic properties and its loss separation analysis10.1016/j.matdes.2020.108769 ↗
9. Power loss separation in Fe-based composite materials10.1016/j.jmmm.2012.09.055 ↗
10. Improved core-loss calculation for magnetic components employed in power electronic systems10.1109/TPEL.2011.2162252 ↗
11. Magnetic properties regulation and loss contribution analysis of FeSi soft magnetic composites doped by carbonyl iron powders10.1016/j.jmmm.2023.170423 ↗
12. Structure and magnetic properties of ZrO2-coated Fe powders and Fe/ZrO2 soft magnetic composites10.1016/j.apt.2017.04.029 ↗
13. In-situ formation of Fe3O4 and ZrO2 coated Fe-based soft magnetic composites by hydrothermal method10.1016/j.ceramint.2018.11.058 ↗
14. Controllable SiO2 insulating layer and magnetic properties for intergranular insulating Fe-6.5wt.%Si/SiO2 composites10.1016/j.apt.2018.12.004 ↗
15. Intergranular insulated Fe/SiO2 soft magnetic composite for decreased core loss10.1016/j.apt.2016.04.002 ↗
16. Fe-based soft magnetic composites coated with NiZn ferrite prepared by a co-precipitation method10.1016/j.jmmm.2016.12.024 ↗
17. Reduction of core loss for FeSi soft magnetic composites prepared using atomic layer deposition-based coating and high-temperature annealing10.1016/j.jallcom.2022.164655 ↗
18. Ultra-low core loss FeSiAl-based soft magnetic composites with ultra-thin MoO3 composites insulting layer10.1016/j.ceramint.2022.06.228 ↗
19. Ultra-low core loss FeSiAl soft magnetic composites with in-situ double oxidation layers of outer Fe3O4 layer and inner super-thin Al2O3/SiO2 hybrid layer10.1016/j.ceramint.2023.05.191 ↗
20. Fe-Si-Al soft magnetic composites with significantly reduced core loss via constructing uniform TiO2 insulation layer10.1007/s10948-022-06289-3 ↗
21. Ultra-low core loss and high permeability Fe-based amorphous soft magnetic composites with ultra-fine FeNi additives
22. Particle size selection principle of Fe-Si-Al SMCs for high-frequency and high-power applications10.1016/j.jmmm.2022.169803 ↗
23. Soft magnetic composites based on Fe elemental, binary and ternary alloys systems fabricated by surface nitridation10.1016/j.jmmm.2019.01.070 ↗
24. Thermodynamic quantitative analysis and formation mechanism on novel multilayered Fe-Si core-shell magnetic abrasives10.1016/j.jmapro.2024.12.042 ↗
25. Static and dynamic magnetic properties of Co2Z barium ferrite nanoparticle composites10.1007/s10853-005-6312-y ↗
26. A two-step stress-annealing with stress-relaxation process for developing low-loss Fe-based nanocrystalline soft magnetic cores10.1016/j.jmmm.2024.172280 ↗
27. Hiralani · 2019
28. Hystersis and eddy-current losses of transformer lamination viewed as an application of poynting theorem
29. Thin Fe-Si-Al alloy sheet fabricated by Al gradient diffusion through PVD for excellent high-frequency magnetic properties