Effect of H2O addition on corrosion and carburization behavior in high-chromium alloys exposed to supercritical CO2 at 500 °C
Source abstract
Abstract
To clarify the role of H 2 O addition on corrosion and carburization behavior, four chromia-forming alloys (SS 347H, Alloy 800HT, SS 310S, and Alloy 625) containing 18–25 wt% Cr were exposed to supercritical–CO 2 (S–CO 2 ) containing 3.1 vol.% H 2 O at 500 °C and 25 MPa for 1000 h. All alloys exhibited very low weight gains and formed thin, continuous oxide scales without spallation or the formation of thick Fe-rich nodular oxides. The oxide scales consisted primarily of chromia (Cr 2 O 3 ) with accompanying (Mn,Fe) 3-x Cr x O 4 spinel. Minor and discontinuous SiO 2 , Al 2 O 3 , and TiO 2 were locally observed depending on alloy composition. Compared with exposures in high-purity S–CO 2 , the presence of H 2 O moderately increased corrosion rates at 500 °C. In the Fe-based alloys, Cr-rich carbides were observed within subsurface Cr-depleted regions. However, no carbon enrichment was detected at the oxide and matrix interface, indicating that these carbides originated from intrinsic carbon rather than carbon ingress from S–CO 2 . Thermodynamic calculations further demonstrate that H 2 O addition increases the oxygen partial pressure while significantly reducing carbon activity. This combination stabilizes chromia formation and effectively suppresses carburization at this intermediate temperature.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: High-Temperature Coating Behaviors · Metal Alloys Wear and Properties · Microstructure and Mechanical Properties of Steels
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (46)
Show source-provided references
1. Review of supercritical CO2 power cycle technology and current status of research and development10.1016/j.net.2015.06.009 ↗
2. Supercritical CO2 Brayton cycles for solar thermal energy10.1016/j.apenergy.2013.06.020 ↗
3. A strategy of mixture preparation for methane direct-fired sCO2 combustors
4. High efficiency and low cost of electricity generation from fossil fuels while eliminating atmospheric emissions, including carbon dioxide10.1016/j.egypro.2013.05.211 ↗
5. Corrosion and carburization behavior of chromia-forming heat-resistant alloys in high-temperature supercritical-carbon-dioxide environment10.1016/j.corsci.2015.07.007 ↗
6. Effect of pressure on the corrosion and carburization behavior of chromia-forming heat-resistant alloys in high-temperature carbon-dioxide environments10.1016/j.corsci.2016.06.004 ↗
7. Characterization of Alloy 600 joints exposed to a high- temperature supercritical-carbon-dioxide environment10.1016/j.matchar.2018.02.025 ↗
8. Alloys SS316 and Hastelloy-C276 in supercritical CO2 at high temperature10.1007/s11085-015-9589-5 ↗
9. Factors in the oxidation assessment of AISI Type 310 steels in high-pressure carbon dioxide10.1016/0010-938X(82)90129-9 ↗
10. Corrosion of a stainless steel and nickel-based alloys in high-temperature supercritical carbon-dioxide environment10.1016/j.corsci.2012.11.041 ↗
11. The performance of Haynes 282 and its weld in supercritical CO210.1016/j.msea.2019.05.080 ↗
12. Effect of surface finish on high-temperature oxidation of steels in CO2, supercritical CO2, and air10.1007/s11085-019-09938-6 ↗
13. Corrosion behavior of typical structural steels in 500 °C, 600 °C and high pressure supercritical carbon dioxide conditions10.1016/j.corsci.2021.109801 ↗
14. Compatibility of FBR structural materials with supercritical carbon dioxide10.1016/j.pnucene.2011.04.030 ↗
15. Effect of stress on corrosion behavior of martensitic and austenitic steels in supercritical carbon dioxide at 550 ◦C and 20 MPa10.1016/j.supflu.2022.105805 ↗
16. Corrosion behaviors of structural materials in high temperature S-CO2 environments10.14773/cst.2014.13.2.41 ↗
17. Corrosion behavior of an alumina-forming austenitic steel exposed to supercritical carbon dioxide10.1016/j.corsci.2013.12.023 ↗
18. Microstructures, tensile properties and corrosion behaviors of Fe20Cr25NiNb stainless steels with different Al contents in supercritical carbon dioxide10.1016/j.jmrt.2023.02.224 ↗
19. Tucker · 2019
20. Carbon transport through oxide scales on Fe-Cr alloys10.1007/BF00751801 ↗
21. Penetration of protective chromia scales by carbon10.1016/j.scriptamat.2014.01.009 ↗
22. Corrosion and creep behavior of a Ni-base alloy in supercritical-carbon dioxide environment at 650 °C10.1016/j.corsci.2020.108843 ↗
23. Corrosion and mechanical performance of grade 92 ferritic-martensitic steel after exposure to supercritical carbon dioxide10.1007/s11661-020-05691-7 ↗
24. Water-vapour effects on corrosion of Fe-Cr and fe-cr-ni alloys containing cerium and manganese in CO2 gas at 818 °C10.1016/j.corsci.2014.08.029 ↗
25. Characterization of chromia scales formed in supercritical carbon dioxide10.1080/09603409.2017.1389371 ↗
26. The effect of CO2 pressure on chromia scale microstructure at 750 °C
27. Corrosion of SS310 and alloy 740 in high-temperature supercritical CO2 with impurities H2O and O210.1016/j.corsci.2021.109350 ↗
28. Corrosion of alloy Haynes 230 in high-temperature supercritical carbon dioxide with oxygen impurity additions10.1007/s11085-016-9654-8 ↗
29. A tracer study on sCO2 corrosion with multiple oxygen-bearing impurities10.1007/s11085-021-10071-6 ↗
30. Effects of CO and O2 impurities on supercritical CO2 corrosion of alloy 62510.1007/s11661-018-4727-8 ↗
31. High-temperature corrosion and carburization behavior of austenitic stainless steels in impurity-added CO2 environments
32. Effect of impurity addition on the corrosion and carburization behavior of alloy 800HT in CO2 environment at 600 °C10.1016/j.jmrt.2024.11.210 ↗
33. Corrosion and carburization behavior of high-chromium alloys in high-temperature supercritical CO2 with 3.1% H2O addition10.1016/j.corsci.2025.113305 ↗
34. Oxidation behaviour and microstructural stability of alloy 625 during long-term exposure in steam10.1007/s10853-014-8344-7 ↗
35. The role of aluminum and titanium on the oxidation process of a nickel-base superalloy in steam at 800 °C10.1007/BF00656727 ↗
36. Corrosion and nodule oxide formation mechanism of alloy 625 in high temperature CO2 environment with impurities10.1016/j.corsci.2025.113307 ↗
37. Effect of pressure and impurities on oxidation in supercritical CO210.1002/maco.201810652 ↗
38. Effect of pressure on high-temperature oxidation of Ni alloys in supercritical CO2 containing impurities10.1016/j.corsci.2023.111055 ↗
39. The oxidation behaviour of metals and alloys at high temperatures in atmospheres containing water vapour: a review10.1016/j.pmatsci.2007.11.001 ↗
40. Growth and adherence of chromia based surface scales on Ni-base alloys in high- and low-pO2 gases10.1016/j.msea.2007.05.035 ↗
41. Role of water vapor in chromia-scale growth at low oxygen partial pressure10.1023/A:1023040010859 ↗
42. Chromium volatilization rates from Cr2O3 scales into flowing gases containing water vapour10.1007/s11085-006-9030-1 ↗
43. High temperature oxidation of Fe–Cr alloy in O2–H2–H2O atmospheres; microstructure and kinetics10.1016/S0921-5093(03)00527-6 ↗
44. Chromium-depleted zones and the oxidation process in stainless steels
45. Prediction of chromium depleted-zone evolution during aging of Ni–Cr–Fe alloys10.1016/S1359-6454(01)00444-X ↗
46. The carburization behavior of alloy 800HT in high temperature supercritical-CO2