Effect of Cl− to SO42− molar ratio on corrosion resistance of Zr41.2Ti13.8Cu12.5Ni10Be22.5 metallic glass
Source abstract
Abstract
The effect of Cl - /SO 4 2- molar ratio on the corrosion behavior of Zr 41.2 Ti 13.8 Cu 12.5 Ni 10 Be 22.5 metallic glass was systematically investigated in mixed MgCl 2 and MgSO 4 solutions with molar ratios of 1:0, 9:1, 7:1, 5:1, 4:1, 3:1, and 0:1. Within the molar ratio range 9:1 to 2:1, decreasing Cl - concentration resulted in a rightward shift of the polarization curves and an elevation of the corrosion potential from -198.8 mV to 18.3 mV. The lowest corrosion current density, the highest pitting potential, and the widest width of the passive region were observed at a Cl - /SO 4 2- molar ratio of 5:1, indicating optimal corrosion resistance under this condition. Notably, no pitting corrosion occurred in pure SO 4 2- solution, whereas the most severe pitting was observed in pure Cl - solution. As the Cl - concentration decreased, the severity of pitting corrosion progressively diminished. At a molar ratio of 2:1, both localized pitting corrosion and “earthen embankment-like” corrosion product deposits were observed on the metallic glass surface. This study identifies a critical Cl - /SO 4 2- molar ratio threshold of 5:1. Above this molar ratio, SO 4 2- inhibits corrosion, while below it, SO 4 2- enhances Cl - -induced pitting corrosion. X-ray photoelectron spectroscopy (XPS) analysis revealed prominent signals corresponding to Zr 4+ , Ti 4+ , Cu + , and O1s, confirming the formation of a protective passive film primarily composed of TiO 2 and ZrO 2 . This oxide layer effectively impedes further interaction between the metallic glass and the corrosive environment. This advances our understanding of the corrosion behavior and mechanisms of metallic glasses in Cl - and SO 4 2- containing solutions, facilitating their application in corrosion protection.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Metallic Glasses and Amorphous Alloys · Metallurgical and Alloy Processes · Electrodeposition and Electroless Coatings
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (58)
Show source-provided references
1. Microbially influenced corrosion—Any progress?10.1016/j.corsci.2020.108641 ↗
2. Passivity breakdown, pit initiation and propagation of pits in metallic materials–review10.1016/j.corsci.2014.10.006 ↗
3. Localized corrosion (pitting): a model of passivity breakdown including the role of the oxide layer nanostructure10.1016/j.corsci.2008.06.047 ↗
4. Materials science: share corrosion data10.1038/527441a ↗
5. The effect of manganese and silicon additions on the corrosion resistance of a polycrystalline nickel-based superalloy10.1016/j.corsci.2020.109042 ↗
6. Effects of chloride and chloride-free accelerators combined with typical admixtures on the early-age cracking risk of concrete repair slabs10.1016/j.conbuildmat.2015.07.003 ↗
7. Long term effect of chloride and sulfate concentration, and cation allied with sulfates on corrosion performance of steel-reinforced in concrete
8. Combined effect of chloride and sulfate ions on the corrosion behavior of Q355B steel in simulated concrete pore solution
9. Influence of KCl and HCl on a laser clad FeCrAl alloy: in-situ SEM and controlled environment high temperature corrosion10.1016/j.corsci.2019.07.003 ↗
10. Correlation between relaxations and plastic deformation, and elastic model of flow in metallic glasses and glass-forming liquids
11. Correlation between boson peak and thermal expansion manifested by physical aging and high pressure10.1007/s11433-021-1815-8 ↗
12. Amorphous physics and materials: interstitialcy theory of condensed matter states and its application to non-crystalline metallic materials10.1088/1674-1056/26/1/016401 ↗
13. Development and implication of amorphous alloys
14. Nanostructured flexible Zr-based metallic glassy hydrogen evolution electrodes10.1016/j.ijhydene.2024.11.321 ↗
15. Hierarchical micro-nanostructured Zr-based metallic glass with tensile plasticity10.1016/j.actamat.2024.120553 ↗
16. Oxygen impurity improving corrosion resistance of a Zr-based bulk metallic glass in 3.5wt.%NaCl solution10.1016/j.corsci.2021.109867 ↗
17. The fracture of bulk metallic glasses10.1016/j.pmatsci.2015.05.002 ↗
18. Cold rolling improves the fracture toughness of a Zr-based bulk metallic glass10.1016/j.jallcom.2016.10.134 ↗
19. Properties of (TiZrNbCu)1-xNix metallic glasses10.1016/j.jallcom.2018.02.169 ↗
20. Zr-Co-Al bulk metallic glass composites containing B2 ZrCo via rapid quenching and annealing10.1016/j.jallcom.2019.153079 ↗
21. Comparison of corrosion resistance of Zr-based amorphous alloys and traditional alloys in seawater
22. Interfacial bonding, corrosion, and wear behavior of Zr-based amorphous (Zr41.2Ti13.8Cu12.5Ni10Be22.5) alloy coatings prepared by plasma spraying technique10.1016/j.surfcoat.2023.129818 ↗
23. Study on corrosion and wear behavior mechanism of Zr-based bulk amorphous
24. Electrochemical corrosion properties of Zr-and Ti-based bulk metallic glasses10.1016/S1003-6326(11)60750-4 ↗
25. Electrochemical corrosion behavior of amorphous alloys in different systems
26. Effect of SO42− and cl− anionic attack on the localized corrosion resistance and morphology of 409 ferritic stainless steel10.1016/j.rinp.2018.12.031 ↗
27. Magnetron sputtered non-toxic and precious element-free ti-zr-ge metallic glass nanofilms with enhanced biocorrosion resistance10.1002/admi.202201223 ↗
28. Chloride-induced alterations of the passive film on 316L stainless steel and blocking effect of pre-passivation10.1016/j.electacta.2019.135159 ↗
29. A high-throughput aqueous passivation testing methodology for compositionally complex alloys using a scanning droplet cell10.1149/1945-7111/aceeb8 ↗
30. A high-throughput structural and electrochemical study of metallic glass formation in ni-ti-al10.1021/acscombsci.9b00215 ↗
31. A mechanistic study on semiconductivity conversion of passive films under varying sulfate to chloride concentration ratios10.3866/PKU.WHXB201405211 ↗
32. Cathodic protection mechanism of iron and steel in porous media10.1038/s43246-024-00454-y ↗
33. Electrochemical and chemical corrosion behaviors of the in-situ Zr-based metallic glass matrix composites in chloride-containing solutions10.1016/j.jallcom.2018.08.174 ↗
34. Electrochemical evaluation of Mg and a Mg-Al 5% Zn metal-rich primers for protection of al-zn-mg-cu alloy in NaCl10.5006/4537 ↗
35. Microstructure-tuned hydrogen embrittlement in 7050 aluminum alloy: combined impedance analysis and advanced characterization10.1149/1945-7111/ae00f8 ↗
36. Cavitation erosion of the AA7050 aluminum alloy in 3.5 wt% NaCl solution—part 2: an impedance investigation of the effect of cavitation intensity on interfacial states10.1016/j.corsci.2025.112936 ↗
37. A mechanistic study on stress corrosion cracking of sensitized AA5083 in a simulated water level fluctuation zone: combined impedance analysis and tensile tests10.1016/j.corsci.2025.112701 ↗
38. Applications of impedance spectroscopy10.1002/9781119381860.ch4 ↗
39. Effect of annealing temperature on microstructure, mechanical properties and corrosion behavior of al-mg-mn-sc-zr alloy10.1016/j.apsusc.2020.146081 ↗
40. Corrosion of carbon steels subjected to chloride and sulfate in simulated concrete pore solutions with different pH10.1016/j.conbuildmat.2024.137445 ↗
41. Surface modification of ZnMgAl-coated steel by dielectric-barrier discharge plasma10.1039/C9RA07378G ↗
42. Barsoukov · 2005 · 58
43. Electrochemical impedance spectroscopy (EIS): principles, construction, and biosensing applications10.3390/s21196578 ↗
44. Electrochemical investigation on the effects of sulfate ion concentration, temperature and medium pH on the corrosion behavior of Mg–Al–Zn–Mn alloy in aqueous ethylene glycol10.1016/j.jma.2016.12.003 ↗
45. Effects of substrate temperature and deposition time on the morphology and corrosion resistance of FeCoCrNiMo0.3 high-entropy alloy coating fabricated by magnetron sputtering10.1007/s12613-020-2149-2 ↗
46. Corrosion behavior of bulk (Zr58Nb3Cu16Ni13Al10) 100-xYx (x= 0, 0.5, 2.5 at.%) metallic glasses in sulfuric acid10.1016/j.corsci.2019.01.016 ↗
47. Sequence of steps in the pitting of aluminum by chloride ions10.1016/S0010-938X(02)00231-7 ↗
48. Chloride ions as integral parts of hydrogen bonded networks in aqueous salt solutions: the appearance of solvent separated anion pairs10.1039/D0CP01806F ↗
49. The history of the point defect model for the passive state: a brief review of film growth aspects10.1016/j.electacta.2010.11.005 ↗
50. Modeling of electrochemical oxide film growth-a PDM refinement
51. Long-term corrosion resistance of new ti-ta-zr alloy in simulated physiological fluids by electrochemical and surface analysis methods10.1016/j.corsci.2015.01.038 ↗
52. Oxygen vacancy defects in Ta2O5 showing long-range atomic re-arrangements10.1063/1.4869553 ↗
53. Differences in pitting growth kinetics between Zr60Ni25A115 and Zr60Cu25Al15 metallic glasses exposed to a 0.6 M NaCl aqueous solution10.1016/j.corsci.2017.09.007 ↗
54. Critical review on the passive film formation and breakdown on the iron electrode and the models for the mechanisms underlying passivity10.1016/j.jelechem.2016.12.020 ↗
55. AgCl-induced hot salt stress corrosion cracking in a titanium alloy10.1016/j.corsci.2021.109497 ↗
56. First principles, explicit interface studies of oxygen vacancy and chloride in alumina films for corrosion applications10.1149/1945-7111/abe7a5 ↗
57. Electrochemical reconfiguration of iron-modified Ni3S2 surface induced oxygen vacancies to immobilize sulfate for enhanced oxygen evolution reaction10.1016/j.jcis.2024.08.052 ↗
58. The anodic passivity of titanium in mixed sulfate-chloride solutions10.1149/2.0451512jes ↗