journal article·2019-01Open access

Hot deformation and processing maps of Al–Zn–Mg–Cu alloy under coupling-stirring casting

Haijun Wang, Chao Wang, Yang Mo, Hui Wang, Jun Xu

Abstract

Compression tests of direct-chill (DC) casting and coupling-stirring (CS) casting Al–Zn–Mg–Cu alloy have been performed in the strain rate range from 0.01 s−1 to 10 s−1 and the temperature range from 320 °C to 480 °C. The effects of DC casting on the processing map, flow behavior and deformation kinetic have been discussed. The result shows that the uniformity of the critical stress, the peak stress and the steady-state stress have been improved and the flow stress has been decreased significantly using the coupling stirring. The processing maps shown that the suitable deformation condition for the DC casting alloy is 0.01–0.1 s−1 and 380–480 °C, and the suitable deformation condition for the CS casting alloy is 0.01–0.05 s−1 and 320–480 °C and 0.05–0.5 s−1 and 400–480 °C. The activation energies at the deterministic domains of the DC casting alloy and CS casting alloy are 210 kJ/mol and 185 kJ/mol, respectively.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Metallurgy and Material Forming · Aluminum Alloy Microstructure Properties · Microstructure and mechanical properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (29)

Show source-provided references
1. Influence of repetitious non-isothermal aging on microstructure and strength of Al–Zn–Mg–Cu alloy10.1016/j.jallcom.2016.08.017 ↗
2. Effect of the deformation on the stress–corrosion cracking of Al–Zn–Mg–Cu alloys10.1002/maco.201005732 ↗
3. Critical conditions for the occurrence of quench cracking in an Al–Zn–Mg–Cu alloy10.1007/s10853-014-8103-9 ↗
4. Effect of Al–5Ti–1B–1Re on the microstructure and hot crack of as-cast Al–Zn–Mg–Cu alloy10.1007/s11665-013-0860-0 ↗
5. Effect of low-frequency electromagnetic field on microstructures and macrosegregation of Φ270mm DC ingots of an Al–Zn–Mg–Cu–Zr alloy10.1016/j.matlet.2005.01.009 ↗
6. Evaluation of cracking resistance of DC casting high strength aluminum ingots10.1016/j.msea.2004.02.026 ↗
7. Precipitation induced densification in a sintered Al–Zn–Mg–Cu alloy10.1016/j.scriptamat.2006.04.021 ↗
8. Electromagnetic refining of aluminum alloys by the CREM process: Part I. Working principle and metallurgical results10.1007/BF02655919 ↗
9. Application research of a new coupling stirring on DC casting process for large-sized aluminum ingots10.4028/www.scientific.net/MSF.817.48 ↗
10. Strategy for the design of thermomechanical processes for AISI type 304L stainless steel using dynamic materials model (DMM) stability criteria and model for the evolution of microstructure10.1023/B:JMSC.0000039286.15633.32 ↗
11. Study on hot workability and optimization of process parameters of a modified 310 austenitic stainless steel using processing maps10.1016/j.matdes.2014.11.041 ↗
12. Study of hot forging behavior of as-cast Mg–3Al–1Zn–2Ca alloy towards optimization of its hot workability10.1016/j.matdes.2014.01.032 ↗
13. Processing maps, microstructure evolution and deformation mechanisms of extruded AZ31-DMD during hot uniaxial compression10.1016/j.msea.2012.09.023 ↗
14. Processing map-microstructure evolution correlation of hot compressed near alpha titanium alloy (TiHy 600)
15. Development and validation of a processing map for zirconium alloys10.1088/0965-0393/10/5/303 ↗
16. A comparative study of various flow instability criteria in processing map of superalloy GH474210.1016/j.jmst.2013.07.008 ↗
17. Hot forging design of as-cast NiTi shape memory alloy10.1016/j.materresbull.2014.04.049 ↗
18. Optimization of thermal processing parameters of Ti555211 alloy using processing maps based on Murty criterion10.1007/s12598-015-0655-6 ↗
19. Characterization of hot deformation behavior of extruded ZK60 magnesium alloy using 3D processing maps10.1016/j.matdes.2013.11.037 ↗
20. Correcting method of flow stress curve for hot compression
21. Forming behavior and workability of 6061/BC composite during hot deformation10.1016/j.compscitech.2011.02.009 ↗
22. Characterization of hot deformation behavior of Ni-base superalloy Rene’41 using processing map10.1016/j.msea.2013.07.066 ↗
23. Optimizing and identifying the process parameters of AZ31 magnesium alloy in hot compression on the base of processing maps10.1016/j.jallcom.2014.12.251 ↗
24. Modeling the initiation of dynamic recrystallization using a dynamic recovery model10.1016/j.jallcom.2011.07.014 ↗
25. Research on the hot deformation behavior of Al–6.2Zn–0.70Mg–0.3Mn–0.17Zr alloy using processing map10.1016/j.jallcom.2015.01.228 ↗
26. Hot deformation behavior of in situ synthesized Ti-1100 composite reinforced with 5vol.% TiC particles10.1016/j.matlet.2005.08.060 ↗
27. High strain rate superplastic deformation behavior of powder-metallurgy processed 17%SiCp/2024 Al composite
28. Dynamic analysis on the formation of velocity gradient of adhesive fluid