journal article·2020-05Open access

Effect of contact solid solution treatment on peak aging of Al-Zn-Mg-Cu alloys

Zhiqiang Zhang, Jianhao Yu, Dongye He

Abstract

Contact solid solution treatment (CST) can shorten peak aging time and improve precipitation strength of Al-Zn-Mg-Cu alloys. The effects of CST on the secondary phase evolution of Al-Zn-Mg-Cu alloys were studied and the strengthening mechanisms were also quantitatively evaluated. Compared with the peak aging time of 24 h for furnace solid solution treatment (FST), only 18 h are needed to reach the peak strength after CST. The results revealed that higher solid solubility caused by CST could increase the driving force of precipitation and reduce the formation temperature of η′ phase. Many fine precipitated phases of the aged sample after CST could be obtained and hinder the dislocation movement and strengthen the alloy.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties · Microstructure and mechanical properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (23)

Show source-provided references
1. Hot deformation and processing map of a typical Al-Zn-Mg-Cu alloy10.1016/j.jallcom.2012.10.114 ↗
2. Effect of equal channel angular pressing on the mechanical and tribological behavior of Al-Zn-Mg-Cu alloy10.1016/j.matchar.2018.03.045 ↗
3. Hot stamping of high-strength aluminium alloy aircraft parts using quick heating10.1016/j.cirp.2017.04.117 ↗
4. Hot stamping of AA7075 aluminum sheets
5. Influence of contact solid-solution treatment on microstructures and mechanical properties of 7075 aluminum alloy10.1016/j.msea.2018.11.108 ↗
6. Characterization of precipitation and phase transformations in Al-Zn-Mg alloy by the differential dilatometry10.1016/j.jallcom.2007.08.016 ↗
7. GP-zones in Al-Zn-Mg alloys and their role in artificial aging10.1016/S1359-6454(01)00251-8 ↗
8. Revisiting the precipitation sequence in Al-Zn-Mg-based alloys by high-resolution transmission electron microscopy10.1016/j.scriptamat.2010.08.001 ↗
9. The rapid age strengthening induced by Ag additions in 7075 aluminum alloy10.1016/j.msea.2015.09.044 ↗
10. Characterization of the composition and volume fraction of η, and η precipitates in an Al-Zn-Mg alloy by a combination of atom probe, small-angle X-ray scattering and transmission electron microscopy10.1016/j.actamat.2005.03.004 ↗
11. Influence of stress-aging processing on precipitates and mechanical properties of a 7075 Aluminum Alloy10.1002/adem.201700583 ↗
12. Strengthening mechanisms in cryomilled ultrafine-grained aluminum alloy at quasi-static and dynamic rates of loading10.1016/j.scriptamat.2008.12.026 ↗
13. Improvement of mechanical properties of AA6063 aluminum alloy after equal channel angular pressing by applying a two-stage solution treatment10.1016/j.msea.2017.01.024 ↗
14. Mechanical behavior and strengthening mechanisms in ultrafine grain precipitation-strengthened aluminum alloy10.1016/j.actamat.2013.09.042 ↗
15. Calorimetric studies of 7000 series aluminum alloys: I. Matrix precipitate characterization of 707510.1007/BF02667403 ↗
16. Microstructure-based modelling of isotropic and kinematic strain hardening in a precipitation-hardened aluminium alloy10.1016/j.actamat.2011.02.035 ↗
17. Strengthening mechanisms in a high-strength bulk nanostructured Cu-Zn-Al alloy processed via cryomilling and spark plasma sintering10.1016/j.actamat.2012.09.036 ↗
18. Coarsening resistance at 400°C of precipitation-strengthened Al-Zr-Sc-Er alloys10.1016/j.actamat.2011.07.057 ↗
19. Precipitation strengthening at ambient and elevated temperatures of heat-treatable Al (Sc) alloys10.1016/S1359-6454(02)00201-X ↗
20. Precipitate behavior and mechanical properties of enhanced solution treated Al-Zn-Mg-Cu alloy during non-isothermal ageing10.1016/j.jallcom.2017.11.178 ↗
21. Characterisation and modelling of precipitate evolution in an Al-Zn-Mg alloy during non-isothermal heat treatments10.1016/S1359-6454(03)00429-4 ↗
22. Modelling the overlap of nucleation, growth and coarsening during precipitation10.1016/j.actamat.2004.06.024 ↗
23. Non-isothermal ageing of an Al-8Zn-2Mg-2Cu alloy for enhanced properties10.1016/j.jmatprotec.2015.07.018 ↗