journal article·2020-05Open access

Wear and corrosion resistant Mn-doped austenitic cast iron prepared by powder metallurgy method

Xiangrong Li, Junbo Liu, Ji Xiong, Lu Yang, Qingshan Gou, Xiangyu Song, Zhixing Guo, Tao Hua, Mengxia Liang

Abstract

Wear and corrosion resistant austenitic cast irons were prepared by powder metallurgy (P/M). In this system, equivalent Mn were doped to replace nickel with a constant Nieq (the Ni equivalent number) to reduce the cost. Conventional high nickel cast iron was employed as a reference in this study. The hardness, dry sliding wear behavior and corrosion behavior of conventional and P/M cast iron were investigated under the same conditions. The result demonstrates that a little difference in hardness is found between Mn0-C (Mn-0wt% prepared by cast) and Mn0-PM (Mn-0wt% prepared by P/M). However, the wear resistance of Mn0-PM is better than Mn0-C due to the evenly distributed lubricating graphite. The wear resistance of P/M cast iron increases with the increase of Mn content which is attributed to the increased hardness. The corrosion behaviors for all the materials tested by using potentiodynamic polarization curves and electrochemical impedance spectroscopy (EIS) are almost the same, largely due to the formation of austenite matrix. Thereinto, Mn5-PM holds the best corrosion behavior with the lowest corrosion current density and highest polarization resistance. Because the potential difference between matrix and carbide is lower than that between matrix and graphite. The decreased graphite with the increased carbide induces a strong corrosion resistance in Mn5-PM.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Metal Alloys Wear and Properties · Microstructure and Mechanical Properties of Steels · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (27)

Show source-provided references
1. Effect of heat treatment parameters on abrasive wear and corrosion resistance of austenitic nodular cast iron Ni–Mn–Cu10.1016/j.acme.2017.08.001 ↗
2. Complex effects of alloy composition and porosity on the phase transformations and mechanical properties of powder metallurgy steels10.1016/j.powtec.2015.07.029 ↗
3. Green machining of powder-metallurgy-steels (PMS): an overview10.1016/j.jmapro.2019.05.009 ↗
4. Influence of residual porosity on the dry and lubricated sliding wear of a powder metallurgy austenitic stainless steel10.1016/j.wear.2015.01.025 ↗
5. Corrosion behaviours of stainless steel parts formed by powder metallurgy process10.1016/j.matpr.2017.10.138 ↗
6. Microstructure and wear behavior of a porous nanocrystalline nickel-free austenitic stainless steel developed by powder metallurgy10.1016/j.matdes.2009.10.008 ↗
7. Characteristic of the porous 316 stainless steel for the friction element of prosthetic joint10.1016/j.wear.2007.01.119 ↗
8. Effects of sintering pressure and temperature on microstructure and tribological characteristic of Cu-based aircraft brake material10.1016/S1003-6326(07)60154-X ↗
9. Effect of inoculation on microstructure, mechanical and corrosion properties of high manganese ductile Ni-resist alloy10.1016/j.matdes.2013.04.064 ↗
10. Improving intergranular corrosion resistance in a nickel-free and manganese-bearing high-nitrogen austenitic stainless steel through grain boundary character distribution optimization10.1016/j.corsci.2016.02.019 ↗
11. Wear behavior and subsurface layer work hardening mechanism of Fe-24.1Mn-1.21C-0.48Si steel10.1016/j.proeng.2017.10.990 ↗
12. Wear behavior and hardening mechanism of novel lightweight Fe-25.1Mn-6.6Al-1.3C steel under impact abrasion conditions10.1007/s11249-016-0751-2 ↗
13. A study of work hardening in austenitic Fe-Mn-C and Fe-Mn-Al-C alloys10.1016/0956-7151(92)90054-I ↗
14. A novel high manganese austenitic steel with higher work hardening capacity and much lower impact deformation than Hadfield manganese steel10.1016/j.matdes.2013.09.057 ↗
15. Manganese distribution and effect on graphite shape in advanced cast irons10.1016/j.matlet.2008.04.056 ↗
16. The effects of replacing Ni with Mn on hydrogen embrittlement in Cr-Ni-Mn-N austenitic steels10.1016/j.corsci.2019.03.012 ↗
17. Structure and high temperature wear characteristics of CVD coating on HEA bonded cermet10.1016/j.ceramint.2019.06.152 ↗
18. Effect of manganese additions and wear parameter on the tribological behaviour of NFGrey (8) cast Iron
19. Microstructure and mechanical properties of modified ductile Ni-resist with higher manganese content10.1016/j.msea.2013.02.038 ↗
20. Corrosion resistances and passivation of powder metallurgical and conventionally cast 316L and 2205 stainless steels10.1016/j.corsci.2012.10.021 ↗
21. Effect of thermo-mechanical processing on the low impact abrasion and low stress sliding wear resistance of austenitic high manganese steels10.1016/j.wear.2018.10.013 ↗
22. Effect of martensite content on friction and oxidative wear behavior of 0.42 Pct carbon Dual-phase steel10.1007/s11661-002-0335-7 ↗
23. Electrochemical study on the corrosion behaviour of a new low-nickel stainless steel in carbonated alkaline solution in the presence of chlorides10.1016/j.electacta.2014.02.107 ↗
24. Thermodynamics of the solid phases in the system Fe-Mn-C10.1007/BF02665426 ↗
25. High temperature phase stability and heat capacity of Fe-0.28Mn-0.55Si-0.045C magnetic alloy: a calorimetric study[J]10.1002/srin.201300456 ↗
26. Effect of Cu additions over the lattice parameter and hardness of the NiAl intermetallic compound[J]
27. Quantitative interpretation of X-Ray diffraction patterns of mixtures III. Simultaneous determination of a set of reference intensities10.1107/S0021889875009454 ↗