journal article·2021-09Open access

On the association between microhardness, corrosion resistance and microstructure of probeless friction stir spot welded Al–Li joint

Q. Chu, S.J. Hao, W.Y. Li, X.W. Yang, Y.F. Zou, D. Wu, A. Vairis

Abstract

The precipitation behavior and development of grain structure have been investigated to reveal their association with the microhardness and corrosion resistance of probeless friction stir spot welded (P-FSSW) joint of an Al–Li alloy. Results identified the primary strengthening phase of T1 (Al2CuLi) to be completely dissolved in the stir zone (SZ), while equiaxed grains were formed. Grain refinement was directly associated with the combined effect of continuous dynamic recrystallization and geometrized effect of imposed strain. However, as localized grain boundary bulging indicated, limited discontinuous recrystallization also participated in the microstructure evolution. The hardness dropped noticeably in the heat affected zone (HAZ) due to the weakening of precipitation and dislocation strengthening, which resulted from partial dissolution or coarsening of T1 phase and recovery effect. Grain refinement and solution strengthening were responsible for the slight increase in hardness of the SZ. In addition, the SZ had minute increased pitting resistance due to the homogenization of intermetallic particles, precipitate dissolution and refined grains.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced Welding Techniques Analysis · Aluminum Alloy Microstructure Properties · Aluminum Alloys Composites Properties

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (52)

Show source-provided references
1. Microstructural evolution and mechanical performance of Al-Cu-Li alloy joined by friction stir welding10.1016/j.jmrt.2020.10.008 ↗
2. Effect of micro morphology in different zones on mechanical properties of 2060 Al-Li alloy laser welded joints10.1016/j.jmapro.2019.12.032 ↗
3. The influence of Cu/Li ratio on precipitation in Al-Cu-Li-x alloys10.1016/j.actamat.2012.12.041 ↗
4. Impact of thermal management on post weld heat treatment efficacy in friction stir welded 2050-T3 alloy10.1016/j.jallcom.2017.06.141 ↗
5. The effect of minor solute additions on the precipitation path of an Al-Cu-Li alloy10.1016/j.actamat.2016.05.050 ↗
6. An effect of the rotation speed on microstructure and mechanical properties of the friction stir welded 2060-T8 Al-Li alloy10.1016/j.matchar.2016.11.011 ↗
7. Influence of dwell time on microstructure evolution and mechanical properties of dissimilar friction stir spot welded aluminum-copper metals10.1016/j.jmrt.2019.02.015 ↗
8. A newly developed tool without probe for friction stir spot welding and its performance10.1016/j.jmatprotec.2010.01.015 ↗
9. Effect of residual alclad on friction stir spot welds of AA2219 alloys10.3139/120.111245 ↗
10. The evolution of precipitation and microstructure in friction stir welded 2195-T8 Al-Li alloy10.1016/j.msea.2014.12.026 ↗
11. Friction stir welding of Al-Mg-Li 1424 alloy10.1016/j.matdes.2016.05.111 ↗
12. Microstructural evolution of 2099 Al-Li alloy during friction stir welding process10.1016/j.matchar.2016.11.045 ↗
13. Texture and microstructure evolution and mechanical properties during friction stir welding of extruded aluminum billets10.1016/j.msea.2013.12.087 ↗
14. Origin of unusual fracture in stirred zone for friction stir welded 2198-T8 Al-Li alloy joints10.1016/j.msea.2017.03.079 ↗
15. Fine-grain evolution in friction-stir processed 7050 aluminum10.1016/S1359-6462(03)00082-4 ↗
16. Friction stir weld of 2060 Al-Cu-Li alloy: microstructure and mechanical properties10.1016/j.jallcom.2015.02.124 ↗
17. Microstructure, texture and mechanical properties during refill friction stir spot welding of 6061-T6 alloy10.1016/j.matchar.2017.03.023 ↗
18. Texture development and material flow behavior during refill friction stir spot welding of AlMgSc10.1007/s11661-017-4381-6 ↗
19. Effect of welding temperature on microstructure of friction-stir welded aluminum alloy 105010.1007/s11661-014-2651-0 ↗
20. Microstructure, mechanical and corrosion behavior of additively manufactured steel: a review (part 1)10.3139/120.111507 ↗
21. Correlation between corrosion resistance, anodic hydrogen evolution and microhardness in friction stir weldment of AA2198 alloy10.1016/j.matchar.2018.07.004 ↗
22. Characterisation and understanding of the corrosion behaviour of the nugget in a 2050 aluminium alloy friction stir welding joint10.1016/j.corsci.2013.04.001 ↗
23. Study on localized corrosion mechanism of 2195 Al-Li alloy in 4.0% NaCi solution (ph 6.5) using a three-electrode coupling system10.1002/maco.200403824 ↗
24. Effect of friction spot welding (FSpW) on the surface corrosion behavior of overlapping AA6181/Ti-6Al-4V joints10.1016/j.matdes.2017.06.005 ↗
25. In-depth microscopic characterization of the weld faying interface revealing stress-induced metallurgical transformations during friction stir spot welding10.1016/j.ijmachtools.2021.103716 ↗
26. Pinless tool for FSSW of AA 6061-T6 aluminum alloy10.1016/j.jmatprotec.2018.12.005 ↗
27. Aging kinetics of friction stir welded Al-Cu-Li-Mg-Ag and Al-Cu-Li-Mg alloys10.1016/j.matdes.2016.07.126 ↗
28. Cooling effect on microstructure and mechanical properties during friction stir welding of Al-Mg-Si aluminum alloys10.1016/j.matlet.2016.05.157 ↗
29. Effect of different aging processes on the microstructure and mechanical properties of a novel Al-Cu-Li Alloy10.1016/j.jmst.2016.01.018 ↗
30. Correlation of microstructure and mechanical properties in friction stir welded 2198-T8 Al-Li alloy10.1016/j.msea.2015.05.038 ↗
31. Microstructure and mechanical optimization of probeless friction stir spot welded joint of an Al-Li alloy10.1016/j.jmst.2018.03.009 ↗
32. Microstructures and mechanical properties of Al-Li 2198-T8 alloys processed by two different severe plastic deformation methods: a comparative study10.1016/j.msea.2016.10.108 ↗
33. Microstructure, texture, and mechanical properties of friction stir welded commercial brass alloy10.1016/j.matchar.2016.07.009 ↗
34. Grain structure formation during friction stir welding observed by the ‘stop action technique’10.1016/j.actamat.2005.03.044 ↗
35. Texture development in friction stir welds10.1179/1362171811Y.0000000010 ↗
36. Role of the inter-pass cooling rate in recrystallization behaviors of Ni-based super alloy during interrupted hot compression10.1016/j.cja.2018.07.013 ↗
37. The effect of thermal exposure on the microstructure and mechanical properties of multiphase AlSi12Cu4MgNi2 alloy10.1016/j.matchar.2019.110032 ↗
38. Microstructural variation due to heat gradient of a thick friction stir welded aluminum 7449 alloy10.1016/j.jallcom.2017.04.147 ↗
39. Effects of the shoulder diameter and weld pitch on the tensile shear load in friction-stir welding of AA6111/AA5023 aluminum alloys10.1016/j.jmatprotec.2016.11.007 ↗
40. Effect of high volume fraction of B4C particles on the microstructure and mechanical properties of aluminum alloy based composites10.1016/j.jallcom.2013.04.141 ↗
41. Microstructural evolution and mechanical behavior of friction spot welded 2198-T8 Al-Li alloy during aging treatment10.1016/j.matdes.2016.11.045 ↗
42. A study on microstructure and mechanical properties of AA 3003 aluminum alloy joints by underwater friction stir welding10.1016/j.matchar.2017.01.039 ↗
43. Defect features, texture and mechanical properties of friction stir welded lap joints of 2A97 Al-Li alloy thin sheets10.1016/j.matchar.2017.01.038 ↗
44. Microstructure and morphology evolution of probeless friction stir spot welded joints of aluminum alloy10.1016/j.jmatprotec.2017.09.003 ↗
45. Localized alkaline corrosion of alloy AA5083 in neutral 3.5% NaCl Solution10.1016/S0010-938X(00)00166-9 ↗
46. Friction stir welding of Al alloy 2219-T8: Part II-mechanical and corrosion
47. Corrosion susceptibility of dissimilar friction stir welds of AA5083 and AA6082 alloys10.1016/j.matchar.2015.07.002 ↗
48. Effect of the electrolyte pH on the corrosion mechanisms of Zn-Mg coated steel10.1016/j.corsci.2016.02.041 ↗
49. Corrosion characteristics of cold gas spray coatings of reinforced aluminum deposited onto carbon steel10.1016/j.corsci.2016.10.019 ↗
50. Corrosion behavior of friction stir welded lean duplex stainless steel10.1016/j.matdes.2014.10.060 ↗
51. The influence of artificial ageing on the corrosion behaviour of a 2050 aluminium-copper-lithium alloy10.1016/j.corsci.2013.11.060 ↗
52. Corrosion behavior of friction stir welded 2A97 Al-Cu-Li alloy10.5006/2418 ↗