journal article·2021-09Open access

Characteristics of powdered layer on silicone rubber surface

Tian Liang, Zhijin Zhang, Xiaohong Ma, Yingzhu Xiang, Huan Huang, Xingliang Jiang

Abstract

In recent years, varying degrees of surface pulverization had been found on composite insulators running for years in severe outdoor environment such as dry, high altitude, salt fog and intensive ultraviolet radiation. Research on the basic characteristics of powdered substance is essential to maintain a high reliability of the power grid. In this study, the characteristics of the powdered layer of the composite insulator sheds aged for more than 10 years under three different environmental stresses are analyzed. The results show that powdered substance of each composite insulator sample contains two parts: the organic silicon which is oxidative degradation product of the original material polydimethylsiloxane (PDMS), and the partially dehydrated and deteriorated flame retardant filler aluminum hydroxide (ATH). However, the thickness of the powdered layer, the particle size distribution of the powdered substance and the composition ratio between the two components are different. The average particle size of powdered substance is between 2–7 μm. The content of Al element is 31.8–34.5%, the content of Si element is 12.7–17.5%, and the mass fraction ratio of two types of powdered substance is about 1/2–1/3. The essence of pulverization is finally concluded that the composite insulator is severely oxidized and degraded under the effect of various aging factors. The organic component silicone rubber is decomposed to fragments, and the bonding between inorganic flame retardant filler and polymer become weak. They will be detached from the main body skeleton and lost partly, then build up at the surface, forming powdered layer.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: High voltage insulation and dielectric phenomena · Aerosol Filtration and Electrostatic Precipitation · Lightning and Electromagnetic Phenomena

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (17)

Show source-provided references
1. Design and testing of an improved profile for silicone rubber composite insulators10.1109/TDEI.2017.006170 ↗
2. Development of composite insulators in China10.1109/94.798115 ↗
3. Outdoor HV composite polymeric insulators10.1109/TDEI.1999.9286745 ↗
4. Review of aging and recovery of silicone rubber insulation for outdoor use10.1109/TDEI.1999.9286749 ↗
5. Degradation of silicone rubber under AC or DC voltages in radiation environment10.1109/TDEI.2009.5128524 ↗
6. Aging evaluation of silicone rubber insulators using leakage current and flashover voltage analysis10.1109/TDEI.2013.6451360 ↗
7. Moisture absorption, desorption, and moisture-induced electrical performances of high-temperature vulcanized silicone rubber10.1109/TDEI.2015.005452 ↗
8. Moisture induced local heating of overhead line composite insulators10.1109/TDEI.2016.005791 ↗
9. A new approach to anti-fog design for polymeric insulators10.1109/TDEI.2010.5448087 ↗
10. A basic study on the effect of voltage stress on a water droplet on a silicone rubber surface10.1109/TDEI.2009.4784558 ↗
11. Electric field analysis of water drop corona10.1109/TPWRD.2004.837672 ↗
12. Modern outdoor insulation-concerns and challenges10.1109/MEI.2005.1541483 ↗
13. The aging characteristics of composite insulators under salt fog conditions
14. Additional salt deposit density of polluted insulators in salt fog10.1049/iet-gtd.2015.1387 ↗
15. Ageing of silicone rubber insulators in coastal and inland tropical environment10.1109/TDEI.2010.5448085 ↗
16. Effects of AC and DC corona on the surface properties of silicone rubber: characterization by contact angle measurements and XPS high resolution scan10.1109/TDEI.2017.006774 ↗
17. Micro characterization and degradation mechanism of liquid silicone rubber used for external insulation10.1109/TDEI.2014.004188 ↗