Effects of Cu-alloying in minute quantities on the corrosion-induced mechanical degradation behaviors of medium C-based ultrahigh-strength steel in aqueous environments

Sung Jin Kim, Jin Sung Park, Hwan Goo Seong

Abstract

This study examined the applicability of Cu-alloying in minute quantities to medium C-based ultrahigh-strength automotive steel with a tensile strength of more than 2000 MPa to improve the resistance to mechanical degradation caused by aqueous corrosion. Cu-alloying of this steel favored the precipitation of fine-(Ti,Mo)C particles, leading to a smaller prior-γ grain size (PAGS) and inter-lath size, resulting in higher tensile strain. In addition, Cu-alloyed steel showed the surface inhibiting characteristics in a neutral aqueous condition based on higher corrosion resistance (i.e., larger polarization resistance and less weight loss). The smaller particle size of corrosion scale (CuxFe3-xO4), more uniform surface roughness, and smaller PAGS can be the major mechanistic reasons for suppressing the reduction in the mechanical properties of Cu-alloyed ultrahigh-strength steel in the corrosive environment.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Hydrogen embrittlement and corrosion behaviors in metals · Corrosion Behavior and Inhibition · Microstructure and Mechanical Properties of Steels

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (47)

Show source-provided references
1. Reducing vehicle weight and improving U.S. energy efficiency using integrated computational materials engineering
2. Advanced lightweight materials and manufacturing processes for automotive applications10.1557/mrs.2015.268 ↗
3. A review on applications of carbon nanotubes in automobiles
4. Effect of carbon nanotube dispersion on mechanical properties of aluminum-silicon alloy matrix composites10.1007/s11665-013-0835-1 ↗
5. Effect of increasing the strength of aluminum matrix nanocomposites reinforced with microadditions of multiwalled carbon nanotubes coated with TiC nanoparticles10.3390/nano9111596 ↗
6. Hydride cellulose-glass fiber composites for automotive applications10.3390/ma12193189 ↗
7. An overview on joining of aluminium and magnesium alloys using friction stir welding (FSW) for automotive lightweight applications10.1088/2053-1591/ab3262 ↗
8. Ultrafine pearlitic transformation behavior of 2000 MPa ultra-high-strength steel wire under Nb microalloying
9. Effect of heat treatment conditions on corrosion and hydrogen diffusion behaviors of ultra-strong steel used for automotive applications
10. One-step quenching and partitioning heat treatment of medium carbon low alloy steel10.1007/s11665-014-0902-2 ↗
11. Mechanical properties and nanoparticles precipitation behavior of multi-component ultra high strength steel10.1016/j.matdes.2020.108637 ↗
12. Co-precipitation of nanoscale particles in steel with ultra-high strength for a new area10.1016/j.mattod.2016.07.002 ↗
13. Effect of particle size on mechanical properties of a TiC containing tool steel by hot isostatic press10.2320/matertrans.MER2007262 ↗
14. Effect of alloying elements (C, Mo) on hydrogen assisted cracking behaviors of A516-65 steels in sour environments10.3390/ma13184188 ↗
15. Cathodic evolution of hydrogen on carbides of iron-family metals
16. Effect of hydrogen in advanced high strength steel materials10.1016/j.ijhydene.2019.08.149 ↗
17. The effect of low-quantity Cr addition on the corrosion behavior of dual-phase high carbon steel10.3390/met8040199 ↗
18. Effect of chromium on the corrosion behavior of low alloy steel in sulfuric acid10.1007/s12540-012-6009-0 ↗
19. The effect of nickel content on the environmental assisted cracking (EAC) behavior of low alloy steels in sour environment-A review10.1016/0308-0161(92)90117-X ↗
20. Effect of Cr, Ni and Cu on the corrosion behavior of low carbon microalloying steel in a Cl- containing environment10.1016/j.jmst.2012.12.013 ↗
21. Influence of plastic deformation and Cu addition on corrosion of carbon steel in acidic aqueous solution10.1016/j.corsci.2019.108122 ↗
22. Effect of copper content of carbon steel on corrosion in sulfuric acid10.5006/0010-9312-21.1.9 ↗
23. Effect of the addition of Cu and Ni on the corrosion behavior of weathering steels in corrosive industrial environments10.1007/s11665-020-04738-5 ↗
24. Five-year atmospheric corrosion of Cu, Cr and Ni weathering steels in a wide range of environments10.1016/j.corsci.2018.06.039 ↗
25. May · 1982
26. Knowledge of the corrosion process of copper-bearing steels
27. Tomashov · 1968 · 367
28. On the atmospheric corrosion of metals which are covered with thin electrolyte layers-Ⅰ. Verification of the experimental technique10.1016/0010-938X(90)90032-Z ↗
29. The influence of microstructure on the corrosion rate of various carbon steel10.1007/s10800-004-6207-7 ↗
30. 2013
31. Effect of carbon contents on corrosion and hydrogen diffusion behaviors of ultra-strong steels for automotive applications10.3365/KJMM.2018.56.8.570 ↗
32. Study on the controlling factors for the quenching crack sensitivity of ultra-strong automotive steel10.1007/s10853-019-04177-1 ↗
33. A mechanistic study on the hydrogen trapping property and the subsequent electrochemical corrosion behavior of quenched and tempered steel10.1016/j.ijhydene.2018.07.187 ↗
34. Inhibiting hydrogen embrittlement in ultra-strong steels for automotive application by Ni-alloying10.1038/s41529-019-0074-5 ↗
35. Behavior of copper and nickel during high temperature oxidation of steel containing them10.4028/www.scientific.net/MSF.522-523.53 ↗
36. Influence of Ni and Cu on oxide-scale structure of steel10.1149/08502.0013ecst ↗
37. Strengthening from Cu addition in 0.2C-(1-2)Mn steels during tempering10.3390/ma12020247 ↗
38. Effect of copper on tensile properties and grain-refinement of steel and it relation to precipitation behavior10.2320/matertrans.45.2239 ↗
39. The role of prior austenite grains in fatigue cracking initiation and propagation in low carbon martensite10.1111/j.1460-2695.1979.tb01083.x ↗
40. Effect of morphology of copper precipitation particles on hydrogen embrittlement behavior in Cu-added ultra low carbon steel10.2320/matertrans.43.2213 ↗
41. Polarization resistance method for determination of instantaneous corrosion rates10.5006/1.3280536 ↗
42. Jones · 1996
43. Corrosion behavior of a quenched and partitioned medium carbon steel in 3.5 wt.% NaCl solution10.1016/j.corsci.2017.10.027 ↗
44. Composition and protective ability of rust layer formed on weathering steel exposed to various environments10.1016/j.corsci.2005.10.004 ↗
45. Microstructural and corrosion characteristics of Al-Fe alloys produced by high-frequency induction-sintering process10.3390/coatings9100686 ↗
46. Influence of Cu on nanostructure of Fe3O4 particles10.1002/maco.201910794 ↗
47. Influence of Fe3O4 particle size on corrosion of carbon steel under wet/dry cyclic conditions10.1002/maco.201810337 ↗