Influence of welding sequences on the microstructure and mechanical properties of dual-pass electron beam welded Ti60/V/Cu/GH3128 joints
Source abstract
Abstract
Electron beam welding of Ti60 titanium alloy to GH3128 nickel-base superalloy was realized by using V/Cu composite interlayers, based on the element metallurgical compatibility. The effects of welding sequences on the microstructures and properties of the joints were analyzed. Microstructures and energy spectrum analysis shown that the reaction of Ti and Ni atoms to form brittle intermetallic compounds (IMC) can be effectively prevented by the interlayers. When the electron beam was first focused on the V foil, the copper foil was melted due to the high melting point of vanadium (1890 °C). Continuously distributed CuTi IMCs were produced near the Ti60 side. When the electron beam was first focused on the Cu foil, CuTi IMCs were replaced by the formation of (Ti,V) solid solutions at the interface of Ti60. A joint with a maximum tensile strength of 392 MPa, 49% of that of the GH3218 alloy was obtained. The fracture morphology proved that the fracture type belonged to brittle fracture.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced Welding Techniques Analysis · Welding Techniques and Residual Stresses · Intermetallics and Advanced Alloy Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (29)
Show source-provided references
1. Pulsed laser welding of Ti-6Al-4V titanium alloy to AISI 316L stainless steel using Cu/Nb bilayer10.1016/j.matlet.2019.02.075 ↗
2. Two pass laser welding of TC4 Titanium alloy to 301L stainless steel via pure v interlayer10.1016/j.jmrt.2019.11.066 ↗
3. Electrochemical deep grinding of cast nickel-base superalloys10.1016/j.jmapro.2019.10.007 ↗
4. Comparison on grindability and surface integrity in creep feed grinding of GH4169, K403, DZ408 and DD6 nickel-based superalloys10.1016/j.jmapro.2019.11.027 ↗
5. Microstructure and mechanical properties of electron beam welded joints of tantalum and GH312810.1016/j.msea.2019.138431 ↗
6. Phase formation in Ti/Ni dissimilar welds10.1016/j.msea.2007.12.041 ↗
7. Weld deposition of nickel on titanium for surface hardening with Ti-Ni-based intermetallic compounds
8. Analysis of embrittlement of Ti60 and GH3128 electron beam welded joint
9. Fibre laser welding of dissimilar alloys of Ti-6Al-4V and Inconel 718 for aerospace applications10.1007/s00170-010-2791-3 ↗
10. Two pass laser welding of TC4 titanium alloy and 304 stainless steel using TA2/Q235 composite interlayer
11. Laser welding of Ti6Al4V to Cu using a niobium interlayer10.1016/j.jmatprotec.2019.03.005 ↗
12. Microstructural characteristics and mechanical properties of an electron beam-welded Ti/Cu/Ni joint10.1007/s11665-018-3325-7 ↗
13. The formation of intermetallics in Ti/steel dissimilar joints welded by Cu-Nb composite filler10.1016/j.jallcom.2020.154389 ↗
14. Diffusion bonding of hydrogenated TC4 alloy and GH3128 superalloy using composite interlayers10.1016/j.jmatprotec.2019.116266 ↗
15. Current research and development status of dissimilar materials laser welding of titanium and its alloys10.1016/j.optlastec.2020.106090 ↗
16. Nd:YAG pulsed laser welding of TC4 Ti alloy to 301L stainless steel using Ta/V/Fe composite interlayer10.1016/j.matlet.2017.10.057 ↗
17. Benefits of interfacial regulation with interlayers in laser welding Ti6Al4V/316L steel10.1016/j.optlastec.2019.106007 ↗
18. Microstructure and mechanical properties of vacuum diffusion bonded joints between Ti-6Al-4V titanium alloy and AISI316L stainless steel using Cu/Nb multi-interlayer10.1016/j.vacuum.2017.08.017 ↗
19. Interlayer thickening for development of laser-welded Ti-SS joint strength10.1016/j.optlastec.2018.11.022 ↗
20. Three-pass laser welding of Ti alloy-stainless steel using Nb and Ni interlayers10.1016/j.jmrt.2019.12.009 ↗
21. Microstructure and mechanical properties of laser welding of Ti6Al4V to Inconel 718 using Nb/Cu interlayer10.1016/j.jmatprotec.2019.116467 ↗
22. 1992
23. Elimination of hot cracking in the electron beam welding of AA2024-T351 by controlling the welding speed and heat input10.1016/j.jmapro.2019.09.003 ↗
24. Microstructural characterization and mechanical performance of Al–Cu–Li alloy electron beam welded joint10.1016/j.ast.2018.08.030 ↗
25. Effect of heat input on microstructure and mechanical properties of Ti/Cu66V34/Cu joints by electron beam welding10.1016/j.jmapro.2019.07.005 ↗
26. Effect of filler metal composition on microstructure and mechanical properties of electron beam welded titanium/copper joint10.1016/j.jallcom.2018.10.222 ↗
27. Effect of Cu66V34 filler thickness on the microstructure and properties of titanium/copper joint by electron beam welding10.1016/j.jmatprotec.2018.12.013 ↗
28. High strength electron beam welded titanium-stainless steel joint with V/Cu based composite filler metals10.1016/j.vacuum.2013.01.015 ↗
29. Forming mechanism and mechanical property of pulsed laser welded Ti alloy and stainless steel joint using copper as interlayer10.1016/j.jmrt.2019.11.068 ↗