Effects of bonding pressures on microstructure and mechanical properties of silver–tin alloy powders synthesized by ball milling for high-power electronics packaging
Source abstract
Abstract
Silver (Ag) sintering is widely adopted as a die attach method for power electronics packaging. However, oxidation, massive grain growth, and increasing porous structure occur in sintered Ag joints at high temperatures, resulting in decreasing mechanical properties of the die attachment in power devices. To solve the problems of sintered Ag joints, a novel die attach material consisting of silver–tin (Ag–Sn) alloy particles is developed in this study. Ag–Sn alloy powders were newly fabricated by high-energy ball milling technique. The microstructural evolutions of the Ag–Sn alloy joints bonded at different pressures were systematically analyzed. With increasing high-temperature storage time at 300 °C, the reactions between sintered Ag–Sn alloy joints and Cu substrates increased, which resulted in the formation of Cu3Sn or Ag-rich diffusion layer. The relationships between microstructures and the formation of each phase were discussed. In addition, the robust sintered Ag–Sn alloy joints exhibited low porosity without pore coarsening and limit oxidation at high temperatures, indicating a dense and stable microstructure of sintered Ag–Sn alloy joints. As a result, high bonding strength did not deteriorate even after high-temperature storage for 2000 h. It is concluded that the novel Ag–Sn alloy paste produced by high-energy ball milling has long-term high-temperature reliability to be used as a die attach material for the power electronics packaging, thus enabling high-power devices to have higher operating temperatures and thermal stability.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · 3D IC and TSV technologies · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (54)
Show source-provided references
1. Performance evaluation of high-power SiC MOSFET modules in comparison to Si IGBT modules10.1109/TPEL.2018.2834345 ↗
2. The changing automotive environment: high-temperature electronics10.1109/TEPM.2004.843109 ↗
3. A review on die attach materials for SiC-based high-temperature power devices10.1007/s11663-010-9365-5 ↗
4. High temperature mechanical behavior of SAC and SAC+X lead free solders
5. Off-eutectic Au–Ge die-attach—microstructure, mechanical strength, and electrical resistivity10.1109/TCPMT.2019.2926528 ↗
6. High temperature interconnect and die attach technology: Au–Sn SLID bonding10.1109/TCPMT.2013.2253353 ↗
7. Highly reliable high-temperature superplastic Al-Zn eutectoid solder joining with stress relaxation characteristics for next generation SiC power semiconductor devices
8. High melting Pb-free solder alloys for die-attach applications10.1002/adem.200500124 ↗
9. Siow · 2019 · 1
10. High-temperature lead-free solder alternatives10.1016/j.mee.2010.12.072 ↗
11. Die attach materials for high temperature applications: a review10.1109/TCPMT.2010.2100432 ↗
12. Koch · 2006
13. Thermal behavior of silver nanoparticles for low-temperature interconnect applications10.1007/s11664-005-0229-8 ↗
14. Review on joint shear strength of nano-silver paste and its long-term high temperature reliability10.1007/s11664-014-3202-6 ↗
15. Low-temperature and pressureless sinter joining of Cu with micron/submicron Ag particle paste in air10.1016/j.jallcom.2018.11.251 ↗
16. Microstructural studies and bonding strength of pressureless sintered nano-silver joints on silver, direct bond copper (DBC) and copper substrates aged at 300 °C10.1016/j.jallcom.2016.06.132 ↗
17. High-temperature reliability of low-temperature and pressureless micron Ag sintered joints for die attachment in high-power device10.1007/s10854-018-8903-9 ↗
18. Microstructural and mechanical evolution of silver sintering die attach for SiC power devices during high temperature applications10.1016/j.jallcom.2018.10.067 ↗
19. Influence of thermal exposure upon mechanical/electrical properties and microstructure of sintered micro-porous silver10.1016/j.microrel.2018.07.048 ↗
20. Ageing sintered silver: relationship between tensile behavior, mechanical properties and the nanoporous structure evolution10.1016/j.msea.2016.05.108 ↗
21. Enhancement of nano-silver chip attachment by using transient liquid phase reaction with indium10.1016/j.jallcom.2018.05.254 ↗
22. Low-pressure micro-silver sintering with the addition of indium for high-temperature power chips attachment10.1016/j.jmrt.2021.10.079 ↗
23. Recent progress in transient liquid phase and wire bonding technologies for power electronics10.3390/met10070934 ↗
24. Overview of transient liquid phase and partial transient liquid phase bonding10.1007/s10853-011-5561-1 ↗
25. Nickel-tin transient liquid phase bonding toward high-temperature operational power electronics in electrified vehicles10.1109/TPEL.2012.2212211 ↗
26. Interfacial reaction in Cu/Sn/Cu system during the transient liquid phase soldering process10.1016/j.actamat.2010.10.053 ↗
27. Low temperature transient liquid phase bonding of Au/Sn and Cu/Sn electroplated material systems for MEMS wafer-level packaging10.1007/s00542-012-1708-5 ↗
28. Transient liquid phase die attach for high-temperature silicon carbide power devices10.1109/TCAPT.2010.2046901 ↗
29. Enhanced pressureless bonding by tin doped silver paste at low sintering temperature10.1016/j.msea.2016.02.082 ↗
30. Ag-Sn bimetallic nanoparticles paste for high temperature service in power devices10.1088/1361-6528/ab92cd ↗
31. Tin nanoparticles modified nano-silver paste for pressureless low-temperature sintering process
32. Influence of process parameters on SAC305 lead-free solder powder produced by centrifugal atomization10.1016/j.powtec.2011.09.015 ↗
33. Microstructures and properties of silver-based contact material fabricated by hot extrusion of internal oxidized Ag–Sn–Sb alloy powders10.1016/j.msea.2012.01.031 ↗
34. Internal oxidation of rapidly solidified silver-tin-indium alloy powders10.1007/BF00541633 ↗
35. Electrodeposition of Ni, Co and Ni–Co alloy powders10.1016/j.electacta.2006.02.022 ↗
36. Ag–Cu bimetallic nanoparticles with enhanced resistance to oxidation: a combined experimental and theoretical study10.1021/jp506069c ↗
37. Ag@Sn core-shell powder preform with a high Re-melting temperature for high-temperature power devices packaging10.1002/adem.201700524 ↗
38. Development of Ag–in alloy pastes by mechanical alloying for die attachment of high-power semiconductor devices10.3390/ma15041397 ↗
39. 2010
40. Effect of stearic acid coating on anti-oxidation property of Sn-Ag-Cu solder powder10.1108/SSMT-08-2018-0021 ↗
41. XXIX. Factors affecting the limit of solubility of elements in copper and silver10.1080/14786443908562230 ↗
42. A first report on sintering diagrams10.1016/0001-6160(74)90167-9 ↗
43. Coarsening in sintering: grain shape distribution, grain size distribution, and grain growth kinetics in solid-pore systems10.1080/10408436.2010.525197 ↗
44. Effect of trace elements on recrystallization temperature of silver10.2472/jsms.30.556 ↗
45. Stored energy and recrystallization temperature of rolled copper and silver single crystals with defined solute contents10.1016/0001-6160(79)90176-7 ↗
46. Influences of temperature and Sn-addition on microstructural evolution of Ag during FSW10.1080/13621718.2019.1665859 ↗
47. Rollett · 2017
48. Kang · 2004
49. Characterizations of a proposed 3300-V press-pack IGBT module using nanosilver paste for high-voltage applications10.1109/JESTPE.2018.2820046 ↗
50. Oxidation mechanism of thin Cu films: a gateway towards the formation of single oxide phase10.1063/1.5028407 ↗
51. 2010
52. Computational measurement of void percolation thresholds of oblate particles and thin plate composites10.1063/1.4730333 ↗
53. 2010
54. Structure and hardness of nanocrystalline silver10.1023/A:1018566303784 ↗