Complete fine-equiaxed β-columnar grains in laser direct energy deposition of Ti–6Al–4V parts
Source abstract
Abstract
Coarse β-columnar grains are often present in Ti-6Al-4V laser-additive-manufactured samples, resulting in anisotropic and inferior fatigue performance under dynamic loading. Fine-equiaxed grains (FEGs) with a mean grain size of approximately 139 μm were successfully obtained by a novel deposition strategy through coordinated regulation of direct energy deposition technological parameters. Microstructures were transformed from α' martensite to α'' martensite. As a result, the comprehensive performance was significantly improved. Without the use of an argon atmosphere glovebox and post heat treatment, the tensile strength and elongation in the horizontal direction of the FEGs were 1091 MPa and 4.09%, respectively. The corrosion resistance was 11.71-fold higher than that of the coarse columnar grains (CCGs). Improving the microstructure and performance by optimizing pulsed laser parameters is simple, effective, and conducive to online regulation of the quality of laser additive samples.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · High Entropy Alloys Studies · Additive Manufacturing and 3D Printing Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (28)
Show source-provided references
1. Designing against phase and property heterogeneities in additively manufactured titanium alloys10.1038/s41467-022-32446-2 ↗
2. Columnar to equiaxed grain transition of laser deposited Ti6Al4V using nano-sized B4C particles10.1016/j.compositesb.2021.108667 ↗
3. Influence of trace boron addition on microstructure, tensile properties and their anisotropy of Ti6Al4V fabricated by laser directed energy deposition10.1016/j.matdes.2019.107943 ↗
4. In situ design of advanced titanium alloy with concentration modulations by additive manufacturing10.1126/science.abj3770 ↗
5. The potential for grain refinement of Wire-Arc Additive Manufactured (WAAM) Ti-6Al-4V by ZrN and TiN inoculation
6. Grain structure control during metal 3D printing by high-intensity ultrasound10.1038/s41467-019-13874-z ↗
7. Application of bulk deformation methods for microstructural and material property improvement and residual stress and distortion control in additively manufactured components10.1016/j.scriptamat.2016.10.031 ↗
8. In-situ grain structure control in directed energy deposition of Ti6Al4V, Addit
9. Additive manufacturing of strong and ductile Ti–6Al–4V by selective laser melting via in situ martensite decomposition10.1016/j.actamat.2014.11.028 ↗
10. Melt-pool motion, temperature variation and dendritic morphology of Inconel 718 during pulsed- and continuous-wave laser additive manufacturing: a comparative study10.1016/j.matdes.2017.01.065 ↗
11. Influences of pulse laser parameters on properties of AISI316L stainless steel thin-walled part by laser material deposition10.1016/j.optlastec.2016.12.021 ↗
12. Microstructure and properties of Ti-6Al-4V fabricated by low-power pulsed laser directed energy deposition10.1016/j.jmst.2019.05.008 ↗
13. Isotropic and improved tensile properties of Ti-6Al-4V achieved by in-situ rolling in direct energy deposition
14. Grain refining of Ti-6Al-4V alloy fabricated by laser and wire additive manufacturing assisted with ultrasonic vibration10.1016/j.ultsonch.2021.105472 ↗
15. Anisotropic tensile behavior of Ti–6Al–4V components fabricated with directed energy deposition additive manufacturing10.1016/j.actamat.2014.12.054 ↗
16. Effects of melt pool variables and process parameters in laser direct metal deposition of aerospace alloys10.1080/10426914.2010.480999 ↗
17. Heat-affected coarsening of β grain in titanium alloy during laser directed energy deposition10.1016/j.scriptamat.2021.114180 ↗
18. The effect of deformation-induced transformation on the fracture toughness of commercial titanium alloys10.1007/BF02672590 ↗
19. Effect of post heat treatment on microstructure and mechanical properties of Ti-6Al-4V jointing parts proceeded by laser additive manufacturing10.1016/j.msea.2020.139544 ↗
20. 3D printing of large-scale components of titanium alloys under open atmosphere
21. Tensile properties and microstructures of laser-formed Ti-6Al-4V10.1007/s11665-010-9670-9 ↗
22. Microstructure, static properties, and fatigue crack growth mechanisms in Ti-6Al-4V fabricated by additive manufacturing: LENS and EBM10.1016/j.engfailanal.2016.05.036 ↗
23. In-situ investigation of the anisotropic mechanical properties of laser direct metal deposition Ti6Al4V alloy10.1016/j.msea.2017.11.106 ↗
24. Fabrication of Ti-6Al-4V scaffolds by direct metal deposition10.1007/s11661-008-9634-y ↗
25. Laser fabrication of Ti6Al4V/TiC composites using simultaneous powder and wire feed10.1016/j.msea.2006.09.093 ↗
26. Yielding nature and Hall-Petch relationships in Ti-6Al-4V alloy with fully equiaxed and bimodal microstructures10.1016/j.scriptamat.2019.07.015 ↗
27. Quantitatively analyzing strength contribution vs grain boundary scale relation in pure titanium subjected to severe plastic deformation10.1007/s11661-016-3391-0 ↗
28. The anisotropic corrosion behaviour of wire arc additive manufactured Ti-6Al-4V alloy in 3.5% NaCl solution10.1016/j.corsci.2018.03.047 ↗