Powder-metallurgy fabrication of ZrB2–hardened Zr3Al2 intermetallic composites by high-energy ball-milling and reactive spark-plasma sintering
Source abstract
Abstract
A powder metallurgy route combining high-energy ball-milling (HEBM) of elemental powders and reactive spark-plasma sintering (SPS) is proposed for the controlled fabrication of novel composites based on a Zr–Al intermetallic matrix hardened with a ceramic second-phase. As proof-of-concept, its suitability is demonstrated on ZrB2–hardened Zr3Al2. Specifically, commercially available powders of ZrH2, Al, and B were first combined in molar ratios of 2:1:1 to give an intermetallic–ceramic composite nominally formed by ∼76.8 vol.% Zr3Al2 plus 23.2 vol.% ZrB2, and were intimately mixed and mechanically activated by HEBM in the form of dry shaker milling for 30 min, next identifying by a dilatometric SPS test at 50 MPa pressure that the densification window of these composites is ∼975–1275 °C. Subsequent densification SPS tests at 50 MPa pressure in that temperature interval, and also at 1350 °C, plus the microstructural and mechanical characterisations of the resulting materials, established 1175 °C as the optimal SPS temperature. It was also identified that densification takes place by transient liquid-phase sintering with molten Al, and that it occurs gradually, not abruptly, because most molten Al disappears in a flash by reacting with Zr to form in situ the intermetallic. It is also shown that the combination of HEBM plus reactive SPS yields Zr3Al2+ZrB2 composites with fine-grained microstructures formed essentially by multitudinous ZrB2 nanograins dispersed within a matrix of submicrometre, or nearly submicrometre, Zr3Al2 grains. Importantly, these intermetallic–ceramic composites were found to be very hard (i.e., ∼11.5 GPa), attributable to the hardening provided by the ZrB2 nanograins, and fairly tough (i.e., ∼4.5 MPa·m1/2), and therefore potential candidate materials for a multitude of structural–tribological applications. Finally, implications for future study are discussed.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · MXene and MAX Phase Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. Stability, elastic properties and electronic structures of the stable Zr–Al intermetallic compounds: a first-principles investigation10.1016/j.jallcom.2013.12.079 ↗
2. Intermetallics in the Zr–Al diffusion zone10.1016/j.intermet.2003.09.002 ↗
3. Schulson · 1994 · vol. 2
4. Cryo-rolling enhanced inhomogeneous deformation and recrystallization grain growth of a zirconium alloy10.1016/j.jallcom.2016.12.300 ↗
5. Microstructures and mechanical properties of Zr–Al binary alloys processed by hot-rolling10.1016/j.msea.2019.138723 ↗
6. Studies on hot hardness of Zr and its alloys for nuclear reactors10.1016/S0022-3115(98)00610-2 ↗
7. Cryo-rolling enhanced inhomogeneous deformation and recrystallization grain growth of a zirconium alloy10.1016/j.jallcom.2016.12.300 ↗
8. Microstructure and mechanical properties of as-cast Zr–Nb alloys10.1016/j.actbio.2011.07.020 ↗
9. Coefficients of thermal expansion for zirconium10.1007/BF03398344 ↗
10. The Al–Zr (aluminum–zirconium) system10.1007/BF02667556 ↗
11. PM processing and characterization of Ti–7Fe low cost titanium alloys10.1179/174329009X457063 ↗
12. Densification of ZrB2–based composites and their mechanical and physical properties: a review10.1016/j.jeurceramsoc.2008.11.008 ↗
13. Mechanical alloying and milling10.1016/S0079-6425(99)00010-9 ↗
14. On the crystallite size refinement of ZrB2 by high-energy ball-milling in the presence of SiC10.1016/j.jeurceramsoc.2011.05.035 ↗
15. On the enhancement of the spark-plasma sintering kinetics of ZrB2–SiC powder mixtures subjected to high-energy co-ball-milling10.1016/j.ceramint.2012.11.001 ↗
16. Spark-plasma-sintering kinetics of ZrC–SiC powder mixtures subjected to high-energy co-ball-milling10.1016/j.ceramint.2013.04.033 ↗
17. Effect of high-energy ball-milling on the spark plasma sinterability of ZrB2 with transition metal disilicides10.1016/j.jeurceramsoc.2020.06.046 ↗
18. Fabrication of ultrafine-grained ZrC–Co cemented carbides with superior sliding-wear resistance from micrometre starting powders10.1016/j.ceramint.2021.05.209 ↗
19. High-strength ZrB2–based ceramics prepared by reactive pulsed electric current sintering of ZrB2–ZrH2 powders10.1016/j.jeurceramsoc.2012.02.035 ↗
20. German · 1996
21. X-ray diffraction analysis of a severely plastically deformed aluminum alloy10.1016/j.actamat.2004.01.012 ↗
22. In situ formation of ZrB2–ZrO2 ultra-high-temperature ceramic composites from high-energy ball-milled ZrB2 powders10.1016/j.jallcom.2011.12.102 ↗
23. A study of the oxidation of ZrB2 powders during high-energy ball-milling in air10.1016/j.ceramint.2011.11.058 ↗
24. Mechanical behavior of cordierite and cordierite–mullite materials evaluated by indentation techniques10.1016/S0955-2219(00)00334-4 ↗
25. Sintering, hardness and indentation fracture toughness (KIC) of mullite and its composite with 15 wt% X-phase sialon10.1016/0955-2219(94)90033-7 ↗
26. Cemented carbide microstructures: a review10.1016/j.ijrmhm.2018.12.004 ↗