journal article·2024-03Open access

Research on B2O3–NaF–SiO2 fluxes for improved fusion defects and mechanical properties of A7N01 alloy with unequal thickness

Ning Cui, Yaojie Chao, Yu Tang, Qian Luo, Desheng Li, Sitong Zang, Hai Lin

Abstract

In the aerospace industry, the additive manufacturing of aluminum alloys has encountered significant challenges owing to fusion defects. In this work, the B2O3–NaF–SiO2 fluxes are employed for the first time to improve the fusion defects and mechanical properties of butt-welded A7N01 alloy with unequal thickness under natural ageing. The finite element analysis (FEA) approach is used to account for the evolution mechanism of residual stresses. The simulated results indicate that the distribution and values of residual compressive stresses are improved, which contribute to the microhardness. After applying a coating-position optimization of the B2O3–NaF–SiO2 fluxes, the fluxes plays a role in enhancing the welding current density and increasing the concentration of oxygen elements. The melt pool morphology and the fusion defect of the thicker side are ameliorated, resulting in a considerable increase in the yield strength and the tensile strength. Therefore, this paper establishes the viability of applying B2O3–NaF–SiO2 fluxes for additive manufacturing of A7N01 aluminum alloys and provides new ideas for exploring the optimal active fluxes of other 7xxx series aluminum alloys.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Fusion materials and technologies · Advanced materials and composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (66)

Show source-provided references
1. Revisiting stress-corrosion cracking and hydrogen embrittlement in 7xxx-Al alloys at the near-atomic-scale10.1038/s41467-022-31964-3 ↗
2. Fatigue life improvement of mig welded aluminium T-joints by friction stir processing10.1016/j.ijfatigue.2013.11.004 ↗
3. Improving the fatigue strength of A7N01 aluminum alloy by adjusting Si content10.1016/j.msea.2018.10.085 ↗
4. Effect of heat treatments on the tensile strength and SCC-resistance of AA7050 in an alkaline saline solution10.1016/j.corsci.2005.11.009 ↗
5. A comparative study on mechanical performance of traditional and magnetically assisted resistance spot welds of A7N01 aluminum alloy10.1016/j.jmapro.2021.04.006 ↗
6. Mechanical and tribological properties of AA7075–TiC metal matrix composites under heat treated (T6) and cast conditions10.1016/j.jmrt.2016.03.011 ↗
7. Microstructure, mechanical and corrosion behavior of high strength AA7075 aluminium alloy friction stir welds – effect of post weld heat treatment10.1016/j.dt.2015.04.003 ↗
8. Investigating local corrosion behavior and mechanism of MAO coated 7075 aluminum alloy10.1016/j.jallcom.2020.153976 ↗
9. Simultaneously improving tensile properties and stress corrosion cracking resistance of 7075-T6 aluminum alloy by USRP treatment10.1016/j.corsci.2023.111211 ↗
10. Fatigue behavior and life prediction of A7N01 aluminium alloy welded joint10.1016/S1003-6326(11)61552-5 ↗
11. Corrosion fatigue crack growth in A7N01S−T5 aluminum alloy MIG welded joints10.1016/j.jmrt.2023.01.103 ↗
12. Additively manufactured materials and structures: a state-of-the-art review on their mechanical characteristics and energy absorption10.1016/j.ijmecsci.2023.108102 ↗
13. Cold metal transfer welding of AlSi7Mg alloy sheets prepared by selective laser melting10.1016/j.jmapro.2022.10.013 ↗
14. Microstructures and fatigue behavior of metal-inert-gas-welded joints for extruded Al-Mg-Si alloy10.1016/j.msea.2018.12.080 ↗
15. Tailoring the microstructure and mechanical properties of wire and arc additive manufactured Al–Mg alloy via interlayer friction stir processing10.1016/j.jmrt.2023.06.053 ↗
16. GTAW flux increases weld joint penetration
17. Effect of activating flux on arc shape and arc voltage in tungsten inert gas welding10.1016/S1003-6326(07)60120-4 ↗
18. Study of the performance of stainless steel A-TIG welds10.1007/s11665-007-9139-7 ↗
19. Effect of molybdenum on mechanical and abrasive wear properties of coating of as weld hadfield steel with flux-cored gas tungsten arc welding10.1016/j.jallcom.2015.11.071 ↗
20. Effect of CaF2, FeMn and NiO additions on impact strength and hardness in submerged arc welding using developed agglomerated fluxes10.1016/j.jallcom.2016.01.133 ↗
21. Effect of oxide-based fluxes on mechanical and metallurgical properties of dissimilar activating flux assisted-tungsten inert gas welds10.1016/j.jmapro.2013.11.001 ↗
22. TIG welding with single-component fluxes10.1016/S0924-0136(99)00435-5 ↗
23. Effects of Cr2O3 active agent on the weld process dynamic behavior and joint comprehensive properties of fiber laser welded stainless steel thick plate10.1016/j.optlaseng.2020.106027 ↗
24. Effects of mix activated fluxes coating on microstructures and mechanical properties of tungsten inert gas welded AZ31 magnesium alloy joints10.1179/1362171812Y.0000000037 ↗
25. Effects of activating flux on weld bead geometry of inconel 718 alloy TIG welds10.1080/10426914.2012.677914 ↗
26. Alternative current flux zoned tungsten inert gas welding process for aluminium alloys10.1179/1362171811Y.0000000087 ↗
27. Flux bounded tungsten inert gas welding for enhanced weld performance—a review10.1016/j.jmapro.2017.05.023 ↗
28. Experimental investigations on tensile strength of flux bounded TIG welds of AA2219-T87 aluminum alloy10.1142/S0219686714500073 ↗
29. A novel perception toward welding of stainless steel by activated TIG welding: a review10.1080/10426914.2020.1854467 ↗
30. Suppression of undercut defects in high-speed GMAW through a compound magnetic field10.1016/j.jmatprotec.2019.116288 ↗
31. Influence of shielding gas on undercutting formation in gas metal arc welding10.1016/j.jmatprotec.2016.03.020 ↗
32. Fatigue strength assessment of butt-welded joints with undercuts10.1016/j.ijfatigue.2017.09.011 ↗
33. Augmentation of weld penetration by flux assisted TIG welding and its distinct variants for oxygen free copper10.1016/j.jmrt.2020.12.009 ↗
34. Effects of weld penetration modes on laser welding characteristics of a novel ultra-high strength steel for aerospace application10.1016/j.jmapro.2023.02.003 ↗
35. Prediction of penetration based on plasma plume and spectrum characteristics in laser welding10.1016/j.jmapro.2022.01.032 ↗
36. Effect of activated flux on penetration depth, microstructure and mechanical properties of Ti-6Al-4V TIG welds10.1016/j.jmatprotec.2018.06.024 ↗
37. Influence of the low voltage pulsed magnetic field on the columnar-to-equiaxed transition during directional solidification of superalloy K416910.1016/j.jmst.2020.02.009 ↗
38. Effects of layer-by-layer ultrasonic impact treatment on microstructure and mechanical properties of 304 stainless steel manufactured by directed energy deposition
39. Design strategy for eliminating cracking and improving mechanical properties of Al-Mg-Si alloys fabricated by laser melting deposition
40. Influence of melting current pulse duration on microstructural features and mechanical properties of AA5083 alloy weldments10.1016/j.msea.2019.01.030 ↗
41. Grain refining in weld metal using short-pulsed laser ablation during CW laser welding of 2024-T3 aluminum alloy10.1088/2631-7990/ab563a ↗
42. Enhancing joint strength of bobbin tool friction stir welded Al–Mg–Si alloy via post-weld aging process10.1016/j.jmrt.2022.11.058 ↗
43. Prediction of welding distortion in butt joint of thin plates10.1016/j.matdes.2009.05.004 ↗
44. Numerical and experimental investigations on the welding residual stresses and distortions of the short fillet welds in high strength steel plates10.1016/j.engstruct.2022.114269 ↗
45. Extension of the double-ellipsoidal heat source model to narrow-groove and keyhole weld configurations10.1016/j.jmatprotec.2017.02.002 ↗
46. Residual stress modification by post-weld treatment and its beneficial effect on fatigue strength of welded structures10.1016/j.ijfatigue.2003.08.020 ↗
47. Microscale residual stresses in additively manufactured stainless steel10.1038/s41467-019-12265-8 ↗
48. Analysis of residual stresses in electron beam welding with filler wire of Ti62A alloy10.1016/j.jmrt.2023.01.081 ↗
49. Mechanical behavior of additively and conventionally manufactured 316L stainless steel plates joined by gas metal arc welding10.1016/j.jmrt.2023.03.080 ↗
50. Influence of martensitic transformation on welding residual stress in plates and pipes10.1080/13621718.2016.1263711 ↗
51. Study on mechanism of the effect of Al element on the arc shape and molten pool fluctuation pattern in flux bands constricting arc welding (FBCA)10.1016/j.jmapro.2023.06.044 ↗
52. Numerical simulation on the nonaxisymmetry arc characteristics in narrow gap TIG welding: responses to welding parameters10.1007/s00170-021-06928-4 ↗
53. Effects of flux bands on arc stability in flux bands constricting arc welding10.1016/j.jmapro.2020.03.012 ↗
54. Marangoni convection and weld shape variations in Ar–O2 and Ar–CO2 shielded GTA welding10.1016/j.msea.2004.05.057 ↗
55. Influence of laser power on molten pool flow field of laser-MIG hybrid welded Invar alloy10.1016/j.optlastec.2020.106539 ↗
56. Effect of flux gap and particle size on the depth of penetration in FBTIG welding of aluminium10.1007/s12666-016-0929-1 ↗
57. Effect of cerium oxide flux on active flux TIG welding of 800MPa super steel10.1016/j.jmatprotec.2015.11.008 ↗
58. Solidification structure evolution and grain refinement mechanism of a deeply undercooled Ni65Cu35 alloy10.1007/s12540-021-01075-7 ↗
59. EBSD study on magnetic field altering crystal texture and grain growth during laser-hybrid welding10.1016/j.matdes.2022.110587 ↗
60. Additive manufacturing of ultrafine-grained high-strength titanium alloys10.1038/s41586-019-1783-1 ↗
61. Motion of grain boundaries incorporating dislocation structure10.1016/j.jmps.2018.05.001 ↗
62. Direct observation of the grain boundaries acting as dislocation sources in nanocrystalline platinum10.1016/j.matchar.2021.111493 ↗
63. Strengthening and fracture mechanisms of a precipitation hardening high-entropy alloy fabricated by selective laser melting10.1080/17452759.2022.2037055 ↗
64. Intermetallic regulation mechanism of inconel 718/Ti6Al4V composite by novel follow-up ultrasonic assisted laser additive manufacturing10.1016/j.compositesb.2022.109736 ↗
65. Effect of silicon addition on microstructure and mechanical properties of a high strength Ti-4Al-4Mo-4Sn alloy prepared by powder metallurgy10.1016/j.jallcom.2021.162267 ↗
66. The microstructure analysis, mechanical properties, and fracture behavior of electron beam welded C-103 niobium-based refractory alloy10.1016/j.jmrt.2023.05.070 ↗