Tribological and electrical properties of laser-clad W–Cu coatings on 7075 aluminum alloy
Source abstract
Abstract
Enhancing the ablation and wear resistance of aluminum-based armature is essential for improving the durability and operational stability of the electromagnetic launcher (EML). In this study, W–40 wt% Cu coatings were deposited on 7075 aluminum alloy (AA 7075) via a strategy combining dual-layer laser cladding with laser remelting to improve wear resistance while retaining electrical conductivity. The effects of laser parameters on the transient formation process, phase distribution, hardness, relative density and electrical conductivity of coatings were investigated. The results indicate that Al diffusion improved W–Cu wettability and may promote the formation of an interpenetrating transition layer at the interface between the two immiscible phases. Nevertheless, low thermal input was required to suppress excessive Al diffusion, which would lead to the formation of brittle intermetallic compounds (IMCs) and a consequent reduction in conductivity. Laser remelting alleviated lack-of-fusion defects, redistributed Al to prevent enrichment and cracks in the overlapping zones, and thus improved the surface relative density. The fabricated coating exhibited an average hardness of 259.5 HV 1 and an electrical conductivity of up to 32.1% IACS. Its wear rate (9.3 × 10 -5 mm 3 /N·m) was 64% lower than that of AA 7075, with adhesive wear as the dominant wear mechanism. At 300 °C, the wear rate further decreased to 8.5 × 10 -5 mm 3 /N⋅m due to the formation of lubricating WO 3 . This work offers a potential approach to improve the wear performance of aluminum-based armatures.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Electromagnetic Launch and Propulsion Technology · High Entropy Alloys Studies · High-Velocity Impact and Material Behavior
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (76)
Show source-provided references
1. Electromagnetic launchers and space
2. Research progress on advanced rail materials for electromagnetic railgun technology10.1016/j.dt.2020.03.014 ↗
3. Parametric analysis and design of the initial contact state of a 400 kA pulsed current C-armature10.1088/1742-6596/2478/9/092003 ↗
4. Research progress on surface damage and protection strategies of armature–rail friction pair materials for electromagnetic rail launch10.3390/ma17020277 ↗
5. Effect of equal channel angular pressing (ECAP) on wear behavior of Al-7075 alloy10.1016/j.mspro.2015.11.116 ↗
6. Wear behavior of 7075-aluminum after ultrasonic-assisted surface burnishing10.1016/j.jmapro.2020.01.026 ↗
7. Fabrication and heat treatment of graphene nanoplatelets reinforced aluminium nanocomposites10.1016/j.msea.2020.139657 ↗
8. Mechanical and conductivity properties of 6061Al matrix composites reinforced with different pH Cu-coated graphene10.1080/09276440.2023.2287330 ↗
9. Effect of liquid film (indium) on thermal and electromagnetic distribution of an electromagnetic launcher with new armature10.1109/ELT.2004.1398111 ↗
10. Solid armature performance: a progress review 1980–199010.1109/20.559918 ↗
11. Time- and frequency-domain characterization of railgun sliding contact noise10.1109/TPS.2017.2705172 ↗
12. Modelling of magneto-electro-thermo-mechanical coupled behavior of the lubricating liquid film for the electromagnetic launch10.1016/j.ijheatmasstransfer.2022.123267 ↗
13. Liquid metal corrosion effects on conventional metallic alloys exposed to eutectic gallium–indium alloy under various temperature states10.1007/s10765-018-2440-x ↗
14. Wear behavior of lubricant conditioned copper rails and armatures in a railgun10.1109/TPS.2010.2062540 ↗
15. Materials selection exercise for electromagnetic launcher rails10.1109/TMAG.2013.2243460 ↗
16. Application of coatings for electromagnetic Gun technology10.1109/20.364607 ↗
17. Improved anti-adhesive wear performance of rail/armature pair via interfacial energy modulation for electromagnetic launching applications10.1016/j.scriptamat.2023.115677 ↗
18. Enhancing anti-adhesion and wear performance at armature/rail interface through synergistic interfacial energy and lubrication effects10.1016/j.jmrt.2025.03.145 ↗
19. Conductive nitrides: growth principles, optical and electronic properties, and their perspectives in photonics and plasmonics10.1016/j.mser.2017.11.001 ↗
20. Two-dimensional electronic transport and surface electron accumulation in MoS210.1038/s41467-018-03824-6 ↗
21. Electrical conductivity models and theoretical value calculation of W–Cu
22. On the correlation of mechanical and physical properties of 7075-T6 Al alloy10.1016/j.engfailanal.2004.09.005 ↗
23. Excellent mechanical, thermal and electrical properties of ultrafine W-Cu alloys via freeze-drying technology10.1016/j.scriptamat.2023.115805 ↗
24. High temperature friction and wear behavior of tungsten–copper alloy10.1016/j.ijrmhm.2018.08.001 ↗
25. Hierarchical nanostructured W-Cu composite with outstanding hardness and wear resistance10.1088/1361-6528/ab548f ↗
26. Fabrication and characterization of W–Cu composite coatings with different W contents by cold spraying10.1016/j.surfcoat.2019.04.034 ↗
27. Analysis of copper-tungsten cold spray coating: kinetics of coating formation and its thermal properties10.1016/j.surfcoat.2020.125376 ↗
28. Enhanced arc erosion resistance via constructing W particle network structure in cold sprayed CuCrZr–W coating: implication for electromagnetic launching system10.1016/j.jmrt.2023.10.074 ↗
29. Tailoring the tribological properties of Cu composite coatings via integrating strengthening W particles and lubricant graphene10.1016/j.apsusc.2024.161248 ↗
30. Research on the elements diffusion behavior and properties in Cu/W composite coatings by high-speed laser cladding/laser remelting10.1016/j.jallcom.2025.181746 ↗
31. Research status of laser cladding technology on aluminum alloy surface10.1007/s00170-025-15204-8 ↗
32. Comparison of laser-clad and furnace-melted Ni-based alloy microstructures10.1016/S0257-8972(00)00732-5 ↗
33. High-speed laser-directed energy deposition of crack-free wear-resistant and anti-corrosive Al/Cu bimetal components10.1080/17452759.2024.2438885 ↗
34. Synthesis and processing techniques of tungsten copper composite powders for electrical contact materials: a review10.13005/ojc/350201 ↗
35. Light absorption of W–Cu powders in laser powder bed fusion10.1016/j.optlastec.2023.109243 ↗
36. Effects of tungsten particle size and copper content on densification of liquid-phase-sintered W–Cu10.1007/s11661-005-0277-y ↗
37. Dispersion of reinforcing micro-particles in the powder bed fusion additive manufacturing of metal matrix composites10.1016/j.actamat.2022.118086 ↗
38. Re-investigation of phase equilibria in the system Al–Cu and structural analysis of the high-temperature phase η1-Al1–δCu10.1016/j.intermet.2011.07.007 ↗
39. Metallographic studies of dissimilar Al–Cu laser-welded joints using various etchants10.1007/s13632-018-0501-y ↗
40. Composition and phases in laser welded Al–Cu joints by synchrotron x-ray microdiffraction10.1016/j.procir.2018.08.006 ↗
41. First-principles research to mechanical, electronic, thermodynamic, and optical properties of Al–Cu intermetallics10.1016/j.physb.2024.416163 ↗
42. Ultrastrong and ductile W–Cu composites via Al-mediated interfacial diffusion layers and matrix-nanoclusters networks10.1016/j.compositesb.2024.111667 ↗
43. In-situ fabrication and characteristics of an Al4W/Al12W composite using infiltration method10.1016/j.vacuum.2018.11.018 ↗
44. Surface tension of liquid Al–Cu binary alloys10.3139/146.110221 ↗
45. Characterization of laser-powder interaction and particle transport phenomena during laser direct deposition of W–Cu composite
46. Study on microstructure and mechanical properties of aluminum–copper dissimilar metals joints by nanosecond laser spiral welding10.1007/s12666-022-02623-4 ↗
47. The impact of ring-shaped laser beam on dissimilar welding of Al–Cu thin sheets for battery tab-to-busbar connection: microstructural, mechanical and electrical characteristics10.1016/j.optlastec.2024.111312 ↗
48. Laser pressure welding of dissimilar aluminium and copper: microstructure and mechanical property10.1080/13621718.2021.2010449 ↗
49. Heat transfer performance of CuCrZr/AlSi7Mg multi-material heat sinks with triply periodic minimal surface manufactured by laser powder bed fusion10.1080/17452759.2025.2523642 ↗
50. The formation and growth of intermetallic compounds during interdiffusion of Al/Cu bimetals10.1088/2053-1591/ac69b4 ↗
51. Mechanisms of formation of Al4Cu9 during mechanical alloying: an experimental study10.1016/j.actamat.2014.12.050 ↗
52. Investigation on indirect laser welding of copper to aluminum10.1016/j.procir.2024.08.065 ↗
53. Achieving both high conductivity and reliable high strength for W–Cu composite alloys using spherical initial powders10.1016/j.vacuum.2020.109620 ↗
54. Electrical resistivity of ten selected binary alloy systems10.1063/1.555684 ↗
55. Enhancing electrical conductivity and mechanical properties of W–Cu composites with additional Ag/La2O3 hybrid10.1007/s10853-024-10400-5 ↗
56. A review on copper alloys with high strength and high electrical conductivity10.1016/j.jallcom.2024.174456 ↗
57. Anisotropic material properties of pure copper with fine-grained microstructure fabricated by laser powder bed fusion process
58. Simultaneous enhancement of strength and conductivity via self-assembled lamellar architecture10.1038/s41467-024-46029-w ↗
59. Multilayered W–Cu composites with enhanced strength, electrical conductivity and wear resistance10.1016/j.compositesb.2024.111641 ↗
60. Effect of temperature on friction and galling behavior of 7075 aluminum alloy sheet based on ball-on-plate sliding test10.1016/j.triboint.2019.105872 ↗
61. Fabrication and high temperature tribological properties of WC reinforced W–Cu composites
62. Investigation on wear mechanism of thermochemically fabricated W–Cu composites10.1016/j.wear.2010.04.026 ↗
63. In situ raman spectroscopy studies for electrochemical CO2 reduction over Cu catalysts
64. The study of the tribological properties of TiAgN/W2N coatings in a wide temperature range10.1088/2053-1591/ab15ef ↗
65. Tungsten: properties, chemistry, technology of the element, alloys
66. Study on the oxidation and reduction of tungsten surface for sub-50 nm patterning process10.1116/1.4758790 ↗
67. A crystal-chemical approach to lubrication by solid oxides10.1023/A:1019183101329 ↗
68. The influence of microstructure on tribological properties of WO3 thin films10.1016/S0043-1648(99)00255-0 ↗
69. Revised effective ionic radii and systematic studies of interatomic distances in halides and chalcogenides10.1107/S0567739476001551 ↗
70. Infiltrated tungsten-copper composite reinforced with short tungsten fibers10.1016/j.vacuum.2019.109123 ↗
71. Wear-resistance enhancement of nanostructured W–Cu–Cr composites10.1016/j.ijrmhm.2021.105673 ↗
72. The process of surface carburization and high temperature wear behavior of infiltrated W–Cu composites10.1016/j.surfcoat.2018.08.088 ↗
73. In-situ synthesis of core-shell structure W(WC) composite grains in W–Cu composites fabricated by infiltration10.1016/j.jallcom.2021.158633 ↗
74. Fabrication and properties of the W-30wt%Cu gradient composite with W@WC core-shell structure10.1016/j.jallcom.2017.03.064 ↗
75. Effect of spark plasma sintering temperature on structure and performance characteristics of Cu–20wt%W composite10.1016/j.jallcom.2022.165246 ↗
76. Solid state and liquid phase sintering of mechanically activated W–20 wt.% Cu powder mixture10.1016/j.jallcom.2007.08.080 ↗