journal article·2025-03Open access

Influence of tundish flux on reoxidation behavior of Al-killed Ti-containing stainless steel

Yeongjin Jun, Yongsug Chung, Sungjin Park, Suchang Kang, Min-Kyu Paek, Joo Hyun Park

Abstract

The cleanliness of Ti-containing ferritic stainless steel (Ti-FSS) has been improved via vacuum-oxygen-decarburization (VOD) and ladle treatment (LT) processes. However, the reoxidation phenomena inevitably occur during melt transfer from ladle to continuous casting tundish, resulting in a loss of titanium yield in conjunction with the formation of reoxidative inclusions. Hence, the present work aims to systematically investigate the combinational effect of different tundish fluxes on the reoxidation behavior of Al-killed Ti-FSS melt. Rice husk ash (RHA) and MgO (M) insulation powders, and calcium aluminate , CaO–Al 2 O 3 (CA) based flux were used for the experiments. When the molten steel was covered by M + CA fluxes, the average size of inclusions decreased. On the other hand, when the RHA + CA fluxes were added, the average size of inclusion decreased, whereas total number of inclusions significantly increased due to a reoxidation reaction by SiO 2 in RHA. When the M + RHA + CA combinative fluxes were added, the size of inclusion decreased, and the number of inclusions exhibited a value between the M + CA and RHA + CA conditions. Consequently, a decrease in total oxygen content in Ti-FSS was most effective in the M + CA flux combination.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Metallurgical Processes and Thermodynamics · Hydrogen embrittlement and corrosion behaviors in metals · High-Temperature Coating Behaviors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (71)

Show source-provided references
1. Growth of initial clog deposits during continuous casting of Ti-ULC steel–formation and reduction of the initial deposits at nozzle/steel interface10.2355/isijinternational.ISIJINT-2019-384 ↗
2. Nozzle deposits in titanium treated stainless steels
3. Nozzle clogging behaviour of Ti-bearing Al-killed ultra low carbon steel10.2355/isijinternational.44.1653 ↗
4. Inclusion agglomeration on ultra-low C liquid steel surface: roles of Ti in the steel and the oxygen potential10.1007/s12540-022-01190-z ↗
5. Characteristics of nozzle clogging and evolution of oxide inclusion for Al-killed Ti-stabilized 18Cr stainless steel10.1007/s11663-019-01708-8 ↗
6. Application of k-means clustering to material research: measurement of layer thickness and contact angle10.1007/s12540-023-01411-z ↗
7. Predicting grain structure in continuously-cast stainless steel slab10.3365/KJMM.2023.61.1.60 ↗
8. Modelling of meniscus behavior and slag consumption during initial casting stage of continuous casting process10.1007/s12540-024-01629-5 ↗
9. Inclusions in stainless steels − A review10.1002/srin.201700130 ↗
10. Pitting corrosion behavior of custom 450 stainless steel using electrochemical characterization10.1007/s12540-020-00640-w ↗
11. Effect of CaO-Al2O3-MgO slags on the formation of MgO-Al2O3 inclusions in ferritic stainless steel10.1007/s11663-005-0041-0 ↗
12. Thermodynamic and kinetic analysis of non-metallic inclusions evolution in Si-killed 316L stainless steel with various refining slags10.1007/s12540-024-01715-8 ↗
13. Thermodynamics of the formation of MgO-Al2O3-TiOx inclusions in Ti-stabilized 11Cr ferritic stainless steel10.1007/s11663-008-9172-4 ↗
14. Thermodynamics of titanium oxide in CaO–SiO2–Al2O3–MgOsatd–CaF2 slag equilibrated with Fe–11mass% Cr melt10.2355/isijinternational.49.337 ↗
15. Removal of inclusion from molten steel in continuous casting tundish10.2355/isijinternational.32.157 ↗
16. Origin and removal of large nonmetallic inclusions occurring during continuous casting of wide slabs10.2355/tetsutohagane1955.62.14_1803 ↗
17. Technology for cleaning of molten steel in tundish10.2355/isijinternational.34.868 ↗
18. Reoxidation behavior of molten steel in tundish10.2355/isijinternational.40.40 ↗
19. Investigation on the effects of ladle change operation and tundish cover powder on steel cleanliness in a continuous casting tundish10.1002/srin.202100072 ↗
20. Reoxidation phenomena of liquid steel in secondary refining and continuous casting processes: a review
21. Optimizing fluid dynamics: an in-depth study for nano-biomedical applications with a heat source10.1007/s10973-024-13472-2 ↗
22. Prevention of steel melt reoxidation by covering powders in tundish
23. Sahai · 2008
24. Oxidation rate of aluminum in molten iron by CaO-SiO2-Al2O3-FeO-MnO slag10.2355/isijinternational.36.Suppl_S34 ↗
25. Kinetics of metal/slag reactions during spontaneous emulsification10.1007/s11663-005-0023-2 ↗
26. A reaction between high Mn-high Al steel and CaO-SiO2-type molten mold flux: Part II. Reaction mechanism, interface morphology, and Al2O3 accumulation in molten mold flux10.1007/s11663-012-9769-5 ↗
27. Reoxidation of Al-Ti containing steels by CaO-Al2O3-MgO-SiO2 slag10.2355/isijinternational.44.1669 ↗
28. Effect of rice husk ash insulation powder on the reoxidation behavior of molten steel in continuous casting tundish10.1007/s11663-017-0971-3 ↗
29. Influence of calcium aluminate flux on reoxidation behaviour of molten steel during continuous casting process10.1080/03019233.2019.1687968 ↗
30. Effect of tundish flux on compositional changes in non-metallic inclusions in stainless steel melts10.2355/isijinternational.ISIJINT-2021-167 ↗
31. Effect of varying Al2O3 contents of CaO–Al2O3–SiO2 slags on lumped MgO dissolution10.1016/j.ceramint.2019.11.088 ↗
32. The effect of FexO content on dissolution behavior of an alumina inclusion in CaO–Al2O3–SiO2–FexO slag by a single hot thermocouple technique10.1016/j.ceramint.2022.08.132 ↗
33. Dissolution behavior of MgAl2O4 spinel inclusions in mold slag10.1002/srin.202400039 ↗
34. Activation energy of alumina dissolution in FeO-bearing slags10.3390/met13101702 ↗
35. Influence of manufacturing conditions on inclusion characteristics and mechanical properties of FeCrNiMnCo alloy10.3390/met10101286 ↗
36. Non-metallic inclusions in different ferroalloys and their effect on the steel quality: a review10.1007/s11663-021-02259-7 ↗
37. Effect of Al deoxidation on the formation behavior of inclusions in Ce-added stainless steel melts10.1007/s12540-014-5022-x ↗
38. Estimation of air oxidation of teeming molten steel10.2355/isijinternational1966.23.598 ↗
39. The effect of gas flow rate on the evolution of the surface oxide on a molten low carbon Al killed steel10.1007/s10853-005-1929-4 ↗
40. Reoxidation and castability of aluminium-killed steels
41. Effect of trace of oxygen in Ar gas on initial growth of nozzle clogging deposits on SEN for Ti added ultra‐low C steel casting10.1002/srin.202200310 ↗
42. Evolution of Al-Ti complex oxide inclusions in interstitial-free steel analyzed using CALPHAD, SEM, EDS, EBSD, and CSLM, metall
43. Reoxidation of Al-killed steel by Cr2O3 from tundish cover flux10.3390/met9050554 ↗
44. Role of slags in steel refining: is it really understood and fully exploited?
45. Evolution of the non-metallic inclusions influenced by slag-metal reactions in Ti-containing ferritic stainless steel10.1007/s11663-021-02314-3 ↗
46. Effect of CaO–MgO–SiO2–Al2O3–TiO2 slags with different CaF2 contents on inclusions in Ti-stabilized 20Cr stainless steel10.2355/isijinternational.ISIJINT-2019-277 ↗
47. The effect of C content in MgO–C on dissolution behavior in CaO–SiO2–Al2O3 slag10.1016/j.ceramint.2022.06.010 ↗
48. In situ observation of the dissolution of SiO2 particles in CaO–Al2O3–SiO2 slags and mathematical analysis of its dissolution pattern10.1111/jace.12665 ↗
49. Refractory–slag–metal–inclusion multiphase reactions modeling using computational thermodynamics: kinetic model for prediction of inclusion evolution in molten steel10.1007/s11663-016-0734-6 ↗
50. Effect of CaO/Al2O3 ratio of ladle slag on formation behavior of inclusions in Mn and V alloyed steel10.2355/isijinternational.ISIJINT-2017-456 ↗
51. Influence of steel grade on oxidation rate of molten steel in tundish10.2355/isijinternational.52.831 ↗
52. Modeling reoxidation behavior of Al–Ti-containing steels by CaO–Al2O3–MgO–SiO2 slag10.1007/s42243-018-0015-5 ↗
53. Effect of silicon on the desulfurization of Al-killed steels: part I. mathematical model10.1007/s11663-013-9813-0 ↗
54. Kinetic modeling of nonmetallic inclusions behavior in molten steel: a review10.1007/s11663-020-01954-1 ↗
55. Effect of LCFeCr alloy additions on the non-metallic inclusion characteristics in Ti-containing ferritic stainless steel10.1007/s11663-021-02296-2 ↗
56. Effect of tundish flux on reoxidation behavior of Si-killed 316L stainless steel10.1016/j.jmrt.2023.04.115 ↗
57. Attraction force estimations of Al2O3 particle agglomerations in the melt10.1002/srin.201600090 ↗
58. Interaction between alumina inclusions in molten steel due to cavity bridge force10.2355/isijinternational.ISIJINT-2016-038 ↗
59. Significance of nonmetallic inclusions for the clogging phenomenon in continuous casting of steel – a review10.1002/srin.202200086 ↗
60. A study on the transient inclusion evolution during reoxidation of a Fe–Al–Ti–O melt10.2355/isijinternational.51.375 ↗
61. Transient evolution of inclusions during Al and Ti additions in Fe-20 mass pct Cr alloy10.3390/met9060702 ↗
62. Gibbs free energy and conditions of spinel (MgO‐Al2O3) formation in liquid steel10.1002/srin.200300165 ↗
63. Thermodynamics on the formation of spinel nonmetallic inclusion in liquid steel10.1007/s11663-997-0023-5 ↗
64. Activities of the constituents in spinel solid solution and free energies of formation of MgO10.2355/isijinternational.40.1059 ↗
65. Deoxidation equilibria among Mg, Al and O in liquid iron in the presence of MgO·Al2O3 spinel10.2355/isijinternational.43.201 ↗
66. A study on the mechanism of reaction between refractory materials and aluminium deoxidised molten steel10.1002/srin.199700542 ↗
67. Mechanism of reaction between refractory materials and aluminum deoxidised molten steel10.2355/isijinternational.36.Suppl_S109 ↗
68. Effect of slag composition on the kinetics of formation of Al2O3–MgO inclusions in aluminum killed ferritic stainless steel10.2355/isijinternational.40.121 ↗
69. Control of MgO·Al2O3 spinel inclusions in stainless steels10.2355/isijinternational.50.1333 ↗
70. Formation mechanism of spinel-type inclusions in high-alloyed stainless steel melts10.1007/s11663-007-9066-x ↗
71. Thermodynamic investigation on the formation of inclusions containing MgAl2O4 spinel during 16Cr–14Ni austenitic stainless steel manufacturing processes10.1016/j.msea.2007.03.011 ↗