Microhardness and microstructural evolution of helical cylindrical pinion mold cavity during plastic torsion forming
Source abstract
Abstract
Plastic helical cylindrical pinions are widely used, and the injection mold cavity is crucial for their manufacturing process. However, it is quite difficult to machine the helical gear cavity by electrical discharge machining (EDM) with spiral discharge, and the quality control issue has long troubled manufacturers. Therefore, the authors proposed a novel method for manufacturing helical gear cavities by plastic torsion forming. This method involves initially machining a straight-tooth cavity using wire electrical discharge machining (WEDM) and then plastically twisting it to manufacture a helical gear cavity, which could significantly reduce the manufacturing difficulty. This paper investigates the evolution of microhardness and microstructure during the plastic torsion forming process of helical gear cavities. A relationship model is established between the helix angle at the pitch circle of the helical gear cavity and the microhardness, as well as the average grain size. The results show that the hardness increases linearly as the helix angle increases, while the average grain size decreases linearly. Specifically, at smaller helix angles, the grain size exhibits a larger fluctuation range, which gradually diminishes as the helix angle increases, leading to improved accuracy of the model predictions. Observations of grain size and dislocations in the torsion samples reveal that strengthening under severe plastic deformation is primarily attributed to grain refinement, while under minor plastic deformation, it is more closely related to changes in internal dislocations. During this process, a strong <111> texture and a secondary <001> texture are formed, contributing to the enhancement of microhardness.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced machining processes and optimization · Metal Forming Simulation Techniques · Powder Metallurgy Techniques and Materials
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. Life and damage mode modeling applied to plastic gears10.1016/j.engfailanal.2015.08.040 ↗
2. Friction and wear behaviour of acetal and nylon gears10.1016/j.wear.2008.10.005 ↗
3. State-of-art review of past research on manufacturing of meso and micro cylindrical gears10.1016/j.precisioneng.2017.07.014 ↗
4. Alhadeff · 2023
5. Gupta K, Jain NK. On micro-geometry of miniature gears manufactured by wire electrical discharge machining n.d.
6. Fabrication of micro gear with intact tooth profile by micro wire electrical discharge machining10.1016/j.jmatprotec.2017.09.002 ↗
7. A pitch deviation compensation technology for precision manufacturing of small modulus copper electrode gears10.1007/s00170-021-07966-8 ↗
8. An efficient method to fabricate the mold cavity for a helical cylindrical pinion10.3390/pr11072033 ↗
9. Analysis on volume invariability of metal circular shaft in torsion deformation
10. Texture evolution in high-pressure torsion processing10.1016/j.pmatsci.2021.100886 ↗
11. Microstructure and microtexture evolution of pure titanium during single direction torsion and alternating cyclic torsion10.1007/s11661-017-4034-9 ↗
12. Evolution of microstructure and texture during annealing in a high-pressure torsion processed Fe-9Cr alloy10.1016/j.mtla.2019.100349 ↗
13. Effect of torsional deformation on microstructure and mechanical properties of pure copper10.1016/j.matchar.2024.114029 ↗
14. Preparation and characterization of Mg alloy rods with gradient microstructure by torsion deformation10.1007/s12540-016-6226-z ↗
15. Jonas JJ. The equivalent strain in high pressure torsion n.d.
16. Enhancing tensile strength of Cu by introducing gradient microstructures via a simple torsion deformation10.1016/j.matdes.2015.10.157 ↗
17. Twinning deformation and yield asymmetry improvement of magnesium alloys by free-end torsion10.1007/s11665-023-08854-w ↗
18. Evolution of texture and microstructure during hot torsion of a magnesium alloy10.1016/j.actamat.2013.05.018 ↗
19. Hardening and softening analysis of pure titanium based on the dislocation density during torsion deformation10.1016/j.msea.2016.06.046 ↗
20. Gradient structure in high pressure torsion compacted iron powder10.1002/adem.201500012 ↗
21. Excellent strengthening of low-carbon steel by severe free-end torsion10.1007/s12540-022-01369-4 ↗
22. Influences of pre-torsion deformation on microstructure and mechanical properties of pure titanium subjected to subsequent tension deformation10.1016/j.cja.2017.10.009 ↗
23. Microstructure and texture in W and W-1wt%La2O3 processed by high-pressure torsion10.1016/j.scriptamat.2017.06.008 ↗
24. Generation of extreme grain aspect ratios in severely deformed tantalum at elevated temperatures10.1016/j.scriptamat.2017.04.024 ↗
25. Microstructural evolution and mechanical properties of ultrafine-grained pure α-iron and Fe-0.02%C steel processed by high-pressure torsion: influence of second-phase particles10.1016/j.msea.2020.139915 ↗
26. Texture development during the torsion testing of α-iron and two IF steels10.1016/1359-6454(96)00114-0 ↗