journal article·2026-01Open access

Effect of initial base metal microstructure on weld hot cracking susceptibilities of Alloy 718 forgings

Seolbin Jeong, Sieun Lim, Gitae Park, Sangwoo Song, Dongyi Seo, Ilguk Jo, Yongjoon Kang

Abstract

The effect of the base metal (BM) microstructure on the hot cracking susceptibilities of Alloy 718 during welding was investigated. A forged ring of Alloy 718 was subjected to a series of heat treatments to produce distinct initial BM microstructures with variations in grain size and precipitate distribution. The cracking susceptibilities in the fusion zone (FZ) and heat-affected zone (HAZ) were quantitatively assessed using Varestraint tests. The results revealed that the FZ cracking susceptibility increased with increasing BM grain size, owing to epitaxial grain growth during solidification that promoted the formation of coarser grains in the FZ. In the HAZ, cracking susceptibility was strongly influenced by Nb-rich precipitates formed during solution treatment, such as Laves and grain boundary δ phases, which promoted constitutional liquation and segregation-induced liquation along grain boundaries, respectively.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Additive Manufacturing Materials and Processes · Microstructure and mechanical properties · Welding Techniques and Residual Stresses

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (77)

Show source-provided references
1. An overview on welding of Inconel 718 alloy - effect of welding processes on microstructural evolution and mechanical properties of joints10.1016/j.matchar.2021.110997 ↗
2. Lippold · 2011
3. Microstructural characteristics of forged and heat treated Inconel-718 disks10.1016/j.matdes.2013.06.004 ↗
4. The effect of δ phase on the mechanical properties of an Inconel 718 superalloy10.1007/s11665-012-0433-7 ↗
5. Effect of precipitated phases on the mechanical properties and fracture mechanisms of Inconel 718 alloy10.1016/j.msea.2023.144598 ↗
6. Effect of heat input on heat affected zone cracking in laser welded ATI Allvac 718Plus superalloy10.1016/j.msea.2006.11.054 ↗
7. Grain boundary segregation in a Ni–Fe-based (Alloy 718) superalloy10.1016/j.msea.2007.01.090 ↗
8. Precipitation kinetics of γ' and γ'' particles in Inconel 718 and its influence on mechanical properties
9. Evolution of delta phase microstructure in Alloy 718
10. Primary carbides in Alloy 718
11. A comparative analysis of Inconel 718 made by additive manufacturing and suction casting: microstructure evolution in homogenization
12. Deformation characteristics of δ phase in the delta-processed Inconel 718 alloy10.1016/j.matchar.2009.10.003 ↗
13. Effects of carbides and its evolution on creep properties of a directionally solidified nickel-based superalloy10.1016/j.msea.2015.02.056 ↗
14. Tailoring Laves phase and mechanical properties of directed energy deposited Inconel 718 thin-wall via a gradient laser power method10.1016/j.msea.2021.141822 ↗
15. The formation and control of Laves phase in superalloy 718 welds10.1023/A:1018541915113 ↗
16. Laves phase tuning for enhancing high temperature mechanical property improvement in laser directed energy deposited Inconel 71810.1016/j.compositesb.2021.108819 ↗
17. The influence of Laves phases on the room temperature tensile properties of Inconel 718 fabricated by powder feeding laser additive manufacturing10.1016/j.actamat.2018.10.032 ↗
18. Effect of cobalt on the mechanical properties of 718 base alloy with 1.2 wt% Al10.1016/j.jallcom.2022.166817 ↗
19. The high temperature oxidation behavior of IN718 alloy in vacuum10.1016/j.corsci.2022.110216 ↗
20. Study of oxide layer formation on Inconel 718 during isothermal oxidation between 800 °C to 1200 °C in hot air10.1016/j.ceramint.2022.07.187 ↗
21. The effect of rejuvenation heat treatments on the repair weldability of wrought Alloy 71810.1016/S0921-5093(02)00187-9 ↗
22. Microstructural analysis of fusion and heat affected zones in electron beam welded ALLVAC® 718PLUS™ superalloy10.1016/j.msea.2007.08.002 ↗
23. Microstructures and mechanical properties of Inconel 718 welds by CO2 laser welding10.1016/j.jmatprotec.2007.11.224 ↗
24. Weldability evaluation of alloy 718 investment castings with different Si contents and thermal histories and hot cracking mechanism in their laser beam welds10.3390/met11030402 ↗
25. Characterization of the microstructures and the cryogenic mechanical properties of electron beam welded Inconel 71810.1007/s11661-015-3269-6 ↗
26. Alternatives to reduce hot cracking susceptibility of IN718 casting alloy laser beam welds with a mushroom shape10.3390/met14091067 ↗
27. Effect of base metal and welding speed on fusion zone microstructure and HAZ hot-cracking of electron-beam welded Inconel 71810.1016/j.matdes.2015.10.082 ↗
28. Improvement of mechanical properties of Inconel 718 electron beam welds – influence of welding techniques and postweld heat treatment10.1007/s00170-008-1751-7 ↗
29. Influence of magnetic arc oscillation and current pulsing on microstructure and high temperature tensile strength of Alloy 718 TIG weldments10.1016/j.msea.2006.05.046 ↗
30. Mitigation of hot cracking in Inconel 718 superalloy by ultrasonic vibration during gas tungsten arc welding10.1016/j.jallcom.2017.12.295 ↗
31. Effect of weld cooling rate on Laves phase formation in Inconel 718 fusion zone10.1016/j.jmatprotec.2013.09.006 ↗
32. Influence of weld cooling rate on microstructure and mechanical properties of Alloy 718 weldments10.1007/s11661-008-9553-y ↗
33. Comparison of hot cracking susceptibility of TIG and laser beam welded alloy 718 by Varestraint testing10.3390/met9090985 ↗
34. Intergranular liquid formation, distribution, and cracking in the HAZ of Alloy 718 welds10.7449/1989/Superalloys_1989_437_455 ↗
35. Welding: solidification and microstructure10.1007/s11837-003-0134-7 ↗
36. Macro–micro scale modeling and simulation of columnar grain evolution during gas tungsten arc welding of nickel-based alloy GH303910.1007/s11661-019-05546-w ↗
37. Role of microstructure evolution during welding on mechanical properties and residual stresses of the Inconel 718 and austenitic stainless steel 304L dissimilar weld joint10.1007/s11661-024-07571-w ↗
38. Varestraint testing of selective laser additive manufactured Alloy 718 — influence of grain orientation10.3390/met9101113 ↗
39. Hot cracking in cast Alloy 71810.1080/13621718.2018.1429238 ↗
40. Effect of heat treatment on the microstructure and mechanical properties of Inconel 71810.1016/j.matpr.2017.11.448 ↗
41. Aging effects on the microstructure and creep behavior of Inconel 718 superalloy10.1016/j.msea.2008.04.097 ↗
42. Hot cracking tests – an overview of present technologies and applications10.1007/s40194-014-0126-y ↗
43. On the interpretation of Varestraint and Transvarestraint hot cracking test results10.1007/s40194-024-01706-8 ↗
44. Design of a double aging treatment for the improvement of mechanical and microstructural properties of pulse micro-plasma arc welded alloy 71810.1007/s10853-021-06121-8 ↗
45. Investigations of γ', γ'' and δ precipitates in heat-treated Inconel 718 alloy fabricated by selective laser melting10.1016/j.matchar.2018.01.006 ↗
46. Dissolution of the Laves phase and δ-precipitate formation mechanism in additively manufactured Inconel 718 during post-printing heat treatments
47. Study of microsegregation and Laves phase in Inconel 718 superalloy regarding cooling rate during solidification10.1007/s11661-014-2614-5 ↗
48. The effects of long-time exposure on Alloy 718
49. Early evolution of δ phase and coarse γ'' phase in Inconel 718 alloy with high-temperature ageing10.1016/j.matchar.2021.111403 ↗
50. Orientational growth behavior and mechanism of delta (δ) phase precipitation in cold-rolled Inconel 718 alloy during heat treatment10.1007/s42243-023-00955-z ↗
51. Correlations between two EBSD-based metrics—kernel average misorientation and image quality—on indicating dislocations of near-failure low-alloy steels induced by tensile and cyclic deformations
52. The dominant role of recrystallization and grain growth behaviors in the simulated welding heat-affected zone of high-Mn steel10.3390/ma17102218 ↗
53. On grain boundary engineering for a 316L austenitic stainless steel10.3390/met12122185 ↗
54. Influence of delta (δ) phase precipitation on static recrystallization of cold-rolled Inconel 718 alloy in solid-solution treatment10.1007/s42243-018-0219-8 ↗
55. The superplasticity improvement of Inconel 718 through grain refinement by large-reduction cold rolling and two-stage annealing10.1016/j.msea.2021.141713 ↗
56. The effect of subsequent heat treatment on the evolution behavior of second-phase particles and mechanical properties of the Inconel 718 superalloy manufactured by selective laser melting10.1016/j.msea.2020.139931 ↗
57. Effect of δ phase on high-temperature mechanical performances of Inconel 718 fabricated with the SLM process10.1016/j.msea.2019.138327 ↗
58. Regulating strength and ductility of additively manufactured Inconel 718 alloy via adding nano-TiC and deep cryogenic treatment10.1016/j.msea.2024.146852 ↗
59. Grain size effect on strain localization, slip–grain boundary interaction and damage in the Alloy 718 Ni-based superalloy at 650 °C10.1016/j.msea.2024.146927 ↗
60. Evaluation of hot cracking in nitrogen-bearing and fully austenitic stainless steel weldments
61. INCONEL 718: a solidification diagram10.1007/BF02650300 ↗
62. The solidification metallurgy of Alloy 718 and other Nb-containing superalloys10.7449/1989/Superalloys_1989_59_68 ↗
63. A simple index for predicting the susceptibility to solidification cracking
64. Relationship between alloy elements and weld solidification cracking susceptibility of austenitic stainless steel10.2355/isijinternational.ISIJINT-2019-035 ↗
65. Grain refining and cracking during solidification10.1007/s11661-024-07563-w ↗
66. Fine grains reduce cracking susceptibility during solidification: insights from phase-field simulations10.1007/s11837-019-03342-w ↗
67. The weld heat-affected zone liquation cracking susceptibility of naval steels
68. The effect of weld heat-affected zone hot cracks on the fatigue crack growth behavior of as-cast alloy 718
69. Kou · 2003
70. Competitive nucleation and rapid growth of Co–Si intermetallic compounds during eutectic solidification under containerless processing condition10.1016/S1005-0302(11)60189-8 ↗
71. The effect of annealing twin-generated special grain boundaries on HAZ liquation cracking of nickel-base superalloys10.1016/S1359-6454(03)00090-9 ↗
72. Mechanism of liquid metal embrittlement by simple experiments: from atomistics to life-time
73. Pathway to understand liquid metal embrittlement (LME) in Fe–Zn couple: from fundamentals toward application10.1016/j.pmatsci.2021.100798 ↗
74. Wetting phase transition of grain boundaries and material performance of novel Inconel 71810.1016/j.matlet.2021.129858 ↗
75. Solidification process and behavior of alloying elements in Ni-based superalloy Inconel 71810.2320/matertrans.45.2728 ↗
76. Effect of grain size on the weldability of cast Alloy 71810.1081/AMP-120029936 ↗
77. Effect of boron segregation at grain boundaries on heat-affected zone cracking in wrought Inconel 71810.1007/s11661-001-0350-0 ↗