Internal friction in high manganese-content Mn–Cu based alloys
Source abstract
Abstract
Mn-Cu binary alloys with high manganese content exhibit enhanced damping capacity, a broader temperature window for noise and vibration reduction, and low cost. However, they are significantly hindered by poor workability, elongation, and corrosion resistance. To enhance the poor workability, elongation, and corrosion resistance of high manganese Mn-Cu binary alloys, alloying with Cr is an effective approach. This work investigates microstructure evolution, amplitude-independent thermally-activated, and transient effects (in a temperature range from -90 °C to 200 °C and frequencies from 0.1 Hz to 10 Hz) in high manganese Mn-(10-13)Cu-(0-6)Cr alloys with different Cr contents. The relaxation activation energy for as-water quenched Mn-13Cu binary alloy is 0.56±0.05 eV. The substitution of Cu or Mn by Cr results in an increase in the activation energy. Phase transitions upon heating and cooling are characterized by modulus softening due to shear phase transition in all analyzed samples before and after ageing, while the transient internal friction peaks are observed not in all structural states. An increase in the volume effect of phase transition leads to an increase in the transitory peaks width and area under the peaks in Mn-10Cu-4Cr compared with Mn-13Cu.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Shape Memory Alloy Transformations · Magnetic Properties and Applications · Metallic Glasses and Amorphous Alloys
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (25)
Show source-provided references
1. Low-cycle fatigue life and plasticity mechanisms of a Fe−15Mn−10Cr−8Ni−4Si seismic damping alloy under cyclic loading at various temperatures10.1016/j.actamat.2021.117267 ↗
2. Damping mechanisms in high damping metals10.4028/www.scientific.net/KEM.319.225 ↗
3. Impact noise reduction due to the use of steels with enhanced dissipative properties in the manufacture of mining equipment parts10.33271/mining19.02.095 ↗
4. Preparation and research on the structure and properties of high damping Mn-Cu alloy10.1016/j.vacuum.2024.113592 ↗
5. Achieving strength-damping synergy in a Mn-Cu alloy by aging after cold deformation10.1016/j.msea.2025.148823 ↗
6. Laser melting deposition of Mn–Cu-based alloy: microstructure, mechanical properties and damping capacities10.1016/j.msea.2024.146875 ↗
7. Application of high-damping alloy M205210.4028/www.scientific.net/KEM.319.217 ↗
8. Research progress on additive manufacturing of Mn-Cu damping alloys10.1016/j.jallcom.2025.181329 ↗
9. Mechanical shock wave suppression structure in hold-down and release apparatus of spacecraft10.2514/1.J064420 ↗
10. Microstructure optimization of cold sprayed M2052 alloy using post-processing heat treatment for tailoring damping capacity10.1007/s12598-025-03235-9 ↗
11. Internal friction in metallic materials
12. Orientation dependence of damping behavior in a Mn-Cu shape memory alloy10.1016/j.scriptamat.2019.05.042 ↗
13. The twinning microstructure and damping behavior in Mn–30Cu (at%) alloy10.2320/matertrans.46.2164 ↗
14. Vinogradova · 2002
15. Transitory effects
16. Thermally activated and transient anelasticity due to phase transitions in Fe-26.6Ga alloy10.1016/j.mseb.2025.119122 ↗
17. The damping behavior of Ni added Mn–Cu damping alloys10.2320/matertrans.44.1671 ↗
18. FCC → FCT martensitic transition in two-phase Mn-Cu alloys10.1134/S0036029517030077 ↗
19. Reverse transformation behavior of a prestrained MnCu alloy10.1016/j.actamat.2005.12.007 ↗
20. Spinodal decomposition and martensitic transformation of the high manganese Mn‒xCu alloys fabricated by additive manufacturing
21. Formation of the thermodeformational properties of Mn-Cu-based alloys having the two-way shape memory effect10.1134/S0036029508040113 ↗
22. Spinodal decomposition influence of austenite on martensitic transition in a Mn-13 at.%Cu alloy10.1016/j.jallcom.2020.157061 ↗
23. Spinodal decomposition in ternary Mn-Cu-Cr alloy and its influence on martensitic transition temperatures10.1016/j.jallcom.2021.161082 ↗
24. Phase decomposition of the austenite phase in a Mn-30at%Cu alloy during aging10.1016/S1359-6454(99)00419-X ↗
25. Mechanical spectroscopy as an in situ tool to study anelasticity of martensitic transition in Fe-16Mn-8Cr-2Co alloy10.1016/j.matlet.2019.126635 ↗