Synergistic control of microstructure and plasticity in hot-rolled Ti/Mg laminated composite plates by matrix composition and interfacial oxidation
Source abstract
Abstract
Ti/Mg laminated composites were fabricated by hot-roll bonding at 400 °C with reduction ratios of 35% to 45%, using pure Mg and AZ31 alloy as base layer and TA1 pure titanium as the cladding layer. This study systematically investigates the synergistic effect of matrix composition and interfacial oxidation on the interfacial microstructure and mechanical properties of the Ti/Mg laminated composites. Initial bonding was achieved via mechanical interlocking under rolling pressure, which was enhanced at higher reduction ratios, resulting in improved tensile-shear strength. At the pure Mg/Ti interface, a MgTiO 3 -reinforced crystalline-amorphous composite structure formed via a Ti-Mg-O ternary reaction, which effectively hindering crack propagation and conferred superior tensile-shear and uniaxial tensile properties. In contrast, at the AZ31/Ti interface, the presence of Al promoted the formation of a multi-element amorphous transition zone rich in Al and O. While this improved the bending strength to some extent, it also induced high interfacial brittleness and unstable shear fracture. This work demonstrates that the O-dominated diffusion pathway achieves a better strength-toughness balance than the Al-dominated multi-element mechanism, providing crucial theoretical insights and experimental support for the interface design and performance optimization of Ti/Mg laminated composites.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Aluminum Alloys Composites Properties · Magnesium Alloys: Properties and Applications · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (47)
Show source-provided references
1. Microstructure and mechanical properties of Ti-Mg lightweight heterostructured materials10.1016/j.msea.2022.143560 ↗
2. Simultaneous sintering of low-melting-point Mg with high-melting-point Ti via a novel one-step high-pressure solid-phase sintering strategy10.1016/j.jallcom.2020.158344 ↗
3. Improving ductility and anisotropy by dynamic recrystallization in Ti/Mg laminated metal composite10.1007/s40195-022-01442-2 ↗
4. Partially degradable Ti-Mg composites for biomedical applications: recent advances and future perspectives10.1016/j.actbio.2025.07.032 ↗
5. Fiorani · 1996
6. Formation conditions of Ti2 O3 , MgTi2O4 , Mg2TiO4 , and MgAl2O4 in Ti-Mg-Al complex deoxidation of molten iron10.1002/srin.201400034 ↗
7. The study of microstructure, corrosion resistance and mechanical properties of ultrasonic assisted welding-brazing of Ti-Mg10.1016/j.jmrt.2022.01.037 ↗
8. Improving shear strength of Ti/Mg bimetal composites prepared by hot‐dip aluminizing and solid–liquid compound casting10.1002/adem.202200298 ↗
9. Design, fabrication, microstructure, and mechanical properties of interlayer-free vacuum diffusion bonding Mg/Ti composites10.1016/j.vacuum.2022.110947 ↗
10. Effect of HEA/Al composite interlayer on microstructure and mechanical property of Ti/Mg bimetal composite by solid-liquid compound casting10.1007/s41230-022-2105-z ↗
11. Effective joining of Mg/Ti dissimilar alloys by friction stir lap welding10.1016/j.jmatprotec.2019.116483 ↗
12. Influence of Ni-coating thickness on laser lap welding-brazing of Mg/Ti10.1016/j.optlastec.2018.07.007 ↗
13. High-strength Ti-Mg interface with 3D interlocking structure via Ti mesh interlayer: fabrication, microstructure, and mechanical properties10.1016/j.jmatprotec.2025.118979 ↗
14. Weifeng L., Lixian L., Zifeng L., Ying L. Preparation and mechanical properties of bicontinuous phase Mg-Ti composite. Rare Met Mater Eng 2023,52(11):3715∼3722.doi:10.12442/j.issn.1002-185X.20230229.
15. Effect of high energy shot peening on the microstructure and mechanical properties of Mg/Ti joints10.1016/j.jallcom.2016.10.262 ↗
16. Effect of Al layer thickness on the bonding and mechanical behavior of a Mg-(Al-)Ti laminated sheet prepared by hot-rolling after differential preheating treatment10.3390/ma15082805 ↗
17. Fabrication of Mg/Ti composite with excellent strength and ductility by hot rolling10.1016/j.msea.2023.145783 ↗
18. Microstructure and bonding properties of magnesium alloy AZ31/CP-Ti clad plates fabricated by rolling bonding10.1016/j.jmapro.2018.02.011 ↗
19. Fabrication, microstructure characterization and mechanical property of the Ti6Al4V-(NiTif/Mg3AlZn) laminate composite10.1016/j.jallcom.2018.10.074 ↗
20. Interfacial characteristics and bending properties of a Ti6Al4V-Mg3AlZn laminate metal composite10.1016/j.jallcom.2020.156065 ↗
21. Effect of amorphous layer parameters on tensile behavior of amorphous/crystalline CuZr/Cu composites
22. Interfacial microstructure and mechanical properties of Al/steel joints fabricated via thermo-compensated resistance brazing welding with cold spray Zn interlayer10.1016/j.jmrt.2023.04.081 ↗
23. Plastic deformation behaviors of Ti-Al laminated composite fabricated by vacuum hot-pressing10.1016/j.vacuum.2018.05.021 ↗
24. Bendability of gradient-structured VK41/AZ31 composite sheets fabricated by asymmetric extrusion10.1016/j.jallcom.2025.185111 ↗
25. The preparation of ZK61/7075 laminated composite by introducing pure Cu transition layer: effect of extrusion temperature on microstructure and mechanical properties10.1016/j.msea.2025.148722 ↗
26. Mechanical behavior and strengthening mechanisms in ultrafine grain precipitation-strengthened aluminum alloy10.1016/j.actamat.2013.09.042 ↗
27. Orientation gradients and geometrically necessary dislocations in ultrafine grained dual-phase steels studied by 2D and 3D EBSD10.1016/j.msea.2010.01.004 ↗
28. Tailoring strength-ductility synergy of Al/Ti laminates by thickness ratio optimization and asymmetric cryorolling10.1016/j.jmrt.2025.10.139 ↗
29. Microstructural evolution and mechanical properties of pure aluminum upon multi-pass caliber rolling10.3390/ma15031206 ↗
30. Microstructure evolution and mechanical properties of Al/Mg-Li/Al laminate metallic composites via hot roll bonding and subsequent cryorolling10.1016/j.msea.2023.146007 ↗
31. Application of nanoindentation technique in martensitic structures
32. Tailoring the microstructure of Al/Ti laminated composite through hot press sintering process to achieve superior mechanical properties10.1016/j.jmatprotec.2024.118349 ↗
33. Microstructure, plastic deformation and strengthening mechanisms of an Al–Mg–Si alloy with a bimodal grain structure10.1016/j.jallcom.2015.01.229 ↗
34. Stress-induced failure transition in metallic glasses10.1016/j.ijplas.2024.104152 ↗
35. Simultaneous enhancement of tensile properties and fracture toughness of bulk metallic glass composites10.1016/j.actamat.2025.121018 ↗
36. Atomic scale insights on mechanical behavior and crack propagation in Mg-Al based nanolaminates
37. Micro-mechanism of mechanical enhancement of NiTiAl amorphous-crystal nanomultilayers10.1016/j.ijmecsci.2025.110020 ↗
38. Dual-nano composite design with grain boundary segregation for enhanced strength and plasticity in CoCrNi-CuZr thin films10.1021/acs.nanolett.4c04755 ↗
39. Ti-based amorphous/nanocrystal composite with high ductility and strain-hardening10.1016/j.msea.2012.09.076 ↗
40. Effect of layered structural parameter on microstructure and mechanical properties of Ti/Al3Ti laminated composites10.1016/j.matchar.2025.115818 ↗
41. The critical roles of twinning and prismatic ⟨a⟩ slipping in affecting the dynamic recrystallization of hot-rolled Mg-Gd-Zr thick plate10.1016/j.jma.2025.07.016 ↗
42. Influence of gradual stress relieving on the microstructure, texture development, grain structure and orientation of the hot-rolled Ti6Al4V–5Cu alloy10.1016/j.jmrt.2024.05.096 ↗
43. Correlation of interfacial stress with the surface roughness of carbon fiber in composites by the improved shear-lag theory10.1080/09276440.2022.2164131 ↗
44. A 3D elastoplastic constitutive model considering progressive damage behavior for thermoplastic composites of T700/PEEK10.3390/ma17133317 ↗
45. A micromechanical cyclic constitutive model for ratchetting deformation of polymeric composites with imperfect interface10.1002/pc.27824 ↗
46. Preparation, structure and properties of Mg/Al laminated metal composites fabricated by roll-bonding, a review10.1016/j.jma.2022.08.001 ↗
47. Fabrication of Ti/Mg bimetal composite in Ti-6Al-4V pyramidal lattice structure via AZ91D melt infiltration10.1016/S1003-6326(25)66833-6 ↗