Moisture-driven chlorination and exfoliation corrosion of Inconel 625 in NaCl–MgCl2 molten salt: Effect of salt purification and surface roughness
Source abstract
Abstract
Corrosion behavior of Inconel 625 was systematically evaluated in molten NaCl–MgCl 2 salt at 650 °C under an argon atmosphere for 300 hours. The effects of salt purification and surface roughness were examined using mass loss measurements, SEM-EDS, XRD, and ICP-OES analyses. Specimens immersed in salt with low H 2 O content exhibited significantly reduced corrosion rates—55.4 μm/year for polished and 79.6 μm/year for ground surfaces—compared to 288.3 μm/year in salt with high H 2 O content. Salt purification effectively suppressed the selective leaching of Cr and Fe and prevented the formation of surface oxides such as Cr 2 O 3 and MgO. In contrast, unpurified salt with residual moisture induced extensive intergranular corrosion (IGC), pitting, and the deposition of oxide layers due to hydrolysis-generated HCl and Cl 2 gases. Thermodynamic calculations using FactSage confirmed that corrosive species can be generated through the stepwise decomposition of MgCl 2 ·H 2 O. ICP-OES analysis revealed that dissolved Cr and Fe were detected in the purified molten salt, whereas in the salt with high H 2 O content these elements were not detected due to secondary reactions leading to the formation of volatile or solid corrosion products. These results clearly demonstrate that corrosion resistance in chloride-based molten salt environments is strongly governed by salt purity and surface condition. Accordingly, proper salt pretreatment and surface preparation are essential for the reliable deployment of Inconel 625 in molten salt reactor applications.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Molten salt chemistry and electrochemical processes · Metallurgical Processes and Thermodynamics · High-Temperature Coating Behaviors
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (59)
Show source-provided references
1. The molten salt reactor (MSR) in generation IV: overview and perspectives10.1016/j.pnucene.2014.02.014 ↗
2. Molten salt for advanced energy applications: a review10.1016/j.anucene.2021.108924 ↗
3. A review of molten salt reactor multi-physics coupling models and development prospects10.3390/en15218296 ↗
4. Experience with the molten-salt reactor experiment
5. Generation IV nuclear reactors: current status and future prospects10.1016/j.enpol.2013.06.101 ↗
6. Corrosion of structural alloys in high-temperature molten fluoride salts for applications in molten salt reactors10.1007/s11837-018-2981-2 ↗
7. Huntley · 1973
8. Impact of corrosion test container material in molten fluorides10.1115/1.4031682 ↗
9. Molten fluorides as power reactor fuels10.13182/NSE57-A35494 ↗
10. Th–U cycle performance analysis based on molten chloride salt and molten fluoride salt fast reactors10.1007/s41365-020-00790-x ↗
11. On the employment of a chloride or fluoride salt fuel system in advanced molten salt reactors. Part 1: thermophysical properties and core criticality10.3390/en15238865 ↗
12. Williams · 2006
13. Simulation-assisted determination of the minimum melting temperature composition of MgCl2–KCl–NaCl salt mixture for next-generation molten salt thermal energy storage10.3389/fenrg.2022.809663 ↗
14. Engineering molten MgCl2–KCl–NaCl salt for high-temperature thermal energy storage: review on salt properties and corrosion control strategies10.1016/j.solmat.2021.111344 ↗
15. Corrosion resistance of hastelloys in molten metal-chloride heat-transfer fluids for concentrating solar power applications10.1016/j.solener.2014.02.002 ↗
16. Influence of MgCl2 content on corrosion behavior of GH1140 in molten NaCl–MgCl2 as thermal storage medium10.1016/j.solmat.2017.11.014 ↗
17. Effects of alloying elements on the corrosion behavior of Ni-based alloys in molten NaCl–KCl–MgCl2 salt at different temperatures10.1016/j.corsci.2018.08.021 ↗
18. Comparative study on high-temperature corrosion of TP347H stainless steel, C22 alloy and laser-cladded C22 coating in molten chloride salts10.1016/j.corsci.2014.03.012 ↗
19. Excellent corrosion resistance of 316 stainless steel in purified NaCl–MgCl2 eutectic salt at high temperature10.1016/j.corsci.2020.108473 ↗
20. Characterization of oxide scales on alloy 800H and stainless steel 316 in supercritical water10.1016/j.corsci.2015.07.035 ↗
21. Electrochemical impedance spectroscopy study of corrosion of steels beneath a molten ZnCl2–KCl film at 400 °C in air10.1007/s11085-009-9154-1 ↗
22. Assessment of effects of Mg treatment on corrosivity of molten NaCl–KCl–MgCl2 salt using Raman and infrared spectroscopy10.1016/j.corsci.2019.108350 ↗
23. Compatibility of Fe-based alloys with purified molten MgCl2–KCl–NaCl salt at 700 °C10.1016/j.apenergy.2022.119708 ↗
24. Hot corrosion behavior of commercial alloys in molten MgCl2/KCl/NaCl under inert atmosphere10.1016/j.solmat.2018.04.025 ↗
25. Corrosion behavior of inconel 625 cladding metal in KCl–MgCl2 molten salt under isothermal and thermal cycling conditions10.1007/s10853-023-08823-7 ↗
26. Grain size effect on corrosion behavior of inconel 625 film against molten MgCl2–NaCl–KCl salt10.1016/j.corsci.2022.110097 ↗
27. High-temperature molten salt corrosion of inconel 625 coatings prepared by high-speed laser cladding
28. Corrosion effect of Fe- and Ni-based alloys in molten salt reactors with additional trivalent salts10.1007/s43207-025-00499-w ↗
29. Effects of Mo and W on corrosion behavior of Ni-based alloys in NaCl–KCl–MgCl2 molten salt10.1016/j.corsci.2024.112313 ↗
30. Corrosion behavior of a multi-principal component alloy in LiCl–KCl–CsCl molten salt at 700 °C10.1007/s10853-024-10435-8 ↗
31. Thermal energy storage using chloride salts and their eutectics10.1016/j.applthermaleng.2016.07.046 ↗
32. High-temperature corrosion behavior of inconel 625 in NaCl–CaCl2–MgCl2 molten salt10.1016/j.solener.2022.03.074 ↗
33. Effect of surface roughness on early-stage oxidation behavior of inconel 62510.3390/asi1030032 ↗
34. Simultaneous effect of surface roughness and passivity on corrosion resistance of metals10.2495/MC150321 ↗
35. Corrosion kinetics of pure metals and alloys in purified molten chloride salt10.1039/D5RA00451A ↗
36. Corrosion mechanisms of P91 steel and inconel 600 in molten chlorides. Part II10.1016/j.solmat.2020.110675 ↗
37. Scalability of purification methods for MgCl2-containing salts10.1016/j.solmat.2020.110663 ↗
38. Redox potential measurements of Cr/Cr2+ and Ni/Ni2+ in molten MgCl2–KCl–NaCl10.1149/1945-7111/aba15a ↗
39. Mechanisms of exfoliation corrosion and stress corrosion cracking
40. Exfoliation corrosion and pitting corrosion in fatigue modeling10.1155/2012/191879 ↗
41. Stress effects in high-temperature oxidation of metals10.1179/imr.1995.40.1.1 ↗
42. Metallic impurities induced corrosion of a Ni–26W–6Cr alloy in molten fluoride salts at 850 °C10.1016/j.corsci.2020.109079 ↗
43. Corrosion behavior of a wear resistant co–mo–cr–si alloy in molten fluoride salts10.1016/j.jnucmat.2020.152529 ↗
44. Wrinkling of α-Al2O3 films grown by thermal oxidation10.1016/S1359-6454(00)00156-7 ↗
45. Damage evolution in thermal barrier coatings with thermal cycling10.1111/j.1551-2916.2011.04496.x ↗
46. Dissimilar metal corrosion in molten chloride salt10.1016/j.solmat.2024.113089 ↗
47. Delamination of polymeric coatings from steel10.1016/S0010-938X(98)00166-8 ↗
48. In situ detection of electrochemical activity differences using scanning kelvin probe force microscopy10.1016/j.corsci.2012.02.006 ↗
49. Kinetics of volatilization of high-temperature corrosion products10.1002/maco.201608841 ↗
50. Influence of NaCl and CaCl2 induced high-temperature corrosion10.1002/maco.201810451 ↗
51. High-temperature chlorination of nickel oxide using calcium chloride10.3390/ma16216888 ↗
52. High-temperature corrosion of a nickel-based alloy in molten chloride: effect of thermal and chemical purification10.1016/j.solmat.2021.111542 ↗
53. Corrosion of a Ni-based alloy in ternary chloride salt for thermal storage10.1016/j.corsci.2022.110673 ↗
54. Effect of surface roughness on corrosion resistance of mooring chains10.3390/met14101181 ↗
55. Influence of surface state on corrosion behavior of 316L produced by LPBF10.1016/j.corsci.2022.110550 ↗
56. Effect of surface roughness on pitting corrosion of duplex stainless steel10.3390/ma12050738 ↗
57. Effect of degree of ordering by varying cooling rate below 550 °C on the initiation of primary water stress corrosion cracking (PWSCC) in alloy 600 tube10.3365/KJMM.2025.63.8.606 ↗
58. In-situ precipitated nanocrystalline β-Ti reinforced porous titanium alloy via molten salt electrolysis10.1007/s12540-023-01497-5 ↗
59. Chemical analysis and electrochemical monitoring of ultra-low concentration MgOHCl impurity in molten MgCl2–KCl–NaCl10.3389/fenrg.2022.811832 ↗