Hot-dip aluminizing of stainless steel and investigation of interfacial intermetallics
Source abstract
Abstract
The types and evolution of Fe-Al intermetallic compounds (IMCs) serve as the theoretical foundation for regulating the microstructure and properties of the aluminum/steel joining interface. In this study, through hot-dip aluminizing experiments of stainless steel at 700–1000°C for 2–30 s, the formation temperatures and durations of various interfacial IMCs were identified, the growth kinetics of IMC layers were analyzed, and the structural similarities and differences among the compounds were compared. With increasing hot-dipping temperature and time, Fe 4 Al 13 formed at 700°C for 2 s, Fe 2 Al 5 and FeAl 2 emerged at 750°C for 30 s, and FeAl appeared at 950°C for 2 s. The total thickness of the IMCs initially decreased with rising temperature, then stabilized, and subsequently increased. An anomalous reduction in total thickness with prolonged time was observed at 750°C, attributed to the formation of multi-layered IMCs at the interface, which decelerated the growth rate of Fe 4 Al 13 . EBSD analysis revealed that the average grain size and texture intensity of the four IMCs followed the order: Fe 2 Al 5 > Fe 4 Al 13 > FeAl > FeAl 2 . All the IMCs predominantly exhibited high-angle grain boundaries. The crystallographic symmetry was relatively poor for Fe 2 Al 5 and FeAl, moderately improved for Fe 4 Al 13 , and optimal for FeAl 2 .
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Intermetallics and Advanced Alloy Properties · Microstructure and Mechanical Properties of Steels · Advanced Welding Techniques Analysis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (68)
Show source-provided references
1. Deep drawing of aluminium–steel tailor-welded blanks10.1016/j.matdes.2006.11.007 ↗
2. Defect structure of deformed Fe2Al5 intermetallic compound10.1016/S0966-9795(03)00050-5 ↗
3. Spreading behavior and microstructure characteristics of dissimilar metals TIG welding–brazing of aluminum alloy to stainless steel10.1016/j.msea.2009.02.036 ↗
4. Investigations on the effects of friction stir welding parameters on intermetallic and defect formation in joining aluminum alloy to mild steel10.1016/j.matdes.2013.01.013 ↗
5. Microstructure evolution in a martensitic 430 stainless steel-Al metallic-intermetallic laminate (MIL) composite10.1016/j.msea.2015.07.014 ↗
6. Influence of accelerated corrosion on Al/steel RSW joints by in situ compression tests10.1016/j.msea.2023.145851 ↗
7. Fatigue crack propagation characteristics of aluminum/steel laser-metal inert gas fusion-brazed joints in different micro-zones10.1016/j.ijfatigue.2024.108261 ↗
8. Fracture mechanisms of Al-steel resistance spot welds: the role of intermetallic compound phases10.1016/j.engfracmech.2024.110520 ↗
9. Wettability and reactivity of liquid aluminium and highly deformed steel10.1016/j.molliq.2024.125379 ↗
10. Effect of anomalous crystal structure of iron aluminides Fe2Al5 and Fe4Al13: low phonon thermal conductivity and potentiality as thermoelectric materials10.2320/matertrans.MF201607 ↗
11. Heat capacity of Fe-Al intermetallics: B2-FeAl, FeAl2, Fe2Al5 and Fe4Al1310.1016/j.jallcom.2017.07.199 ↗
12. Heat capacity of η-AlFe (Fe2Al5)10.1016/j.intermet.2016.07.002 ↗
13. Influence of intermetallic phases and Kirkendall-porosity on the mechanical properties of joints between steel and aluminium alloys10.1016/j.msea.2011.02.057 ↗
14. Polymorphic phase transformation of Fe4Al13 causing multiple twinning with decagonal pseudo-symmetry10.1107/S0108768194008086 ↗
15. Pearson · 1967
16. Evolution mechanism of interfacial microstructure and regulation of mechanical properties of laser-arc hybrid weld-brazing aluminum/steel joints under different post-welding heat-treatment temperatures10.1016/j.jmrt.2024.01.168 ↗
17. Kinetics of intermetallic compound layers between AISI 321 stainless steel and molten aluminum10.1016/j.matchar.2023.113062 ↗
18. Kinetic interactions between solid iron and molten aluminium10.1016/S0921-5093(03)00469-6 ↗
19. An assessment of the entire Al–Fe system including D03 ordering10.1016/j.actamat.2009.02.046 ↗
20. Orientation relationship of intergrowth Al2Fe and Al5Fe2 intermetallics determined by single-crystal X-ray diffraction10.3390/met14030337 ↗
21. Interaction of 18Cr-10Ni stainless steel with liquid aluminium10.1007/BF00575397 ↗
22. Structure refinement of the iron-aluminium phase with the approximate composition Fe2Al510.1107/S0108768193013989 ↗
23. Phases and phase equilibria in the Fe–Al–Zr system10.1515/ijmr-2004-0096 ↗
24. Achieving room-temperature brittle-to-ductile transition in ultrafine layered Fe-Al alloys10.1126/sciadv.abb6658 ↗
25. A study on the formation of iron aluminide (FeAl) from elemental powders10.1016/j.jallcom.2015.02.132 ↗
26. Thermodynamic factor from X-ray diffuse scattering: FeAl DO3-phase study10.1016/S1359-6462(99)00103-7 ↗
27. Evaluation of hydrogen embrittlement in FeAl assisted by mechanical milling
28. Deformation and fracture evolution of FeAl-based metallic-intermetallic laminate (MIL) composites10.1016/j.actamat.2020.04.005 ↗
29. Analysis of process parameters effects on friction stir welding of dissimilar aluminum alloy to advanced high strength steel10.1016/j.matdes.2014.02.003 ↗
30. Microstructural evolution during friction stir welding of dissimilar aluminum alloy to advanced high-strength steel10.1007/s00170-015-7531-2 ↗
31. Intermetallic compound formation in Fe-Al-Si ternary system: Part II10.1016/S1044-5803(03)00005-6 ↗
32. Welding of FeAl porous materials and stainless steel
33. Joining of aluminum alloy 5052 and low-carbon steel by laser roll welding
34. In-situ formed amorphous phase in aluminum/steel friction stir welds: interface evolution and strength improvement
35. Study of microstructure and phase evolution of hot-dipped aluminide mild steel during high-temperature diffusion using electron backscatter diffraction10.1016/j.apsusc.2010.12.118 ↗
36. Microstructure studies of an aluminide coating on 9Cr-1Mo steel during high temperature oxidation10.1016/j.surfcoat.2005.11.038 ↗
37. Control of intermetallic compound layers at interface between steel and aluminum by diffusion-treatment10.1016/S0921-5093(02)00053-9 ↗
38. Fabrication and microstructure evolution of B2 structure-based metal-intermetallic-laminate composites10.1016/j.jallcom.2021.162073 ↗
39. Understanding formation mechanisms of intermetallic compounds in dissimilar Al/steel joint processed by resistance spot welding10.1016/j.jmapro.2022.08.062 ↗
40. An investigation of the effect of steel alloying elements on iron-aluminum intermetallic characteristics for dissimilar resistance spot welding10.1016/j.matdes.2024.113514 ↗
41. Evolution of iron aluminide in Al/Fe in situ composites fabricated by plasma synthesis method10.1016/S0921-5093(03)00639-7 ↗
42. Reactions between low alloyed steel and initially pure as well as iron-saturated aluminium melts between 670 and 800°C10.1515/ijmr-1986-770408 ↗
43. Intermetallic FexAly-phases in a steel/Al-alloy fusion weld10.1007/s10853-006-0644-0 ↗
44. Evolution of intermetallics between solid Fe-Cr/Fe-Ni alloys and molten aluminium10.1016/j.ijmecsci.2023.108549 ↗
45. Kinetics of intermetallic compound layers during initial period of reaction between mild steel and molten aluminum10.3139/146.111735 ↗
46. Interaction and intermetallic phase formation between aluminum and stainless steel10.1016/j.rinp.2018.11.076 ↗
47. Bioactive coating with antibacterial and anticorrosive properties deposited on ZA6-1 alloy bone implant10.1016/S1003-6326(23)66199-0 ↗
48. Effect of welding time on the joining phenomena of diffusion welded joint between aluminum alloy and stainless steel10.1080/10426914.2012.663122 ↗
49. GTA weld brazing a joint of aluminum to stainless steel10.29391/2019.98.030 ↗
50. Intermetallic compound layer growth between solid iron and molten aluminium10.1016/S0921-5093(98)00573-5 ↗
51. Growth behavior of Fe2Al5 during reactive diffusion between Fe and Al at solid-state temperatures10.1016/j.msea.2007.01.099 ↗
52. Dynamic growth model of Fe2Al5 during dissimilar joining of Al to steel using the variable polarity cold metal transfer (VP-CMT)10.1016/j.jmatprotec.2021.117477 ↗
53. Formation of Fe5Si3 precipitate in the Fe2Al5 intermetallic layer of the Al/steel dissimilar arc welding joint: a transmission electron microscopy (TEM) study10.1016/j.matchar.2021.111236 ↗
54. Characterization of intermetallic compound at the interfaces of Al-steel resistance spot welds10.1016/j.jmatprotec.2016.11.017 ↗
55. Effect of silicon, manganese and nickel present in iron on the intermetallic growth at iron-aluminum alloy interface10.1016/j.jallcom.2018.07.364 ↗
56. In situ SEM, TEM, EBSD characterization of nucleation and early growth of pure Fe/pure Al intermetallic compounds10.3390/ma16176022 ↗
57. Development of new Fe–Al–Nb(–B) alloys for structural applications at high temperatures10.1557/s43580-021-00045-w ↗
58. On the formation of antiphase boundaries in Fe4Al13 intermetallics during a high temperature treatment10.1016/j.scriptamat.2022.114726 ↗
59. Microstructural and mechanical evolution of Al/steel interface with Fe2Al5 growth in resistance spot welding of aluminum to steel10.1016/j.jmapro.2018.06.024 ↗
60. The transition from discontinuous to continuous recrystallization in some aluminium alloys: I - the deformed state10.1016/j.actamat.2004.03.030 ↗
61. Microstructure, texture and mechanical properties of friction stir welded butt joints of 2A97 AlLi alloy ultra-thin sheets10.1016/j.jallcom.2016.08.330 ↗
62. Microstructure evolution and corrosion behavior of Fe-Al-based intermetallic aluminide coatings under acidic condition10.1016/S1003-6326(18)64847-2 ↗
63. Microstructural evolution and mechanical properties of friction stir welded butt joints of 5A06 alloy ultra-thin sheets10.3390/ma12233906 ↗
64. Deformation twinning feature and its effects on significant enhancement of tensile ductility in columnar-grained Fe–6.5wt.%Si alloy at intermediate temperatures10.1016/j.intermet.2011.12.011 ↗
65. The effect of grain size and grain orientation on deformation twinning in a Fe–22 wt.% Mn–0.6 wt.% C TWIP steel10.1016/j.msea.2010.02.041 ↗
66. Microstructural analysis of friction stir welded ferritic stainless steel10.1016/j.msea.2010.12.061 ↗
67. Sub-nanometer-scale mapping of crystal orientation and depth-dependent structure of dislocation cores in SrTiO310.1038/s41467-023-35877-7 ↗
68. Programming liquid crystal elastomers for multistep ambidirectional deformability10.1126/science.adq6434 ↗