Effect of TiC addition on the isothermal aging performance of Sn–Bi/Sn–Ag–Cu hybrid solder joints
Source abstract
Abstract
The demand for 3D packaging has grown with the drive toward high-performance, lightweight, and miniaturized electronics. However, issues such as warpage, interfacial delamination, and thermal stress accumulation intensify under repeated high-temperature bonding processes. The widely used Sn–3.0Ag–0.5Cu (SAC305) solder exacerbates these problems owing to its high melting point of 217 °C. Although Sn58Bi solder, with a low melting point of 139 °C, can mitigate thermal damage, its high Bi content induces brittleness and reduces long-term reliability owing to Bi segregation during isothermal aging. In this study, Sn58Bi–xTiC (x = 0, 0.1)/SAC305 hybrid solder joints were fabricated to investigate the effect of TiC nanoparticles on long-term reliability. Sn58Bi–xTiC (x = 0, 0.1) solder paste was printed onto Organic Solderability Preservative (OSP)-finished Cu pads, and reflowed with SAC305 solder balls at 185 °C. Subsequently, isothermal aging was conducted at 110 °C for up to 1000 h. With aging, the Cu 6 Sn 5 intermetallic compound (IMC) transformed from scallop-type to layer-type, with Cu 3 Sn growing underneath, and no Bi segregation was observed. TiC nanoparticles effectively suppressed IMC growth and grain coarsening, while delaying Bi-rich phase diffusion and agglomeration. Nanoindentation tests revealed that the hardness and elastic modulus decreased up to 100 h, followed by an increase, converging to ∼420 MPa and 53 GPa after 1000 h, respectively. TiC-containing joints exhibited higher values across all aging intervals. Shear tests confirmed that TiC-containing joints displayed higher shear strength and fracture energy after aging, with a persistent ductile fracture mode. These findings demonstrate that the addition of TiC nanoparticles is effective in enhancing the long-term reliability of Sn58Bi/SAC305 hybrid solder joints.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Electronic Packaging and Soldering Technologies · 3D IC and TSV technologies · Nanomaterials and Printing Technologies
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (39)
Show source-provided references
1. Enabling technologies for 3D integration: from packaging miniaturization to advanced stacked ICs
2. Challengeable mechanical issues in microelectronic packages for developments
3. Advances and challenges in 2D semiconductor devices for monolithic 3D integration10.1088/2053-1583/adf236 ↗
4. Enhancement of cooling performance in MEMS by modifying 3D packaging structure: a design, integration, analysis and test study10.1016/j.applthermaleng.2023.121758 ↗
5. 3D packaging and Moore's law10.1088/1742-6596/2798/1/012048 ↗
6. A review on the fabrication and reliability of three-dimensional integration technologies for microelectronic packaging: through-Si-via and solder bumping process10.3390/met11101664 ↗
7. Characterization of packaging warpage, residual stress and their effects on the mechanical reliability of IGBT power modules10.1016/j.engfailanal.2023.107517 ↗
8. Thermomechanical challenges of 2.5-D packaging: a review of warpage and interconnect reliability10.1109/TCPMT.2023.3317383 ↗
9. Optimization for warpage and residual stress due to reflow process in IGBT modules based on pre-warped substrate10.1016/j.mee.2015.04.019 ↗
10. A review of low-temperature solders in microelectronics packaging10.1109/TCPMT.2023.3271269 ↗
11. The status of low temperature solders
12. Effect of electric pulse incubation melt on solidified microstructures and mechanical properties of Sn58Bi alloy10.1007/s10854-023-11506-3 ↗
13. Low melting temperature Sn-Bi solder: effect of alloying and nanoparticle addition on the microstructural, thermal, interfacial bonding, and mechanical characteristics10.3390/met11020364 ↗
14. Effect of Bi segregation on the asymmetrical growth of Cu-Sn intermetallic compounds in Cu/Sn-58Bi/Cu sandwich solder joints during isothermal aging10.1007/s11664-013-2749-y ↗
15. Effect of pre-soldering temperatures on the microstructures and shear behaviors of SnBi-SAC/ENIG solder joints10.1007/s10854-024-12702-5 ↗
16. Analysis of SAC305/SnBi hybrid solder interface and comparison of the relationship between hardness and shear of solder
17. Design and performance evaluation of Sn58Bi/SAC305 layered composite solder for low-temperature applications10.3390/met15020185 ↗
18. Microstructure and shear behavior of solder joint with Sn58Bi/Sn3.0Ag0.5Cu/Cu superposition structure10.1007/s10854-019-01773-4 ↗
19. Sn-3.0Ag-0.5Cu/Sn-58Bi composite solder joint assembled using a low-temperature reflow process for PoP technology10.1016/j.matdes.2019.108144 ↗
20. A review: effect of nanoparticle additions on the physical, microstructural, interfacial and mechanical properties of low temperature SnBi solder alloys
21. Influences of doping Ti nanoparticles on microstructure and properties of Sn58Bi solder10.1007/s10854-019-02107-0 ↗
22. Effect of nanoparticles addition on the microstructure and properties of lead-free solders: a review10.3390/app9102044 ↗
23. Effect of silver (Ag) nanoparticle size on the microstructure and mechanical properties of Sn58Bi–Ag composite solders10.1016/j.jallcom.2015.05.023 ↗
24. Effect of adding Ni nanoparticles on the melting characteristics, mechanical properties and intermetallic compound growth of Sn58Bi solder10.1108/SSMT-09-2024-0053 ↗
25. Effects of TiC nanoparticle addition on microstructures and mechanical properties of Sn-58Bi solder joints10.1016/j.mtcomm.2024.109860 ↗
26. Microstructural, compositional and hardness evolutions of 96.5 Sn–3Ag–0.5 Cu/TiC composite solder under thermo-migration stressing10.1007/s10854-020-03491-8 ↗
27. Microstructure, mechanical properties, electrical conductivity and wear behavior of high volume TiC reinforced Cu-matrix composites10.1016/j.matchar.2008.09.014 ↗
28. Study on the electrical and mechanical properties of TiC particle-reinforced copper matrix composites regulated by different rare earth elements10.3390/nano15020096 ↗
29. Performance of Sn–3.0 Ag–0.5 Cu composite solder with TiC reinforcement: physical properties, solderability and microstructural evolution under isothermal ageing10.1016/j.jallcom.2016.05.245 ↗
30. Effect of isothermal aging on the microstructure, shear behavior and hardness of the Sn58Bi/Sn3.0Ag0.5Cu/Cu solder joints10.1016/j.rinp.2019.102701 ↗
31. Microstructure and mechanical properties of Sn58Bi composite solder reinforced with carbon nanotubes and nano-nickel10.1007/s10854-025-16023-z ↗
32. Microstructure evolution at the interface between Cu and eutectic Sn–Bi alloy with the addition of Ag or Ni10.1016/j.jmrt.2023.09.159 ↗
33. Solid-state diffusion of Bi in Sn: effects of anisotropy, temperature, and high diffusivity pathways10.1007/s11837-018-3145-0 ↗
34. Evolution of the microstructure of Sn58Bi solder paste with Sn-3.0Ag-0.5Cu addition during isothermal aging10.1007/s11664-018-06865-1 ↗
35. Effect of thermal aging on microstructural and shear-strength changes in Sn-3.0Ag-0.5Cu/Sn-58Bi solder joint10.1007/s10854-025-15277-x ↗
36. Investigation of isothermal aged Sn-3Ag-0.5Cu/Sn58Bi-Co hybrid solder joints on ENIG and ENEPIG substrate with various mechanical performances
37. Effect of multiple reflow cycles and isothermal aging on shear strength in SAC305/Sn58Bi/Cu-OSP hybrid solder joint
38. Al2O3 nanofibers reinforced Sn58Bi/SAC305 hybrid joints for low temperature ball grid array bonding
39. A new low-temperature solder assembly technique to replace eutectic Sn-Bi solder assembly10.3390/mi13060867 ↗