The effect of minor Ti and Mn additions on the microstructure and mechanical properties of additive manufactured Al–Ce–Mg alloys
Source abstract
Abstract
The Al–Ce-based alloys have gained increasing attentions owing to their favorable properties of high castability and good thermal stability, as well as excellent mechanical performance. However, since Ce has high chemical activity, it tends to bond with other impurities from the raw materials and affect the properties. In the present study, the influence of Ti and Mn impurities on the microstructure and mechanical properties of Al–Ce–Mg alloys was investigated. Both Al–Ce–Mg and Al–Ce–Mg–Ti–Mn alloys exhibit good formability traits during directed energy deposition additive manufacturing. Mechanical testing indicated that Ti and Mn significantly reduce the ductility by forming rosette-shaped Al20Ce(Ti, Mn)2 ternary intermetallic compounds, which provide favorable sites for the crack initiation in Al–Ce–Mg sample with Ti and Mn impurities. Compared to traditional hot extrusion, the lower solidification rate of direct energy deposition additive manufacturing coarsens the Al11Ce3 precipitates that compromise the strength but enhance the elongation in the sample without Ti and Mn addition.
Source: expertdata · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Additive Manufacturing Materials and Processes · Additive Manufacturing and 3D Printing Technologies · Aluminum Alloys Composites Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (26)
Show source-provided references
1. Meng F, Chaudhary RP, Gandha K et al (2018) Rapid assessment of the Ce-Co-Fe-Cu system for permanent magnetic applications. JOM 70:872–878. https://doi.org/10.1007/s11837-018-2862-810.1007/s11837-018-2862-8 ↗
2. Sims ZC, Weiss D, McCall SK et al (2016) Cerium-based, intermetallic-strengthened aluminum casting alloy: high-volume co-product development. JOM 68:1940–1947. https://doi.org/10.1007/s11837-016-1943-910.1007/s11837-016-1943-9 ↗
3. Stromme ET, Henderson HB, Sims ZC et al (2018) Ageless aluminum-cerium-based alloys in high-volume die casting for improved energy efficiency. JOM 70:866–871. https://doi.org/10.1007/s11837-018-2861-910.1007/s11837-018-2861-9 ↗
4. Sims ZC, Rios OR, Weiss D et al (2017) High performance aluminum–cerium alloys for high-temperature applications. Mater Horiz 4:1070–1078. https://doi.org/10.1039/C7MH00391A10.1039/C7MH00391A ↗
5. Vončina M, Kores S, Mrvar P, Medved J (2011) Effect of Ce on solidification and mechanical properties of A360 alloy. J Alloy Compd 509:7349–7355. https://doi.org/10.1016/j.jallcom.2011.04.05910.1016/j.jallcom.2011.04.059 ↗
6. Olakanmi EO, Cochrane RF, Dalgarno KW (2011) Densification mechanism and microstructural evolution in selective laser sintering of Al–12Si powders. J Mater Process Technol 211:113–121. https://doi.org/10.1016/j.jmatprotec.2010.09.00310.1016/j.jmatprotec.2010.09.003 ↗
7. Olakanmi EO, Cochrane RF, Dalgarno KW (2015) A review on selective laser sintering/melting (SLS/SLM) of aluminium alloy powders: processing, microstructure, and properties. Prog Mater Sci 74:401–477. https://doi.org/10.1016/j.pmatsci.2015.03.00210.1016/j.pmatsci.2015.03.002 ↗
8. Sames WJ, List FA, Pannala S, Dehoff RR, Babu SS (2016) The metallurgy and processing science of metal additive manufacturing. Int Mater Rev 61:315–360. https://doi.org/10.1080/09506608.2015.111664910.1080/09506608.2015.1116649 ↗
9. Wu Z, Wu S, Qian W et al (2023) Structural integrity issues of additively manufactured railway components: progress and challenges. Eng Fail Anal 149:107265. https://doi.org/10.1016/j.engfailanal.2023.10726510.1016/j.engfailanal.2023.107265 ↗
10. Mertens AI, Delahaye J, Lecomte-Beckers J (2017) Fusion‐based additive manufacturing for processing aluminum alloys: state‐of‐the‐art and challenges. Adv Eng Mater 19:1700003. https://doi.org/10.1002/adem.20170000310.1002/adem.201700003 ↗
11. Spierings AB, Dawson K, Kern K, Palm F, Wegener K (2017) SLM-processed Sc-and Zr-modified Al-Mg alloy: mechanical properties and microstructural effects of heat treatment. Mater Sci Eng A 701:264–273. https://doi.org/10.1016/j.msea.2017.06.08910.1016/j.msea.2017.06.089 ↗
12. Croteau JR, Griffiths S, Rossell MD et al (2018) Microstructure and mechanical properties of Al-Mg-Zr alloys processed by selective laser melting. Acta Mater 153:35–44. https://doi.org/10.1016/j.actamat.2018.04.05310.1016/j.actamat.2018.04.053 ↗
13. Plotkowski A, Rios O, Sridharan N et al (2017) Evaluation of an Al-Ce alloy for laser additive manufacturing. Acta Mater 126:507–519. https://doi.org/10.1016/j.actamat.2016.12.06510.1016/j.actamat.2016.12.065 ↗
14. Totten GE, Scott MacKenzie D (2003) Handbook of Aluminum: Vol. 1: Physical Metallurgy and Processes. CRC Press10.1201/9780203912607 ↗
15. Perrin AE, Michi RA, Leonard DN et al (2023) Effect of Mn on eutectic phase equilibria in Al-rich Al-Ce-Ni alloys. J Alloy Compd 965:171455. https://doi.org/10.1016/j.jallcom.2023.17145510.1016/j.jallcom.2023.171455 ↗
16. Czerwinski F (2020) Cerium in aluminum alloys. J Mater Sci 55:24–72. https://doi.org/10.1007/s10853-019-03892-z10.1007/s10853-019-03892-z ↗
17. Henderson HB, Hammons JA, Baker AA et al (2021) Enhanced thermal coarsening resistance in a nanostructured aluminum-cerium alloy produced by additive manufacturing. Mater Des 209:109988. https://doi.org/10.1016/j.matdes.2021.10998810.1016/j.matdes.2021.109988 ↗
18. Mercelis P, Kruth JP (2006) Residual stresses in selective laser sintering and selective laser melting. Rapid Prototyp J 12:254–265. https://doi.org/10.1108/1355254061070701310.1108/13552540610707013 ↗
19. Gremaud M, Carrard M, Kurz W (1990) The microstructure of rapidly solidified Al Fe alloys subjected to laser surface treatment. Acta Metall Mater 38:2587–2599. https://doi.org/10.1016/0956-7151(90)90271-H10.1016/0956-7151(90)90271-H ↗
20. Scipioni Bertoli U, Guss G, Wu S, Matthews MJ, Schoenung JM (2017) In-situ characterization of laser-powder interaction and cooling rates through high-speed imaging of powder bed fusion additive manufacturing. Mater Des 135:385–396. https://doi.org/10.1016/j.matdes.2017.09.04410.1016/j.matdes.2017.09.044 ↗
21. Niemann S, Jeitschko W (1995) Ternary aluminides AT2Al20 (A= rare earth elements and uranium; T= Ti, Nb, Ta, Mo, and W) with CeCr2Al20-type structure. J Solid State Chem 114:337–341. https://doi.org/10.1006/jssc.1995.105210.1006/jssc.1995.1052 ↗
22. Plotkowski A, Sisco K, Bahl S et al (2020) Microstructure and properties of a high temperature Al–Ce–Mn alloy produced by additive manufacturing. Acta Mater 196:595–608. https://doi.org/10.1016/j.actamat.2020.07.01410.1016/j.actamat.2020.07.014 ↗
23. Kangas MJ, Schmitt DC, Sakai A, Nakatsuji S, Chan JY (2012) Structure and physical properties of single crystal PrCr2Al20 and CeM2Al20 (M= V, Cr): a comparison of compounds adopting the CeCr2Al20 structure type. J Solid State Chem 196:274–281. https://doi.org/10.1016/j.jssc.2012.06.03510.1016/j.jssc.2012.06.035 ↗
24. Winiarski MJ, Wiendlocha B, Sternik M et al (2016) Rattling-enhanced superconductivity in M V2 Al20 (M= Sc, Lu, Y) intermetallic cage compounds. Phys Rev B 93:134507. https://doi.org/10.1103/PhysRevB.93.13450710.1103/PhysRevB.93.134507 ↗
25. Wu Z, Wu S, Bao J et al (2021) The effect of defect population on the anisotropic fatigue resistance of AlSi10Mg alloy fabricated by laser powder bed fusion. Int J Fatigue 151:106317. https://doi.org/10.1016/j.ijfatigue.2021.10631710.1016/j.ijfatigue.2021.106317 ↗
26. Ma H, Zhang X, Liu C, Zhao L, Jiang W (2019) Structural, elastic, anisotropic and thermodynamic properties of the caged intermetallics RETi2Al20 (RE= La, Ce, Gd and Ho): a first-principles study. Solid State Sci 89:121–129. https://doi.org/10.1016/j.solidstatesciences.2018.12.02310.1016/j.solidstatesciences.2018.12.023 ↗