A study on the microstructure and property development of d.c. magnetron cosputtered ternary titanium aluminium nitride coatings Part III effect of substrate bias voltage and temperature
Source abstract
Abstract
Advanced ternary (Ti,Al)N coatings were produced by reactive magnetron co-sputtering technique with separate titanium and aluminium targets at a 30° magnetron configuration under various substrate bias voltages and temperatures. The effect of substrate bias and temperature on the microstructure and property development of the coatings was investigated. It was found that an increase in substrate bias and/or substrate temperature imposed no major effect on the composition and phase formation of the (Ti,Al)N coatings, but had significant influence on the development of their microstructure and surface morphology. As the substrate bias and/or temperature increased, the coating structure was densified with development of fine grain size and reduced surface roughness, resulting in a substantial increase of the coating hardness. However as the substrate bias increased over 200 volts, excessive residual stress was built up, causing a fracture of the coatings. It is believed that the microstructure and property enhancement is attributed to an increased translational kinetic energy of the depositing atoms and a greater thermal energy provided to the substrate and the coating material with increasing substrate bias and/or temperature. The adatom mobility and the surface diffusion of atoms are enhanced to reduce the detrimental effects induced by the statistical roughening and self-shadowing of asputter deposition process. A densified zone T structure with low porosity and improved properties is produced.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Metal and Thin Film Mechanics · GaN-based semiconductor devices and materials · Semiconductor materials and devices
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (24)
Show source-provided references
1. J. E. SUNDGREN, B. O. JOHANSSON, H. T. G. HENTZELL and S. E. KARLSSON, Thin Solid Films 105 (1983) 385.10.1016/0040-6090(83)90320-6 ↗
2. W. D. SPROUL, P. J. RUDNIK, C. A. GOGOL and R. A. MUELLER, Surf. Coat. Technol. 39/40 (1989) 499.10.1016/S0257-8972(89)80011-8 ↗
3. W. D. SPROUL, P. J. RUDNIK and M. E. GRAHAM, ibid. 39/40 (1989) 355.10.1016/0257-8972(89)90068-6 ↗
4. W. D. SPROUL, P. J. RUDNIK, M. E. GRAHAM and S. L. ROHDE, ibid. 43/44 (1990) 270.10.1016/0257-8972(90)90080-V ↗
5. F. RICHTER, H. KUPFER, H. GEIGENGACK, G. SCHAARSCHMIDT, F. SCHOLZE, F. ELSTNER and G. HECHT, ibid. 54/55 (1992) 338.10.1016/0257-8972(92)90185-D ↗
6. D. S. RICKERBY and P. J. BURNETT, Thin Solid Films 157 (1988) 195.10.1016/0040-6090(88)90004-1 ↗
7. S. L. ROHDE, W. D. SPROUL and J. R. ROHDE, J. Vac. Sci. Technol. A9 (1991) 1178.10.1116/1.577598 ↗
8. J. MUSIL, V. POULEK, V. VALVODA, R. JR. KUZEL, H. A. JEHN and M. E. BAUMGARTNER, Surf. Coat. Technol. 60 (1993) 484.10.1016/0257-8972(93)90137-D ↗
9. J. A. THORNTON, J. Vac. Sci. Technol. 11 (1974) 666.10.1116/1.1312732 ↗
10. H. FRELLER and H. HASSLER, Surf. Coat. Technol. 36 (1988) 219.10.1016/0257-8972(88)90152-1 ↗
11. B. F. COLL, P. SATHRUM, R. FONTANA, J. P. PEYRE, D. DUCHATEAU and M. BENMALEK, ibid. 52 (1992) 57.10.1016/0257-8972(92)90371-G ↗
12. J. R. ROOS, J. P. CELIS, E. VANCOILLE, H. VELTROP, S. BOELENS, F. JUNGBLUT, J. EBBERINK and H. HOMBERG, Thin Solid Films 193/194 (1990) 547.10.1016/S0040-6090(05)80064-1 ↗
13. G. HAKANSSON, J. E. SUNDGREN, D. MCINTYRE, J. E. GREEN and W. D. MUNZ, ibid. 153 (1987) 55.10.1016/0040-6090(87)90169-6 ↗
14. L. COMBADIERE and J. MACHET, Surf. Coat. Technol. 88 (1996) 17.10.1016/S0257-8972(96)02870-8 ↗
15. Idem., ibid. 88 (1996) 28.10.1006/bare.1996.0005 ↗
16. L. MENG, M. ANDRITSCHKY and M. P. DOS SANTOS, Thin Solid Films 223 (1993) 242.10.1016/0040-6090(93)90528-W ↗
17. Y. K. WANG, X. Y. CHENG, W. M. WANG, X. H. GU, L. F. XIA, T. C. LEI and W. H. LUI, Surf. Coat. Technol. 72 (1995) 71.10.1016/0257-8972(94)02331-J ↗
18. R. MESSIER, A. P. GIRI and R. A. ROY, J. Vac. Sci. Technol. A2 (1984) 500.10.1116/1.572604 ↗
19. R. MESSIER, ibid. A4 (1986) 490.10.1116/1.573866 ↗
20. G. HAKANSSON, L. HULTMAN, J. E. SUNDGREN, J. E. GREEN and W. D. MUNZ, Surf. Coat. Technol. 48 (1991) 51.10.1016/0257-8972(91)90128-J ↗
21. D. L. SMITH, in “Thin-Film Deposition: Principles and Practice” (McGraw-Hill, New York, 1995) p. 162.
22. K. H. MULLER, Phys. Rev. 35 (1987) 7906.10.1103/PhysRevB.35.7906 ↗
23. Idem., J. Appl. Phys. 62 (1987) 1796.10.1063/1.339559 ↗
24. O. KNOTEK, R. ELSING, G. KRAMER and F. JUNGBLUT, Surf. Coat. Technol. 46 (1991) 265. Received 18 June and accepted 18 December 2001 200410.1016/0257-8972(91)90169-W ↗