Abstract

The wettability of low-carbon, 0.3 wt%Si–0.4 wt%Mn interstitial-free steel by liquid zinc at 450 °C was investigated using the dispensed sessile drop method. Before the wetting tests, the steel samples were annealed in a 15%H2–Ar gas atmosphere at three different dew points, namely −60, −40, and 0 °C. It was found that as the dew point was increased from −60 to −40 °C, the wettability became poorer. However, as the dew point was increased further to 0 °C, the wettability was dramatically improved and was better than that of −60 °C. In order to understand the dramatic change in wettability, the surfaces of the steel samples after annealing were analyzed with SEM and TEM. It was found that the surface oxide changed from randomly distributed hemisphere particles of 20–30-nm high on a very thin oxide film to a film-like layer ~15-nm thick as the dew point was increased from −60 to −40 °C, and at the dew point of 0 °C, internal oxidation was so pronounced that a very thin surface oxide layer 1–2-nm thick was formed. It was believed that the improvement of the wettability at the dew point of 0 °C was caused by the short diffusion distance in the surface oxide layer.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Corrosion Behavior and Inhibition · Metal and Thin Film Mechanics · High-Temperature Coating Behaviors

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (21)

Show source-provided references
1. Kyono K, Kato C, Sakata K (2003) Kawasaki Steel Tech Rep 35:33
2. Pichler A, Traint S, Arnolder G, Stiaszny P, Blaimschein M, Werner EA (2003) Iron Steelmaker 30(6):21
3. Lee J, Matsuoka K, Shimada S, Tanaka T (2004) 6th international conference on zinc and zinc alloy coated sheet steels. Association for Iron & Steel Technology, Warrendale, p 987
4. Lee J, Park J, Jeon SH (2009) Metall Mater Trans B 40B:103510.1007/s11663-009-9288-1 ↗
5. Mataigne JM, Lamberigts M, Leroy V (1992) In: Pradhan R, Gupta I (eds) Developments in the annealing of sheet steels. TMS, Warrendale
6. Yamashita T, Yamamoto A, Kato C (1994) CAMP-ISIJ 7:388
7. Kato C, Sekine T, Umino S, Yamashita T, Mochizuki K, Masuda M (1994) CAMP-ISIJ 7:1511
8. Cassie ABD (1948) Discuss Frad Soc 3:1110.1039/df9480300011 ↗
9. Hirose Y, Togawa H, Sumiya J (1982) Tetsu-to-Hagané 68:65810.2355/tetsutohagane1955.68.6_658 ↗
10. Bordignon L (2007) Rev Metall 104:30010.1051/metal:2007119 ↗
11. Zakharova TV, Popel SI (1972) Iz VUZ Chern Metall 3:17
12. Ebrill N, Durandet Y, Strezov L (2000) Metall Mat Trans B 31:106910.1007/s11663-000-0082-3 ↗
13. Shimada S, Takada Y, Lee J, Tanaka T (2008) ISIJ Int 48:124610.2355/isijinternational.48.1246 ↗
14. Takada Y, Shimada S, Lee J, Kurosaki M, Tanaka T (2009) ISIJ Int 49:10010.2355/isijinternational.49.100 ↗
15. Li XS, Baek S-I, Oh C-S, Kim S-J, Kim Y-W (2008) Scripta Mater 59:29010.1016/j.scriptamat.2008.03.025 ↗
16. Khondker R, Mertens A, McDermid JR (2007) Mater Sci Eng A 463:15710.1016/j.msea.2006.09.116 ↗
17. Gong YF, Kim HS, De Cooman BC (2008) ISIJ Int 48:174510.2355/isijinternational.48.1745 ↗
18. Protsenko P, Terlain A, Traskine V, Eustathopoulos N (2001) Scripta Mater 45:143910.1016/S1359-6462(01)01181-2 ↗
19. Ueda S, Taguchi O, Iijima Y, Takahashi G, Yamaguchi K (2008) J Mater Sci 43:5666. doi: 10.1007/s10853-008-2767-y10.1007/s10853-008-2767-y ↗
20. Wagner C (1959) Z Elektrochem 63:772
21. Lide DR (2005–2006) CRC handbook of chemistry and physics. Taylor & Francis, Boca Raton