The effect of high-temperature heat-treatment on the strength of C/C–SiC joints

Xiaofei Chen, Shujie Li, Zhijun Chen, Ning Wen

Journal of Materials Science· Volume 46· Issue 3
Publisher page

Abstract

Joining of carbon fiber reinforced C–SiC dual matrix composite (denoted by C/C–SiC) is critical for its aeronautical and astronautical applications. Joining of C/C–SiC has been realized through a reaction joining process using boron-modified phenolic resin with micro-size B4C and nano-size SiO2 powder additives. The effect of the heat-treatment temperature on the retained strength of the joints, calculated by dividing the strength of the heat-treated joints by the strength of the joints before heat-treatment, was studied. The maximum retained strength of the joints is as high as 96.0% after the heat-treatment at 1200 °C for 30 min in vacuum, indicating good heat resistance of the joints. The thickness of the interlayer of the joint after the heat-treatment is about 18 μm and it is uniform and densified. There are no obvious cracks or pores at the interfaces. During the heat-treatment, carbon, oxygen, silicon, and boron diffuse at the interfacial area. The interlayer is composed of B4C, SiO2, glassy carbon, amorphous B2O3, and borosilicate glass. SiC appears in the interlayer of the joint heat-treated at 1400 °C for 30 min in vacuum. The addition of B4C and SiO2 powders contributes to the densification of the interlayer, the bonding at the interfaces and the heat resistance of the joints.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · Fiber-reinforced polymer composites

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (20)

Show source-provided references
1. Asthana R, Singh M (2008) J Eur Ceram Soc 28:61710.1016/j.jeurceramsoc.2007.06.017 ↗
2. Asthana R, Singh M (2009) Scr Mater 61:25710.1016/j.scriptamat.2009.03.053 ↗
3. Shirzadi AA, Zhu Y, Bhadeshia HKDH (2008) Mater Sci Eng A 496:50110.1016/j.msea.2008.06.007 ↗
4. Mustafa A (2008) J Fac Eng Archit Gazi Univ 23:595
5. Halbig MC, Singh M, Shpargel TP, Kiser JD (2006) Ceram Eng Sci Proc 27:13310.1002/9780470291313.ch13 ↗
6. Li SJ, Duan HP, Liu S, Zhang YG, Dang ZJ, Zhang Y, Wu CG (2000) Int J Refract Met Hard Mater 18:3310.1016/S0263-4368(00)00008-1 ↗
7. Lu YW, Zhang YD, Hu HF, Zhang CR (2008) Key Eng Mater 368–372:104410.4028/www.scientific.net/KEM.368-372.1044 ↗
8. Li SJ, Liu WH, Lu YK, Li XG, Mao YW (2008) Acta Mater Compos Sin 25:72
9. Hernández-Padrón G, Rojas F, Castaño V (2006) Surf Coat Technol 201:120710.1016/j.surfcoat.2006.01.070 ↗
10. Abidzina V, Tereshko I, Elkin I, Muntele I, Muntele C, Minamisawa RA (2007) Methods Phys Res Sect B 257:523
11. Gadiou R, Serverin S, Gibot P, Vix-Guterl C (2008) J Eur Ceram Soc 28:226510.1016/j.jeurceramsoc.2008.02.022 ↗
12. Cermignani W, Palulson TE, Onneby C, Pantano C (1995) Carbon 4:36710.1016/0008-6223(94)00160-2 ↗
13. Jacques S, Guette A, Bourrat X, Langlais F, Guimon C, Labrugere C (1996) Carbon 9:113510.1016/0008-6223(96)00075-9 ↗
14. Trick KA, Saliba TF (1995) Carbon 11:l509
15. Wang JG, Jiang N, Guo QG, Liu L, Song JR (2006) J Nucl Mater 348:10810.1016/j.jnucmat.2005.09.008 ↗
16. Sheehan JE (1989) Carbon 27:70910.1016/0008-6223(89)90204-2 ↗
17. Wang JG, Jiang N, Jiang HY (2006) Int J Adhes Adhes 26:53210.1016/j.ijadhadh.2005.07.005 ↗
18. Myalski J, Sleziona J (2006) J Mater Process Technol 175:29110.1016/j.jmatprotec.2005.04.054 ↗
19. Cheng LF, Xu YD, Zhang LT, Yin XW (2002) J Mater Sci 37:5339. doi: 10.1023/A:102108941114110.1023/A:1021089411141 ↗
20. Wang DC, Chang GW, Chen Y (2008) Polym Degrad Stab 93:12510.1016/j.polymdegradstab.2007.10.021 ↗