journal article·2021-04

Achieving high energy storage density of PLZS antiferroelectric within a wide range of components

Yucheng Liu, Shaopeng Liu, Tongqing Yang, Hongsheng Wang

Journal of Materials Science· Volume 56· Issue 10
Publisher page

Abstract

In this paper, (Pb0.98La0.02) (ZrxSn1-x)0.995 O3 (PLZS) antiferroelectric materials with different Zr/Sn ratios were fabricated by means of the rolling process, and the effects of Zr/Sn ratio on the phase structure and dielectric properties were systemically studied. All samples exhibited an orthorhombic structure. Furthermore, the results showed that the ABO3 phase structure could be easily formed when the Zr/Sn ratio was close to 1:1. The saturation polarization strength and the energy storage density increased with increasing Zr content, reaching peak value of 36 μC/cm2 and 9.5 J/cm3 at 0.49 and 0.55, respectively, and then decreased with a further increase of the Zr content. Besides, with increasing Zr content, the energy storage efficiency initially maintained a stable value of ~ 90% and then gradually decreased. The switching electric field of these materials was around 30 kV/mm and increased slightly with increasing Zr content. For all these samples, the dependence of dielectric constant on temperature varied similarly. A new intermediate state named “multicell cubic” appeared during the phase transition from the antiferroelectric phase to the paraelectric phase, which was different from the phase transition of traditional antiferroelectric materials. Moreover, the Curie temperature increased with increasing Zr content and then decreased. Based on the above result, PLZS AFEs could be a promising high-power energy storage material.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Ferroelectric and Piezoelectric Materials · Acoustic Wave Resonator Technologies · Dielectric materials and actuators

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (25)

Show source-provided references
1. Kittel C (1951) Theory of antiferroelectric crystals. Phys Rev 82:729–73210.1103/PhysRev.82.729 ↗
2. Sawaguchi E, Maniwa H, Hoshino S (1951) Antiferroelectric structure of lead zirconate. Phys Rev 83:107810.1103/PhysRev.83.1078 ↗
3. Jaffe B (1961) Antiferroelectric ceramics with field-enforced transitions: a new nonlinear circuit element. Proc Ire 49:1264–126710.1109/JRPROC.1961.287917 ↗
4. Sawaguchi E (1953) Ferroelectricity versus Antiferroelectricity in the Solid Solutions of PbZrO3 and PbTiO3. J Phys Soc Jpn 8:615–62910.1143/JPSJ.8.615 ↗
5. Berlincourt D, Krueger HHA, Jaffe B (1964) Stability of phases in modified lead zirconate with variation in pressure, electric field, temperature and composition. J Phys Chem Solids 25:659–67410.1016/0022-3697(64)90175-1 ↗
6. Dai X, Xu Z, Viehland D (1995) Phase stability and transformations in pure and lanthanum modified lead zirconate ceramics. J Appl Phys 77:5086–509410.1063/1.359317 ↗
7. Cai H, Yan S, Zhou M, Liu N, Ye J, Li S (2019) Significantly improved energy storage properties and cycling stability in La-doped PbZrO3 antiferroelectric thin films by chemical pressure tailoring. J Eur Ceram Soc 39:4761–476910.1016/j.jeurceramsoc.2019.07.024 ↗
8. Qi X, Chen H, Deng B, Zhao J, Wei M, Gao L (2019) Energy-storage properties of Sr-doped PLZST bulk ceramics and thick films. J Mater Sci Mater Electron 30:17916–1792210.1007/s10854-019-02144-9 ↗
9. Kainz T, Bitschnau B, Mautner FA, Reichmann K (2016) Comparison of lanthanum and bismuth modification of lead zirconate-lead titanate PZT—a structural and dielectric study. J Eur Ceram Soc 36:507–51410.1016/j.jeurceramsoc.2015.10.008 ↗
10. Zhang Q, Tong H, Chen J, Lu Y, Yang T, Yao X (2016) High recoverable energy density over a wide temperature range in Sr modified (Pb, La)(Zr, Sn, Ti)O3 antiferroelectric ceramics with an orthorhombic phase. Appl Phys Lett 109:26290110.1063/1.4973425 ↗
11. Jinfei W, Tongqing Y, Shengchen C, Gang L, Xi Y (2012) Characteristics and dielectric properties of (Pb0.97−xLa0.02Bax)(Zr0.72Sn0.22Ti0.06)O3 ceramics. J Alloys Compd 539:280–28310.1016/j.jallcom.2012.06.028 ↗
12. Ciuchi IV, Craciun F, Mitoseriu L, Galassi C (2015) Preparation and properties of La doped PZT 90/10 ceramics across the ferroelectric–antiferroelectric phase boundary. J Alloys Compd 646:16–2210.1016/j.jallcom.2015.05.119 ↗
13. Qiao P, Zhang Y, Chen X, Zhou M, Yan S, Dong X (2019) Enhanced energy storage properties and stability in (Pb0.895La0.07)(ZrxTi1-x)O3 antiferroelectric ceramics. Ceram Int 45:15898–1590510.1016/j.ceramint.2019.05.096 ↗
14. Bd A (1996) Transducers using forced transitions between ferroelectric and antiferroelectric states. IEEE Trans Sonics Ultrasonics 13:116–124
15. Jiang S, Zhang L, Zhang G, Liu S, Yi J, Xiong X (2013) Effect of Zr: Sn ratio in the lead lanthanum zirconate stannate titanate anti-ferroelectric ceramics on energy storage properties. Ceram Int 39:5571–557510.1016/j.ceramint.2012.12.071 ↗
16. Wang X, Yang T, Shen J, Damjanovic D (2016) High-energy storage performance in (Pb0.98La0.02)(Zr0.45Sn0.55)0.995O3 AFE thick films fabricated via a rolling process. J Am Ceram Soc 99:3569–357210.1111/jace.14406 ↗
17. Wang H, Liu Y, Yang T, Zhang S (2019) Ultrahigh energy-storage density in antiferroelectric ceramics with field-induced multiphase transitions. Adv Funct Mater 29:180732110.1002/adfm.201807321 ↗
18. Breval EWC, Dougherty JP (2005) PLZT phases near lead zirconate: 1. Determination by X-ray diffraction. J Am Ceram Soc 2:437–44210.1111/j.1551-2916.2005.00102.x ↗
19. Breval E, Wang C, Dougherty JP, Yilmazbayhan A, Gachigi KWA, Stewart M (2006) PLZT phases near lead zirconate: 2. Determination by capacitance and polarization. J Am Ceram Soc 89:3681–368810.1111/j.1551-2916.2006.01320.x ↗
20. Dan Y, Xu H, Zou K, Zhang Q, Lu Y, Chang G (2018) Energy storage characteristics of (Pb, La)(Zr, Sn, Ti)O3 antiferroelectric ceramics with high Sn content. Appl Phys Lett 113:06390210.1063/1.5044712 ↗
21. Dan Y, Zou K, Chen G, Yu Y, Zhang Y, Zhang Q (2019) Superior energy-storage properties in (Pb, La)(Zr, Sn, Ti)O3 antiferroelectric ceramics with appropriate La content. Ceram Int 45:11375–1138110.1016/j.ceramint.2019.03.001 ↗
22. Tan X, Ma C, Frederick J, Beckman S, Webber KG, Green DJ (2011) The antiferroelectric ↔ ferroelectric phase transition in lead-containing and lead-free perovskite ceramics. J Am Ceram Soc 94:4091–410710.1111/j.1551-2916.2011.04917.x ↗
23. Liu X, Li Y, Sun N, Hao X (2020) High energy-storage performance of PLZS antiferroelectric multilayer ceramic capacitors. Inorg Chem Front 7:756–76410.1039/C9QI01416K ↗
24. Viehland D, Forst D, Li JF (1994) Compositional heterogeneity and the origins of the multicell cubic state in Sn-doped lead zirconate titanate ceramics. J Appl Phys 75:4137–414310.1063/1.355995 ↗
25. Viehland DFD, Xu Z (1995) Incommensurately modulated polar structures in antiferroelectric Sn-modified lead zirconate titanate: the modulated structure and its influences on electrically induced polarizations and strains. J Am Ceram Soc 78:2101–211210.1111/j.1151-2916.1995.tb08622.x ↗