Mechanisms of temper embrittlement and recovery in cast HY-80 high-strength low-alloy steel
Source abstract
Abstract
To better understand the mechanisms and rate of temper embrittlement in cast HY-80 high-strength low-alloy steel, samples were subjected to embrittlement and recovery treatments after a typical industrial heat treatment. The embrittlement rate was studied between 315 and 565 °C at varied logarithmic time intervals up to 10000 min. The embrittlement recovery rate was studied between 593 and 704 °C at logarithmic time intervals up to 1000 min. Metallographic and computational work for these samples supports a conclusion that the observed embrittlement and subsequent recovery cannot be solely explained by the segregation of phosphorus and other embrittling elements to grain boundaries as has been previously suspected in this alloy system. Rather it is shown that alloy carbides such as M23C6 play a key role in embrittlement, whereas carbide coarsening and/or nucleation at the prior austenite grain boundaries and in the bulk in the embrittling temperature range. The evolution of these carbides serves both to create initiation sites for cleave and depletes the matrix of Mo, which is a P scavenger. Recovery from embrittlement is thus proposed to be related to both the removal of P from the boundary and the dissolution of carbides from the boundary. Earlier work showing the suspected maximum embrittlement rate occurs at 482 °C with the maximum recovery rate at 648 °C has been rigorously confirmed for a high carbon equivalent cast chemical composition.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Microstructure and Mechanical Properties of Steels · High Temperature Alloys and Creep · Metal Alloys Wear and Properties
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (13)
Show source-provided references
1. Viswanathan R, Sherlock TP (1972) Long-time isothermal temper embrittlement in Ni–Cr–Mo–V steels. Metall Mater Trans B 3(2):463–47210.1007/BF02642050 ↗
2. Kula EB, Anctil AA (1967) Tempered martensite embrittlement and fracture toughness in 4340 steel. Defense Technical Information Center, Fort Belvoir10.21236/AD0651066 ↗
3. Horn RM, Ritchie RO (1978) Mechanisms of tempered martensite embrittlement in low alloy steels. Metall Trans A 9(8):1039–105310.1007/BF02652208 ↗
4. Wu R, Freeman AJ (1994) Nature of phosphorus embrittlement of the FeZ3 110 (111) grain boundary. Phys Rev 50:75–7910.1103/PhysRevB.50.75 ↗
5. Willner AR, Salive ML (1966) Effects of tempering above the lower critical temperature a sub C1 on the properties of an HY-80 steel. Defense Technical Information Center, Fort Belvoir10.21236/AD0628979 ↗
6. Salive ML, Willner AR (1962) Comparison of standard and subsize HY-80 dropweight specimens for various conditions of heat treatment. Department of the Navy, David Taylor Model Basin, Washington, DC, p 18
7. Salive M (1972) Effects of microstructure, composition, and strength on the NIL ductility transition (NDT) temperature of HY-80 steel. Naval Ship Research and Development Center
8. Willner AR, Salive ML (1961) The effects of austenitizing and tempering on the mechanical properties of fully quenched HY-80 steels. Naval Ship Research and Development Center
9. Willner AR, Salive ML (1965) The effects of tempered non-martensitic products on the notch toughness and mechanical properties of an HY-80 steel. Naval Ship Research and Development Center
10. Willner AR, Salive ML (1964) Evaluation of commercially produced HY-80 Steel. Naval Ship Research and Development Center
11. Bandyopadhyay N, Briant CL, Hall EL (1985) Carbide precipitation, grain boundary segregation, and temper embrittlement in NiCrMoV rotor steels. Metall Trans A 16(5):721–73710.1007/BF02814824 ↗
12. Dépinoy S et al (2017) Carbide precipitation in 2.25 Cr-1 Mo bainitic steel: effect of heating and isothermal tempering conditions. Metall Mater Trans A 48(5):2164–217810.1007/s11661-017-4045-6 ↗
13. Draper MC (2013) Control of monatomic hydrogen in high strength steel castings. In: Steel Founders Society of America T&O proceedings, p 17