Deformation and fracture behavior of an Al–Li alloy 8090
Source abstract
Abstract
The effect of microstructure on the deformation mode and fracture behavior of age-hardened alloys has been the topic of many investigations. The deformation behavior could be modified by varying the aging condition. In the underaged (UA) condition, precipitate shearing tends to lead to an inhomogeneous distribution of slip, whereas, in the overaged (OA) condition, precipitate bypass by dislocations tends to homogenize the slip distribution [1–5]. Varying the aging condition also alters the grain boundary structure. If aging is continued, precipitate free zone (PFZ) adjacent to the grain boundaries widens and the grain boundary precipitates coarsen. This effect, together with changes of slip distribution, influences the tensile properties, fatigue properties, and fracture behavior of the alloys. In commercial age-hardened Al alloys, Mn, Cr, or Zr are usually added to form dispersoids. These dispersoids are incoherent with the matrix and can not be sheared by dislocations. Dispersoids bypassing would promote homogeneous distribution of slip. Dispersoids can also inhibit recrystallization so as to improve the toughness and stress corrosion cracking resistance of the alloys. At present, Al–Li-based alloys are used in industry. The addition of Li can increase the specific strength and specific stiffness and decrease the weight of the structures. The microstructure and mechanical properties of the alloys have been studied extensively [6]. However, the effect of slip distribution on the fracture behavior is not yet available. A commercial Al–Li–Cu–Mg–Zr alloy was used in this work to study the influences of microstructure on slip distribution and fracture behavior. The alloy 8090 (Al–2.43Li–1.17Cu–0.74Mg– 0.12Zr–0.09Fe–0.09Si–0.03Ti, all wt.%) used was from a 50-mm thick hot rolled plate in T651 state. All the specimens were cut along the rolling direction. The alloy was solution treated at 530 ◦C for 30 min, quenched in water at room temperature and aged immediately. Tensile tests were performed at an initial strain rate of 3.3 × 10−4 s−1. Tension–tension fatigue tests were performed sinusoidally at 60 Hz, using a stress ratio of 0.25, in laboratory air. Tensile and fatigue fractures were examined in a S-570 scanning electron microscope (SEM). The microstructure of the alloy was examined in a CM-12 electron transmission microscope (TEM). According to the results of the tensile tests, two aging conditions have been selected to carry out fatigue tests and microstructural examination. The aging condition, tensile and fatigue properties of the alloys are given in Table I. It can be seen that, with an increase of tensile strength, the fatigue strength increases, and the fatigue strength/tensile strength ratio also increases. The UA alloy shows the higher tensile and fatigue strengths as well as fatigue strength/tensile strength ratios. The microstructures of the alloy have been examined using TEM. The UA alloy contains a fine dispersion of δ′ particles. For the OA alloy, δ′ particle coarsening has taken place coupled with the formation of other precipitates of S and T1 phases, which are heterogeneously distributed and preferentially precipitated on the subgrain boundaries and dislocations. Grain boundary precipitates and precipitate free zone (PFZ) adjacent to the grain boundaries can be also seen for the OA alloy. In the UA and OA conditions, Al3Zr dispersoids exist and not be affected by the aging. The size of the δ′ particle has been measured. The diameters of the δ′ particle are 10 nm in the UA condition and 42 nm in the OA condition. Thin foils were taken from the deformed (about 6%) tensile specimens. The UA alloy shows heterogeneous deformation with planar slip bans formed mainly by the activation of one slip system (Fig. 1a). The OA alloy shows homogeneous deformation with tangled dislocations, no pronounced slip bands could be seen (Fig. 1b). The UA alloy showed dimpled tensile fracture. The OA alloy exhibited mixed rupture with dimples and a small amount of intergranular fracture. Fatigue fractures are different from the tensile fractures. Almost all of the fatigue fracture in the UA alloy was faceted. The surfaces of the facets were parallel to the maximum shear stress direction (Fig. 2a). In the OA alloy, fatigue fracture was transgranular, perpendicular to the tensile axis, with clear and regular striations on the surface (Fig. 2b). From the TEM results, it can be seen that the deformation mode of the alloy is controlled by the interaction of dislocations and precipitates. In the UA condition, the dislocations cut precipitates, the precipitates shearing promoted heterogeneous deformation and produced planar slip bands. For the OA alloy, the precipitates could not be sheared by dislocations, and deformation was homogeneous. The dislocations were bowed out around the precipitates and no slip bands were formed. The Al3Zr dispersoids could not control the deformation mode in this alloy. For the other age-hardend Al alloy, the deformation mode is usually controlled by dispersoids [7, 8]. The UA alloy showed dimpled tensile fracture. The OA alloy exhibited mixed rupture with dimples and intergranular fracture. The difference in fracture mode could be accounted for the grain boundary structure.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Aluminum Alloy Microstructure Properties · Fatigue and fracture mechanics · Metal Forming Simulation Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (12)
Show source-provided references
1. E. HORNBOGEN and K. H. ZUM GAHR, Acta Metall. 24 (1976) 581.10.1016/0001-6160(76)90104-8 ↗
2. J. LINDINGKEIT, A. GYSLER and G. LUTJERING, Metall. Trans. A 12 (1981) 1613.10.1007/BF02643567 ↗
3. A. K. BUSBY, L. EDWARDS and J. W. MARTIN, Mater. Sci. Technol. 2(4) (1986) 363.10.1179/mst.1986.2.4.363 ↗
4. P. DONNADIEU, G. F. DIRRAS and J. DOUIN, in Proceedings of the 8th International Conference ICAA8, edited by P. J Gregson and S. J. Harris (Cambridge, UK, 2002) p. 1019.10.4028/www.scientific.net/MSF.396-402.1019 ↗
5. F. DELMAS, M. J. CASANOVE, A. COURET and A. COUJOU, in Proceedings of the 8th International Conference ICAA8, edited by P. J Gregson and S. J. Harris (Cambridge, UK, 2002) p. 1109.10.4028/www.scientific.net/MSF.396-402.1109 ↗
6. C. P. BLACKENSHIP and E. A. STARKE JR., Acta Metall. Mater. 42(3) (1994) 845.10.1016/0956-7151(94)90279-8 ↗
7. D. M. JIANG and C. WANG, Mater. Sci. Eng. A 352 (2003) 29.10.1016/S0921-5093(02)00456-2 ↗
8. D. M. JIANG, B. D. HONG, T. C. LEI, D. A. DOWNHAM and G. W. LORIMER, Mater. Sci. Technol. 7(11) (1991) 1010.10.1179/mst.1991.7.11.1010 ↗
9. R. M. N. PELLOUX, “Fracture” (Chapman & Hall, London, 1969) p. 731.
10. C. Q. BOWLES and D. BROEK, Int. J. Fracture Mech. 8 (1972) 15.10.1007/BF00185199 ↗
11. D. M. JIANG, S. B. KANG and H. W. KIM, Mater. Sci. Technol. 15 (1999) 1401.10.1179/026708399101505536 ↗
12. Y. XU, P.J. GREGSON and I. SINCLAIR, in Proceedings of the 7th International Conference ICAA7, edited by E. A. Starke, Jr., T. H. Sanders, Jr. and W. A. Cassada (Charlottesville, Virginia, 2000) p. 1525.