Abstract
Typical epoxy molding compounds (EMC) contain chlorine ions that cause silver wire-bond failures under highly accelerated temperature/humidity stress test (HAST). To understand the corrosion mechanisms, experiments were designed to emulate the HAST environment and conditions and performed. Specifically, Ag–Al joints, Ag, Al, Ag3Al, and Ag2Al samples were encapsulated in chlorine-containing EMC, respectively, and went through HAST. EMC with high chlorine content (1000 ppm) was chosen to accelerate the corrosion rate and shorten experiment time. The experimental results show that chlorine-induced corrosion occurs only on Ag3Al and Ag2Al compounds. It does not occur on Ag or Al samples. The corrosion rates of bulk Ag3Al and Ag2Al disks were measured under HAST up to 125 h. The corrosion rate of Ag3Al is twice of that of Ag2Al, meaning that Ag2Al is more resistant to corrosion. Careful evaluations reveal that the corrosion is caused by both moisture and Cl− ions. Microstructures, compositions, and phases of corroded regions were examined in details. In the corroded regions, Ag3Al and Ag2Al compounds disintegrate into aluminum oxide pieces and dispersed Ag precipitates with voids and cracks. The chlorines detected near voids and cracks suggest formation of aluminum chloride as an intermediate product that is hydrolyzed into aluminum oxide. A corrosion chemical model is proposed to establish the reactions of Ag3Al and Ag2Al compounds with chlorine-containing EMC. New information obtained in this research can help the search of new processes and techniques to counter or reduce the chlorine-induced corrosion of devices and packages. The corrosion test method presented may possibly become an acceptable test standard to consider.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Corrosion Behavior and Inhibition · Electronic Packaging and Soldering Technologies · Recycling and Waste Management Techniques
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (28)
Show source-provided references
1. C. Harper, Electronic Packaging and Interconnection Handbook, (McGraw-Hill, New York, 2004)
2. E.R.R. Tummala, E.J. Rymaszewski, Microelectronics Packaging Handbook, (Springer, New York, 1997)
3. G.G. Harman, Wire Bonding in Microelectronics, (McGraw-Hill, New York, 2010)
4. J. Cho, H. Jeong, J. Moon, S. Yoo, J. Seo, S. Lee, S. Ha, E. Her, S. Kang and K. Oh, Thermal reliability & IMC behavior of low cost alternative Au–Ag–Pd wire bonds to Al metallization, in 2009 IEEE 59th Electronic Components and Technology Conference (ECTC) (2009), pp. 1569–1573
5. C.L. Gan, U. Hashim, Evolutions of bonding wires used in semiconductor electronics: perspective over 25 years. J. Mater. Sci. 26(7), 4412–4424 (2015)
6. Z. Zhong, Overview of wire bonding using copper wire or insulated wire. Microelectron. Reliab. 51(1), 4–12 (2011)10.1016/j.microrel.2010.06.003 ↗
7. B.K. Appelt, A. Tseng, C. Chen, Y. Lai, Fine pitch copper wire bonding in high volume production. Microelectron. Reliab. 51(1), 13–20 (2011)10.1016/j.microrel.2010.06.006 ↗
8. C. Yu, C. Chan, L. Chan, K. Hsieh, Cu wire bond microstructure analysis and failure mechanism. Microelectron. Reliab. 51(1), 119–124 (2011)10.1016/j.microrel.2010.04.022 ↗
9. R. Guo, T. Hang, D. Mao, M. Li, K. Qian, Z. Lv, H. Chiu, Behavior of intermetallics formation and evolution in Ag–8Au–3Pd alloy wire bonds. J. Alloys Compd. 588, 622–627 (2014)10.1016/j.jallcom.2013.11.140 ↗
10. T. Chuang, C. Tsai, H. Wang, C. Chang, C. Chuang, J. Lee, H. Tsai, Effects of annealing twins on the grain growth and mechanical properties of Ag–8Au–3Pd bonding wires, J. Electron. Mater. 41(11), 3215–3222 (2012)10.1007/s11664-012-2225-0 ↗
11. C. Cheng, H. Hsiao, S. Chu, Y. Shieh, C. Sun, C. Peng, Low cost silver alloy wire bonding with excellent reliability performance. in 2013 IEEE 63rd Electronic Components and Technology Conference (ECTC) (2013), pp. 1569–1573
12. H. Kim, J.Y. Lee, K. Paik, K. Koh, J. Won, S. Choe, J. Lee, J. Moon, Y. Park, Effects of Cu/Al intermetallic compound (IMC) on copper wire and aluminum pad bondability. IEEE Trans. Compon. Packag. Technol. 26(2), 367–374 (2003)10.1109/TCAPT.2003.815121 ↗
13. Y. C. Jang, S. Y. Park, H. D. Kim, Y. C. Ko, K. W. Koo, M. R. Choi, H. G. Kim, N. K. Cho, I.T. Kang, J.H. Yee, Study of intermetallic compound growth and failure mechanisms in long term reliability of silver bonding wire, in 2014 IEEE 16th Electronics Packaging Technology Conference (EPTC) (2014), pp. 704–708
14. J. Tsai, A. Lan, D. Jiang, L. W. Wu, J. Huang, J. Hong, Ag alloy wire characteristic and benefits, in 2014 IEEE 64th Electronic Components and Technology Conference (ECTC) (2014), pp. 1533–1538
15. L.J. Kai, L.Y. Hung, L.W. Wu, M.Y. Chiang, D.S. Jiang, C. Huang, Y. P. Wang, Silver alloy wire bonding, in 2012 IEEE 62nd Electronic Components and Technology Conference (ECTC) (2012), pp. 1163–1168
16. J. Xi, N. Mendoza, K. Chen, T. Yang, E. Reyes, S. Bezuk, J. Lin, S. Ke, E. Chen, Evaluation of Ag wire reliability on fine pitch wire bonding, in 2015 IEEE 65th Electronic Components and Technology Conference (ECTC) (2015), pp. 1392–1395
17. A. McAlister, The Ag–Al (silver–aluminum) system. Bull. Alloy Phase Diagr. 8(6), 526–533 (1987)10.1007/BF02879428 ↗
18. S. Lim, P. Rossiter, J. Tibballs, Assessment of the Al–Ag binary phase diagram. Calphad 19(2), 131–141 (1995)10.1016/0364-5916(95)00014-6 ↗
19. Y. Chiu, T. Chiang, P. Yang, L. Huang, C. Hung, S. Uegaki, K. Lin, The corrosion behavior of Ag alloy wire bond on Al pad in molding compounds of various chlorine contents under biased-HAST, in Electronics Packaging (ICEP), 2016 international conference (2016), pp. 497–501
20. M. Lue, C. Huang, S. Huang, K. Hsieh, Bromine-and chlorine-induced degradation of gold-aluminum bonds, J. Electron. Mater. 33(10), 1111–1117 (2004)10.1007/s11664-004-0112-z ↗
21. C.L. Gan, C. Francis, B.L. Chan, U. Hashim, Extended reliability of gold and copper ball bonds in microelectronic packaging. Gold Bull. 46(2), 103–115 (2013)10.1007/s13404-013-0087-8 ↗
22. P. Su, H. Seki, C. Ping, S. Zenbutsu, S. Itoh, L. Huang, N. Liao, B. Liu, C. Chen, W. Tai, An evaluation of effects of molding compound properties on reliability of Cu wire components, in 2011 IEEE 61st Electronic Components and Technology Conference (ECTC) (2011), pp. 363–369
23. T. Uno, Bond reliability under humid environment for coated copper wire and bare copper wire. Microelectron. Reliab. 51(1), 148–156 (2011)10.1016/j.microrel.2010.03.006 ↗
24. C. May, Epoxy Resins: Chemistry and Technology (CRC Press, Boca Raton, 1987)
25. H. B. Fan, E. K. Chan, C. K. Wong, M. M. Yuen, Investigation of moisture diffusion in electronic packages by molecular dynamics simulation. J. Adhes. Sci. Technol. 20(16), 1937–1947 (2006)10.1163/156856106779116588 ↗
26. S.K. Prasad, Advanced Wire Bond Interconnection Technology, (Springer, New York, 2004)
27. B.D. Craig, Fundamental Aspects of Corrosion Films in Corrosion Science, (Springer, New York, 2013)
28. H.K. Farag, F. Endres, Studies on the synthesis of nano-alumina in air and water stable ionic liquids. J. Mater. Chem. 18(4), 442–449 (2008)10.1039/B711704C ↗