Fabrication and characterization of CuInS2 films by chemical bath deposition in acid conditions
Source abstract
Abstract
Non-crystalline copper indium disulphide (CuInS2) thin films had been deposited on ITO glass by chemical bath deposition (CBD) in acid conditions. Then polycrystalline CuInS2 films were obtained after sulfuration in sulfur atmosphere at 450 °C for 1.5 h. The films had been characterized by X-ray diffraction (XRD), scanning electronic microscopy (SEM), Raman scattering measurements and energy dispersive X-ray analysis (EDX). The optical and electrical property of the thin films was also measured. The results showed that the pure, flatness, and well crystallized CuInS2 thin films with good electrical and optical property had been obtained, meaning that the chemical bath deposition in acid conditions is suitable for the deposition of CuInS2 thin films.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Chalcogenide Semiconductor Thin Films · Quantum Dots Synthesis And Properties · Copper-based nanomaterials and applications
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (16)
Show source-provided references
1. A. Joswig, M. Gossla, H. Metzner, U. Reislöhner, T. Hahn, W. Witthuhn, Thin Solid Films 515(15), 5921–5924 (2007). doi: 10.1016/j.tsf.2006.12.05310.1016/j.tsf.2006.12.053 ↗
2. T.T. John, M. Mathew, C.S. Kartha, K.P. Vijayakumar, T. Abe, Y. Kashiwaba, Sol. Energy Mater. Sol. Cells 89(1), 27–36 (2005). doi: 10.1016/j.solmat.2004.12.00510.1016/j.solmat.2004.12.005 ↗
3. A.M. Abo, E.I. soud, H.A. Zayed, L.I. Soliman, Thin Solid Films 229(2), 232–236 (1993). doi: 10.1016/0040-6090(93)90370-510.1016/0040-6090(93)90370-5 ↗
4. M. Zribi, M. Kanzari, B. Rezig, Mater. Sci. Eng. B 149(1), 1–6 (2008). doi: 10.1016/j.mseb.2007.10.00810.1016/j.mseb.2007.10.008 ↗
5. Y.B. He, A. Krost, J. Bläsing, W. Kriegseis, A. Polity, B.K. Meyer et al., Thin Solid Films 451–452, 229–232 (2004). doi: 10.1016/j.tsf.2003.10.100
6. Y. Shi, Z. Jin, C. Li, H. An, J. Qiu, Appl. Surf. Sci. 252(10), 3737–3743 (2006). doi: 10.1016/j.apsusc.2005.05.05510.1016/j.apsusc.2005.05.055 ↗
7. A.M. Martinez, A.M. Fernández, L.G. Arriaga, U. Cano, Mater. Chem. Phys. 95(2–3), 270–274 (2006). doi: 10.1016/j.matchemphys.2005.06.01810.1016/j.matchemphys.2005.06.018 ↗
8. S. Bini, K. Bindu, M. Lakshmi, C.S. Kartha, K.P. Vijayakumar, Y. Kashiwaba et al., Renew. Energy 20(4), 405–413 (2000). doi: 10.1016/S0960-1481(99)00122-610.1016/S0960-1481(99)00122-6 ↗
9. T.T. John, T. Sebastian, C.S. Kartha, K.P. Vijayakumar, T. Abe, Y. Kashiwaba, Physica B 388(1–2), 1–9 (2007). doi: 10.1016/j.physb.2006.04.03510.1016/j.physb.2006.04.035 ↗
10. B. Yahmadi, N. Kamoun, R. Bennaceur, M. Mnari, M. Dachraoui, K. Abdelkrim, Thin Solid Films 473(2), 201–207 (2005). doi: 10.1016/j.tsf.2004.04.00210.1016/j.tsf.2004.04.002 ↗
11. N.A. Zeenath, P.K.V. Pillai, K. Bindu, M. Lakshmy, K.P. Vijayakumar, J. Mater. Sci. 35, 2619–2624 (2000). doi: 10.1023/A:100478351759510.1023/A:1004783517595 ↗
12. X.-P. Liu, L.-X. Shao, Surf. Coat. Technol. 201, 5340–5343 (2007). doi: 10.1016/j.surfcoat.2006.07.18210.1016/j.surfcoat.2006.07.182 ↗
13. I. Oja, M. Nanu, A. Katerski, M. Krunks et al., Thin Solid Films 480–481, 82–86 (2005). doi: 10.1016/j.tsf.2004.11.01310.1016/j.tsf.2004.11.013 ↗
14. J. Alvarez-García, A. Pérez-Rodríguez, A. Romano-Rodríguez, T. Jawhari, J.R. Morante, R. Scheer et al., Thin Solid Films 387, 216–218 (2001). doi: 10.1016/S0040-6090(00)01714-410.1016/S0040-6090(00)01714-4 ↗
15. Y.B. He, A. Polity, H.R. Alves, I. Österreicher, W. Kriegseis, D. Pfisterer et al., Thin Solid Films 403–404, 62 (2002). doi: 10.1016/S0040-6090(01)01533-4
16. Y.X. Chen, X. He, X.J. Zhao, M.X. Song, X.Y. Gu, Mater. Sci. Eng. B 139, 88–94 (2007). doi: 10.1016/j.mseb.2007.01.03610.1016/j.mseb.2007.01.036 ↗