Effect of La2O3 additive on the dielectric properties of barium strontium titanate glass–ceramics
Source abstract
Abstract
The barium strontium titanate (BaxSr1–xTiO3) glass–ceramics doped with different content of La were prepared via controlled crystallization. Phase compositions, microstructure and dielectric behaviors were investigated systematically. The results revealed that La2O3 additives had little influence on the dielectric constant but significantly changed the microstructure of the glass–ceramics, which led to improved breakdown strength (BDS). The optimized energy-storage density of 3.18 J/cm3 was achieved in the glass–ceramics with 1.0 wt% La2O3 content which is 2.56 times higher than pure BST glass–ceramics, suggesting glass–ceramics of this composition could be an attractive candidate for energy-storage applications.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Ferroelectric and Piezoelectric Materials · Microwave Dielectric Ceramics Synthesis · Advanced ceramic materials synthesis
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (21)
Show source-provided references
1. D. Yi, J.C. Yuan, H.Y. Liu, Y. Shen, Y.H. Lin, C.W. Nan, X. Xi, J.L. He, J. Electroceram. 29, 95–98 (2012)10.1007/s10832-012-9752-1 ↗
2. K. Zhou, S.A. Boggs, R. Ramprasad, M. Aindow, C. Erkey, S.P. Alpay, Appl. Phys. Lett. 93, 102908 (2008)10.1063/1.2982086 ↗
3. J. Wang, L.J. Tang, B. Shen, J.W. Zhai, Ceram. Int. 40, 2261–2266 (2014)10.1016/j.ceramint.2013.07.145 ↗
4. J. Chen, Y. Zhang, C.S. Deng, X.M. Dai, L.T. Li, J. Am. Ceram. Soc. 92, 1350–1353 (2009)10.1111/j.1551-2916.2009.03028.x ↗
5. Y. Zhang, J. Huang, T. Ma, X. Wang, C. Deng, X. Dai, J. Am. Ceram. Soc. 94, 1805–1810 (2011)10.1111/j.1551-2916.2010.04301.x ↗
6. E.P. Gorzkowski, M.J. Pan, B. Bender, C.C.M. Wu, J. Electroceram. 18, 269–276 (2007)10.1007/s10832-007-9127-1 ↗
7. Y.K. Zeng, X.Y. Qin, S.L. Jiang, G.Z. Zhang, L. Zhang, J. Am. Ceram. Soc. 94, 469–473 (2011)10.1111/j.1551-2916.2010.04223.x ↗
8. X.R. Wang, Y. Zhang, T. Ma, Z.B. Yuan, Q. Zhang, C.S. Deng, T.X. Liang, Int. J. Appl. Ceram. Technol. 10, 301–306 (2013)10.1111/j.1744-7402.2011.02733.x ↗
9. J. Chen, Y. Zhang, C.S. Deng, X.M. Dai, J. Am. Ceram. Soc. 92, 1863–1866 (2009)10.1111/j.1551-2916.2009.03100.x ↗
10. J. Takahashi, H. Nakano, K. Kageyama, J. Eur. Ceram. Soc. 26, 2123–2127 (2006)10.1016/j.jeurceramsoc.2005.09.070 ↗
11. E.P. Gorzkowski, M.J. Pan, B. Bender, C.C.M. Wu, J. Am. Ceram. Soc. 91, 1065–1069 (2008)10.1111/j.1551-2916.2007.02254.x ↗
12. M. Capron, A. Douy, J. Am. Ceram. Soc. 85, 3036–3040 (2002)10.1111/j.1151-2916.2002.tb00575.x ↗
13. C.R. Gautam, D. Kumar, P. Singh, O. Parkash, ISRN Spectrosc 2012, 410583 (2012)10.5402/2012/410583 ↗
14. W. Ruland, Acta Crystallogr 14, 1180–1185 (1961)10.1107/S0365110X61003429 ↗
15. S. Kemethmüller, A. Roosen, F. Neunhoeffer, J. Neubauer, J. Am. Ceram. Soc. 89, 2632–2637 (2006)10.1111/j.1551-2916.2006.01113.x ↗
16. Z. Zhao, V. Buscaglia, M. Viviani, M.T. Buscaglia, L. Mitoseriu, A. Testino, P. Nanni, Phys. Rev. B: Condens. Matter 70, 024107 (2004)10.1103/PhysRevB.70.024107 ↗
17. K. Uchino, E. Sadanaga, T. Hirose, J. Am. Ceram. Soc. 72, 1555–1558 (1989)10.1111/j.1151-2916.1989.tb07706.x ↗
18. P. Lu, Y. Zheng, J.S. Cheng, D.Y. Guo, Ceram. Int. 39, 8207–8212 (2013)10.1016/j.ceramint.2013.04.004 ↗
19. A.K. Yadav, C. Gautam, P. Singh, New J Glass Ceram 02, 126–131 (2012)10.4236/njgc.2012.23018 ↗
20. J.J. Huang, Y. Zhang, T. Ma, H.T. Li, L.W. Zhang, Appl. Phys. Lett. 96, 042902 (2010)10.1063/1.3293456 ↗
21. X.R. Wang, Y. Zhang, X.Z. Song, Z.B. Yuan, T. Ma, Q. Zhang, C.S. Deng, T.X. Liang, J. Eur. Ceram. Soc. 32, 559–567 (2012)10.1016/j.jeurceramsoc.2011.09.024 ↗