In this study, a micro-porous titania (TiO2) layer was synthesized on commercial pure Ti using the microplasma oxidation (MPO) method. Ti/Ti, MPO-TiO2 (MPO-Ti)/Ti and MPO-Ti/MPO-Ti were successfully active soldered using this Sn3.5Ag4Ti(Ce) active filler metal at 250 °C for 60 s. The microstructure and mechanical properties of the active soldered joints were investigated. Results indicate that trace Ce reacts with the MPO-Ti layer to form both CeO2 and Ti, corresponding to the reaction between Ti and Sn to form Ti6Sn5, and nano-sizes Ag3Sn phases adsorb at the active filler/MPO-Ti interfaces. Shear strength of soldered Ti/Ti, MPO-Ti/Ti, and MPO-Ti/MPO-Ti specimens were measured to be 16.3 ± 1.39, 11.3 ± 1.56, and 9.5 ± 1.24 MPa, respectively. The fracture of Ti/Ti specimen was found to produce along the Ti2Sn3 and solder matrix. In the MPO-Ti/MPO-Ti specimen, the fractures occurred through the active filler/MPO-Ti interface. In the MPO-Ti/Ti specimen, the fracture failure mode transferred from MPO layer/Ti interfacial fracture to fracture within the active filler.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Electronic Packaging and Soldering Technologies · Intermetallics and Advanced Alloy Properties · Advanced ceramic materials synthesis

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (35)

Show source-provided references
1. J.G. Li, Energetics of metal/ceramic interfaces, metal-semiconductor Schottky contacts, and their relationship. Mater. Chem. Phys. 47, 126–145 (1997)10.1016/S0254-0584(97)80041-7 ↗
2. S. Jin, Rare-earth-enabled universal solders for microelectromechanical systems and optical packaging. J. Electron. Mater. 32, 1366–1370 (2003)10.1007/s11664-003-0102-6 ↗
3. L.C. Tsao, S.Y. Chang, M.S. Huang, C.S. Chen, Direct robust active bonding between Al heat sink and Si substrate, 2012 International Conference on Electronic Packaging Technology and High Density Packaging (ICEPT-HDP) (2012) 1635–163810.1109/ICEPT-HDP.2012.6474921 ↗
4. C.L. Chuang, L.C. Tsao, H.K. Lin, L.P. Feng, Effects of small amount of active Ti element additions on microstructure and property of Sn3.5Ag0.5Cu solder. Mater. Sci. Eng., A 558, 478–484 (2012)10.1016/j.msea.2012.08.031 ↗
5. H. Mavoori, A.G. Ramirez, S. Jin, Lead-free universal solders for optical and electronic devices. J. Electron. Mater. 31, 1160–1165 (2002)10.1007/s11664-002-0005-y ↗
6. J. Lin, N. Ma, Y. Lei, Investigation of interface layer failure and shear strength of CMT brazed lap joints in dissimilar materials. Transactions of JWRI 40, 101–107 (2011)
7. S.Y. Chang, L.C. Tsao, M.J. Chiang, C.N. Tung, G.H. Pan, T.H. Chuang, Active soldering of indium tin oxide (ITO) with Cu in air using an Sn3.5Ag4Ti(Ce, Ga) filler. JMEPEG 12, 383–389 (2003)10.1361/105994903770342890 ↗
8. S.Y. Chang, T.H. Chuang, L.C. Tsao, C.L. Yang, Z.S. Yang, Active soldering of ZnS–SiO2 sputtering targets to copper backing plates using an Sn3.5Ag4Ti(Ce, Ga) filler metal. J. Mater. Process. Tech. 202, 22–26 (2008)10.1016/j.jmatprotec.2007.08.045 ↗
9. S.Y. Chang, T.H. Chuang, C.L. Yang, Low temperature bonding of alumina/alumina and alumina/copper in air using an Sn3.5Ag4Ti(Ce, Ga) filler. J. Electron. Mater. 36, 1193–1198 (2007)10.1007/s11664-007-0190-9 ↗
10. R. Kolenˇak, P. Šebo, M. Provaznik, M. Kolenˇakova, K. Ulrich, Shear strength and wettability of active Sn3.5Ag4Ti(Ce, Ga) solder on Al2O3 ceramics. Mater. Des. 32, 3997–4003 (2011)10.1016/j.matdes.2011.03.022 ↗
11. J.C. Yan, Z.W. Xu, L. Shi, X. Ma, S.Q. Yang, Ultrasonic assisted fabrication of particle reinforced bonds joining aluminum metal matrix composites. Mater. Des. 32, 343–347 (2011)10.1016/j.matdes.2010.06.036 ↗
12. T.H. Chuang, M.S. Yeh, Y.H. Chai, Metall. Brazing of Zirconia with AgCuTi and SnAgTi Active Filler Metals. Mater. Trans. A 31, 1591–1597 (2000)10.1007/s11661-000-0169-0 ↗
13. K. Bobzin, E. Lugscheider, H. Zhuang, F. Ernst, N. Bagcivan, M. Maes, J. Rösing, S. Ferrara, A. Erdle, A. Krämer, New soldering processes and solder systems for hybrid microsystems: developments and applications. Microsystem Tech. 12, 620–625 (2006)10.1007/s00542-006-0079-1 ↗
14. S.Y. Chang, M. H. Lu, L.C. Tsao, T.H. Chuang, Active soldering of ITO to copper, welding J. (2006) 81s–83s
15. X.W. Bao, S.S. Yan, F. Chen, J.L. Zhang, Preparation of TiO2 photocatalyst by hydrothermal method from aqueous Peroxotitanium Acid. Mater. Lett. 59, 412–415 (2005)10.1016/j.matlet.2004.09.035 ↗
16. D. Cahen, G. Hodes, M. Gratzel, J.F. Guillemoles, I. Riess, Nature of photovoltaic action in dye-sensitized solar cells. J. Phys. Chem. B 104, 2053–2059 (2000)10.1021/jp993187t ↗
17. A.M. Ruiz, A. Cornet, K. Shimanoe, J.R. Morante, N. Yamazoe, Effects of various metal additives on the gas sensing performances of TiO2 nanocrystals obtained from hydrothermal treatments. Sens. Actuators, B 108, 34–40 (2005)10.1016/j.snb.2004.09.045 ↗
18. S.Y. Chang, H.K. Lin, L.C. Tsao, W.T. Huang, Y.T. Huang, Effect of voltage on the microstructure and corrosion resistance of micro arc oxidation coatings on CP-Ti Corrosion. Eng. Sci. Tech. (2013). doi: 10.1179/1743278213Y.0000000097
19. A. Kikuchi, H. Taniguchi, Y. Yoshida, M. Tomonaga, T. Takeuchi, New Ti–Sn intermetallic compound and (Nb, Ti)3Sn conductor. IEEE Trans. Appl. Supercond. 19, 2556–2559 (2009)10.1109/TASC.2009.2018031 ↗
20. L.C. Tsao, Direct active soldering of micro-arc oxidized Ti/Ti joints in air using Sn3.5Ag0.5Cu4Ti(RE) filler. Mater. Sci. Eng., A 565, 63–71 (2013)10.1016/j.msea.2012.12.036 ↗
21. L.C. Tsao, Suppressing effect of 0.5 wt% nano-TiO2 addition into Sn-3.5Ag-0.5Cu solder alloy on the intermetallic growth with Cu substrate during isothermal aging. J. Alloys Compd. 509, 8441–8448 (2011)10.1016/j.jallcom.2011.05.116 ↗
22. L.C. Tsao, Evolution of nano-Ag3Sn particle formation on Cu–Sn intermetallic compounds of Sn3.5Ag0.5Cu composite solder/Cu during soldering. J. Alloys Compd. 509, 2326–2333 (2011)10.1016/j.jallcom.2010.11.010 ↗
23. S.Y. Chang, C.C. Jain, T.H. Chuang, L.P. Feng, L.C. Tsao, Effect of addition of TiO2 nanoparticles on the microstructure, microhardness and interfacial reactions of Sn3.5AgXCu solder. Mater. Des. 32, 4720–4727 (2011)10.1016/j.matdes.2011.06.044 ↗
24. T.H. Chuang, L.C. Tsao, C.H. Chung, S.Y. Chang, Evolution of Ag3Sn compounds and microhardness of Sn3.5Ag0.5Cu nano-composite solders during different cooling rate and aging. Mater. Des. 39, 475–483 (2012)10.1016/j.matdes.2012.03.021 ↗
25. B. Thomas, Reed free energy of formation of binary compounds (MIT Press, Cambridge, 1971)
26. Stanley M. Howard, Ellingham Diagrams, http://showard.sdsmt.edu/MET320/Handouts/EllinghamDiagrams/Ellingham_v22_Macro.pdf
27. W.L. Wang, Y.C. Tsai, Microstructural characterization and mechanical property of active soldering anodized 6061 Al alloy using Sn–3.5Ag–xTi active solders. Mater. Character. 68, 42–48 (2012)10.1016/j.matchar.2012.03.007 ↗
28. R.J. Cui, X.X. Tang, M. Gao, H. Zhang, S.K. Gong, Thermodynamic analysis of interactions between Ti−Al alloys and oxide ceramics. Trans. Nonferrous Met. Soc. China 22, 887–894 (2012)10.1016/S1003-6326(11)61261-2 ↗
29. J.S. Pimenta, A.J.A. Buschinelli, R.M. Do Nascimento, A.E. Martinelli, J. Remmel, Joining of zirconia mechanically metallized with titanium. Cerâmica 56, 212–221 (2010)10.1590/S0366-69132010000300002 ↗
30. W.B. Hanson, K.I. Ironside, J.A. Fernie, Active metal brazing of zirconia. Acta Mater. 48, 4673–4676 (2000)10.1016/S1359-6454(00)00256-1 ↗
31. S. Itoh, Y. Inoue, Activity measurement of titanium–tin alloys by knudsen effusion method. Mater. Trans. 52, 704–708 (2011)10.2320/matertrans.M-M2011801 ↗
32. L. Gremillard, E. Saiz, V.R. Radmilovic, A.P. Tomsia, Role of titanium on the reactive spreading of lead-free solders on alumina. J. Mater. Res. 21, 3222–3233 (2006)10.1557/jmr.2006.0393 ↗
33. S.M.L. Nai, J. Wei, M. Gupta, Improving the performance of lead-free solder reinforced with multi-walled carbon nanotubes. Mater. Sci. Eng., A 423, 166–169 (2006)10.1016/j.msea.2005.10.072 ↗
34. L.C. Tsao, S.Y. Chang, C.I. Lee, W.H. Sun, C.H. Huang, Effects of nano-Al2O3 additions on microstructure development and hardness of Sn3.5Ag0.5Cu solder. Mater. Des. 31, 4831–4835 (2010)10.1016/j.matdes.2010.04.033 ↗
35. R.K. Rakesh, W.E. Thomas, Tin-Based reactive solders for ceramic/metal joints. Metallurgical trans. B 20, 919–924 (1989)10.1007/BF02670197 ↗