Preparation and properties of alkali activated foam cement reinforced with polypropylene fibers
Source abstract
Abstract
A new form of foam cement was produced by mixing alkali-activated slag, clay, a small amount of polypropylene fibers with prepared foam during stirring. The preparation of the material is quite different from the normal one, which is produced just at room temperature and without baking. The fabrication of this energy-saving and low-price material can be favorable for lowering carbon emission by using recycled industrial wastes. Thermal conductivity of 0.116 W/(m·k), compressive strength of 3.30 MPa, flexural strength of 0.8 MPa and density of 453 kg/m3 can be achieved after 28 days aging. The hydration product is C-S-H with less Ca(OH)2, calcium aluminum and zeolite, which was characterized by X-ray diffraction(XRD) measurement. This prospective foam cement may be expected to be an excellent economical energy-saving building material.
Source: openaire · Quality: candidate unverified · Source record ↗
Research context
OpenAlex topics: Innovative concrete reinforcement materials · Geotechnical Engineering and Soil Stabilization · Concrete and Cement Materials Research
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
References (10)
Show source-provided references
1. F K Akthar, J R G Evans. High Porosity(>90%) Cementitious Foams[J]. Cement and Concrete Research, 2010, 40(2): 352–35810.1016/j.cemconres.2009.10.012 ↗
2. Guoqiang Li, Venkata D, Muthyala. A Cement Based Syntactic Foam[J]. Materials Science and Engineering A, 2008, 478(1–2): 77–8610.1016/j.msea.2007.05.084 ↗
3. Rongxi Shen, Qi Cui, Qinghai Li. New Type Fibre Reinforced Cement-Based Composites[M]. Beijing: China Building Material Industry Publishing House, 2004
4. Chaosheng Tang, Bin Shi, Wei Gao, et al. Stength and Mechanical Behavior of Short Polypropylene Fiber Reinforced and Cement Stabilized Clayey Soil[J]. Geotextiles and Geomembrances, 2007, 25: 194–20210.1016/j.geotexmem.2006.11.002 ↗
5. F. Puertas, T Amat, A Fernandez-Jimenez, et al. Mechanical and Durable Behaviour of Alkaline Cement Mortars Reinforced with Polypropylene Fibres[J]. Cement and Concrete Research, 2003, 33(12): 2 031–2 03610.1016/S0008-8846(03)00222-9 ↗
6. Nangru Yang. Basement of Physical and Chemical for the Formation of Alkali-Activated Cementious MaterialI[J]. Journal of Chiness Ceramic Society, 1996, 24(2): 209–215
7. P I A Malek, D M Roy. Alkali Activated Geopolymer[C]. Tenth International Congress on the Chemistry of Cement, 1997
8. A JUST, B Middendorf. Microstructure of High-Strength Foam Concrete[J]. Materials Characterization, 2009, 60(7): 741–74810.1016/j.matchar.2008.12.011 ↗
9. E K Kunhanandan Nambiar, K Ramamurthy. Influence of Filler Type on the Properties of Foam Concrete[J]. Cement and Concrete Composites, 2006, 28(5): 475–48010.1016/j.cemconcomp.2005.12.001 ↗
10. Wang Lijiu. Building Material[M]. Beijing: China Waterpower Press, 2008