journal article·2016-12

Preparation and anti-oxidation mechanism of mullite/yttrium silicate coatings on C/SiC composites

Qingsong Ma, Lihui Cai

Publisher page

Abstract

In order to enhance the oxidation resistance of C/SiC composites, mullite/yttrium silicate coatings were fabricated on C/SiC composites through dip-coating route. Al2O3-SiO2 sol with high solid content was selected as the raw material for mullite and “silicone resin + Y2O3 powder” slurry was used to synthesize yttrium silicate. The microstructure and phase composition of coatings were characterized, and the investigation on oxidation resistance and anti-oxidation mechanism was emphasized. The as-fabricated coatings consisting of SiO2-rich mullite phase and Y2Si2O7 phase show high density and favorable bonding to C/SiC composites. After oxidized at 1 400 °C and 1 500 °C for 30min in static air, the coating-containing C/SiC composites possess 91.9% and 102.4% of the original flexural strength, respectively. The desirable thermal stability of coatings and the further densification of coatings due to viscous flow of rich SiO2 and Y-Si-Al-O glass are responsible for the excellent oxidation resistance. In addition, the coating-containing composites retain 99.0% of the original flexural strength and the coatings exhibit no cracking and desquamation after 12 times of thermal shock from 1 400 °C to room temperature, which are ascribed to the combination of anti-oxidation mechanism and preferable physical and chemical compatibility among C/SiC composites, mullite and Y2Si2O7. The carbothermal reaction at 1 600 °C between free carbon in C/SiC substrate and rich SiO2 in mullite results in severe frothing and desquamation of coatings and obvious degradation in oxidation resistance.
Source: openaire · Quality: candidate unverified · Source record ↗

Research context

OpenAlex topics: Advanced ceramic materials synthesis · Advanced materials and composites · MXene and MAX Phase Materials

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

References (28)

Show source-provided references
1. Naslain R. Design, Preparation and Properties of Non-oxide CMCs for Application in Engines and Nuclear Reactors: An Overview[J]. Compos. Sci. Technol., 2004, 64: 155–17010.1016/S0266-3538(03)00230-6 ↗
2. Ma QS, Liu HT, Pan Y, et al. Research Progress on the Application of C/SiC Composites in Scramjet[J]. J. Inorg. Mater., 2013, 28(3): 248–255 (in Chinese)
3. Zhang BF, Wang S, Li W, et al. Mechanical Behavior of C/SiC Composites under Simulated Space Environments[J]. Mater. Sci. Eng., A, 2012, 534: 408–41210.1016/j.msea.2011.11.087 ↗
4. Chen SA, Hu HF, Zhang YD, et al. Rapid Densification of C/SiC Composites by Joint Processes of CLVD and PIP[J]. Mater. Lett., 2011, 65(19-20): 3137–313910.1016/j.matlet.2011.06.100 ↗
5. Li W, Chen ZH. Pore Geometry of 3D-Cf/SiC Composites by Mercury Intrusion Porosimetry[J]. Ceram. Int., 2009, 35(2): 747–75310.1016/j.ceramint.2008.02.011 ↗
6. Xiang Y, Li W, Wang S, et al. Oxidation Behavior of Oxidation Protective Coatings for PIP-C/SiC Composites at 1500 °C[J]. Ceram. Int., 2012, 38(1): 9–1310.1016/j.ceramint.2011.06.063 ↗
7. Xiang Y, Li W, Wang S, et al. Ablative Property of ZrC-SiC Multilayer Coating for PIP-C/SiC Composites under Oxy-acetylene Torch[J]. Ceram. Int., 2012, 38(4): 2893–289710.1016/j.ceramint.2011.11.063 ↗
8. Huang JF, Li HJ, Zeng XR, et al. Yttrium Silicate Oxidation Protective Coating for SiC Coated Carbon/Carbon Composites[J]. Ceram. Int., 2006, 32: 417–42110.1016/j.ceramint.2005.03.018 ↗
9. Huang JF, Li HJ, Zeng XR, et al. A New SiC/Yttrium Silicate/Glass Multi-layer Oxidation Protective Coating for Carbon/Carbon Composites[J]. Carbon, 2004, 42: 2356–235910.1016/j.carbon.2004.05.005 ↗
10. Huang JF, Zeng XR, Li HJ, et al. SiC/Yttrium Silicate Multi-layer Coating for Oxidation Protection of Carbon/Carbon Composites[J]. J. Mater. Sci., 2004, 39: 7383–738510.1023/B:JMSC.0000048756.96547.bf ↗
11. Argirusis C, Damjanović T, Borchardt G. Yttrium Silicate Coating System for Oxidation Protection of C/C-Si-SiC Composites: Electrophoretic Deposition and Oxygen Self-diffusion Measurements[J]. J. Eur. Ceram. Soc., 2007, 27: 1303–130610.1016/j.jeurceramsoc.2006.05.026 ↗
12. Liu M, Huang JF, Zhang YT, et al. Phase, Microstructure, and Oxidation Resistance of Yttrium Silicates Coatings Prepared by a Hydrothermal Electrophoretic Deposition Process for C/C Composites[J]. J. Coat. Technol. Res., 2009, 6(4): 531–53510.1007/s11998-008-9122-8 ↗
13. Aparicio M, Durán A. Preparation and Characterization of 50SiO2–50Y2O3 Sol-gel Coatings on Glass and SiC(C/SiC) Composites[J]. Ceram. Int., 2005, 31: 631–63410.1016/j.ceramint.2004.08.002 ↗
14. Huang JF, Li HJ, Zeng XR, et al. Oxidation Resistant Yttrium Silicates Coating for Carbon/Carbon Composites Prepared by a Novel In-situ Formation Method[J]. Ceram. Int., 2007, 33: 887–89010.1016/j.ceramint.2006.01.007 ↗
15. Huang JF, Li HJ, Zeng XR, et al. Preparation and Oxidation Kinetics Mechanism of Three-layer Multi-layer-coatings-coated Carbon/Carbon Composites[J]. Surf. Coat. Tech., 2006, 200: 5379–538510.1016/j.surfcoat.2005.06.011 ↗
16. Zheng XH, Du YG, Xiao JY, et al. Celsian/Yttrium Silicate Protective Coating Prepared by Microwave Sintering for C/SiC Composites Against Oxidation[J]. Mater. Sci. Eng. A, 2009, 505 (1-2): 187–19010.1016/j.msea.2008.11.008 ↗
17. Bernardo E, Parcianello G, Colombo P. Novel Synthesis and Applications of Yttrium Silicates from a Silicone Resin Containing Oxide Nano-particle Fillers[J]. Ceram. Int., 2012, 38: 5469–547410.1016/j.ceramint.2012.03.059 ↗
18. Liu J, Zhang LT, Hu F, et al. Polymer-derived Yttrium Silicate Coatings on 2D C/SiC Composites[J]. J. Eur. Ceram. Soc., 2013, 33: 433–43910.1016/j.jeurceramsoc.2012.08.032 ↗
19. Aparicio M, Durán A. Yttrium Silicate Coatings for Oxidation Protection of Carbon-silicon Carbide Composites[J]. J. Am. Ceram. Soc., 2000, 83(6): 1351–135510.1111/j.1151-2916.2000.tb01392.x ↗
20. Fukuda K, Matsubara H. Thermal Expansion of δ-yttrium Dsilicate[J]. J. Am. Ceram. Soc., 2004, 87(1): 89–9210.1111/j.1551-2916.2004.00089.x ↗
21. Torrey JD, Bordia RK. Processing of Polymer-derived Ceramic Composites Coatings on Steel[J]. J. Am. Ceram. Soc., 2008, 91(1): 41–4510.1111/j.1551-2916.2007.02019.x ↗
22. Liu J, Zhang LT, Liu QM, et al. Polymer-derived SiOC-BSAS Coatings as an Environmental Barrier for C/SiC Composites[J]. J. Am. Ceram. Soc., 2010, 93(12): 4148–415210.1111/j.1551-2916.2010.04000.x ↗
23. Ma QS, Ma Y, Chen ZH. Fabrication and Characterization of Nanoporous SiO2 Ceramics via Pyrolysis of Silicone Resin Filled with Nanometer SiO2 Powders[J]. Ceram. Int., 2010, 36(8): 2269–227210.1016/j.ceramint.2010.07.020 ↗
24. Hwang SL, Chen IW. Reaction Hot Pressing of α′-and β′-Sialon Ceramics[J]. J. Am. Ceram. Soc., 1994, 77(1): 165–17110.1111/j.1151-2916.1994.tb06972.x ↗
25. Lee KN, Fox DS, Bansal NP. Rare Earth Silicate Environmental Barrier Coatings for SiC/SiC Composites and Si3N4 Ceramics[J]. J. Eur. Ceram. Soc., 2005, 25: 1705–171510.1016/j.jeurceramsoc.2004.12.013 ↗
26. Ma QS, Cai LH. Fabrication of Y2Si2O7 Coating and Its Oxidation Protection for C/SiC Composites[J]. Transactions of Nonferrous Metals Society of China(submitted)
27. Fan CY, Ma QS. Research Progress in Yttrium Silicate Coatings for Anti-oxidation at High Temperature[J]. Journal of Ceramics, 2014, 35(4): 351–355 (in Chinese)
28. Zeng KH, Ma QS, Cai LH. Fabrication of Mullite Coating and Its Oxidation Protection for Carbon Fiber Reinforced SiC Composites[J]. Key Engineering Materials, 2016, 697: 476–48010.4028/www.scientific.net/KEM.697.476 ↗