Preparation and Performance of LiNi1–xAlxO2 Electrodes for Low-Temperature Ceramic Fuel Cells
Source abstract
Abstract
The electrochemical performances of LiNi 1– x Al x O 2 (LNA) doped with different amounts of Al as electrodes for low-temperature ceramic fuel cells were investigated. It was found that the maximum power density of the cell with LNA-82 as the symmetrical electrode and GDC as the electrolyte was 798 mW·cm –2 at 550 °C in H 2 /air fuel cell conditions, with the ionic conductivity of the electrolyte reaching as high as 0.679 S·cm –1 . The diffusion of the molten salts such as LiOH generated by the reduction of LNA in the cell anode by H 2 into the electrolyte to form a “GDC-Li compound” composite electrolyte with ultrahigh ionic conductivity is the key to its excellent low-temperature power generation performance. It is found that as the Al doping concentration in LNA exceeds a certain critical value, LiAlO 2 begins to form in LNA. As the doping concentration of Al increased, the amount of lithium compound molten salts containing LiOH generated by the reduction of LNA electrodes in H 2 decreased, resulting in a significant decrease in the electrochemical performance of the cell.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advancements in Solid Oxide Fuel Cells · Fuel Cells and Related Materials · Thermal Expansion and Ionic Conductivity
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
School of Metallurgy,Northeastern University, Shenyang 110819, China
Liaoning Key Laboratory for Metallurgical Sensor and Technology, Northeastern University, Shenyang 110819, China
Funding
National Natural Science Foundation of China
References (33)
Show source-provided references
1. 10.1016/j.nanoen.2017.12.04410.1016/j.nanoen.2017.12.044 ↗
2. 10.1016/j.ijhydene.2011.08.05410.1016/j.ijhydene.2011.08.054 ↗
3. 10.1002/aenm.20140189510.1002/aenm.201401895 ↗
4. 10.1016/j.ceramint.2014.02.06410.1016/j.ceramint.2014.02.064 ↗
5. 10.1016/j.jpowsour.2014.07.07610.1016/j.jpowsour.2014.07.076 ↗
6. 10.1016/j.ijhydene.2012.09.16010.1016/j.ijhydene.2012.09.160 ↗
7. 10.1016/j.ijhydene.2013.06.05010.1016/j.ijhydene.2013.06.050 ↗
8. 10.1016/j.mtener.2021.10066110.1016/j.mtener.2021.100661 ↗
9. 10.1021/acsami.8b2045410.1021/acsami.8b20454 ↗
10. 10.1016/j.ijhydene.2017.11.05610.1016/j.ijhydene.2017.11.056 ↗
11. 10.1016/j.ceramint.2020.04.05310.1016/j.ceramint.2020.04.053 ↗
12. 10.1016/j.mtener.2023.10136510.1016/j.mtener.2023.101365 ↗
13. 10.1016/j.ijhydene.2020.04.19210.1016/j.ijhydene.2020.04.192 ↗
14. 10.1016/j.ijhydene.2019.07.22310.1016/j.ijhydene.2019.07.223 ↗
15. 10.1016/j.mtener.2023.10129210.1016/j.mtener.2023.101292 ↗
16. 10.1016/j.ijhydene.2022.08.22210.1016/j.ijhydene.2022.08.222 ↗
17. 10.1016/j.jpowsour.2021.23007010.1016/j.jpowsour.2021.230070 ↗
18. 10.1016/j.ijhydene.2018.04.00610.1016/j.ijhydene.2018.04.006 ↗
19. 10.20517/energymater.2021.0610.20517/energymater.2021.06 ↗
20. 10.1021/acsaem.0c0036410.1021/acsaem.0c00364 ↗
21. 10.1149/1945-7111/ac908a10.1149/1945-7111/ac908a ↗
22. 10.1016/j.ijhydene.2021.06.01710.1016/j.ijhydene.2021.06.017 ↗
23. 10.1021/acsaem.1c0161310.1021/acsaem.1c01613 ↗
24. 10.1016/j.ijhydene.2020.06.18910.1016/j.ijhydene.2020.06.189 ↗
25. 10.1016/j.mineng.2020.10645010.1016/j.mineng.2020.106450 ↗
26. 10.1016/j.etran.2023.10027610.1016/j.etran.2023.100276 ↗
27. 10.1016/j.jpowsour.2014.04.10910.1016/j.jpowsour.2014.04.109 ↗
28. 10.1016/j.electacta.2018.01.14410.1016/j.electacta.2018.01.144 ↗
29. 10.1016/j.electacta.2007.05.07110.1016/j.electacta.2007.05.071 ↗
30. 10.1016/j.jpowsour.2014.01.11010.1016/j.jpowsour.2014.01.110 ↗
31. 10.1021/acsami.8b1008710.1021/acsami.8b10087 ↗
32. 10.1038/3510462010.1038/35104620 ↗
33. 10.1007/s10008-012-1771-y10.1007/s10008-012-1771-y ↗