journal article·2026-01-12Open access

Online Mass Spectrometry Investigation of SEI Formation on Carbon Electrode Surfaces in Sodium-Ion Batteries: Oxygen and Additive Effects

Puhan Zhang, Seiya Nakahata, Baoxu Peng, Bingbing Li, Dongyu Zhang, Ken-ichi Inoue, Limin Wang, Itaru Honma, Shen Ye

ACS Applied Energy Materials· Volume 9· Issue 1

Abstract

High Resolution Image Download MS PowerPoint Slide Lithium-ion batteries (LIBs) are widely used due to their high cyclability and stability. However, the high cost of raw materials has spurred interest in sodium-ion batteries (SIBs) as a cost-effective alternative. Despite this, SIBs suffer from lower energy density and poorer cyclability, leaving them in a developmental stage. The formation of the solid electrolyte interphase (SEI) is critical for battery performance as it stabilizes the electrode and prevents further solvent degradation during cycling. This study investigated the SEI formation mechanism in sodium-based EC/DEC electrolyte by monitoring the evolution of volatile products and comparing them with those in lithium-based electrolytes under Ar and O 2 atmospheres using online electrochemical mass spectrometry and vibrational spectroscopy. It was demonstrated that the SEI forms via similar reaction pathways in both sodium- and lithium-based electrolytes. However, Na + lead to more significant ethylene (C 2 H 4 ) evolution during this process. Upon introducing O 2 into the operating environment, carbon dioxide (CO 2 ) and water were produced during the initial cycle. At the same time, the amount of C 2 H 4 evolved was significantly lower than under Ar. The results indicate that in the presence of O 2, the superoxide (O 2 – ) generated during the oxygen reduction reaction (ORR) alters the decomposition of EC molecules into two pathways. Because O 2 – is more stable in sodium-based electrolytes, a larger fraction of O 2 – participates in the decomposition of EC. This alters the electrochemical reduction reaction (ERR) pathway of C 2 H 4 generated from EC decomposition to an ORR pathway that yields CO 2 . We also found that specific additives, such as vinylene carbonate (VC) and fluoroethylene carbonate (FEC), can improve SEI stability in SIBs by inhibiting solvent decomposition and promoting the formation of a denser, stronger SEI. These findings provide valuable insights into the development of stable SEI, particularly for advancing the performance of SIBs.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced Battery Materials and Technologies · Advancements in Battery Materials · Advanced Battery Technologies Research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Chemistry, Graduate School of Science

Tohoku University

Changchun Institute of Applied Chemistry, Chinese Academy of Sciences (CAS)

Institute of Multidisciplinary Research for Advanced Materials

Funding

Strategic International Collaborative Research Program · Tohoku University · Japan Society for the Promotion of Science · Japan Science and Technology Agency

References (57)

Show source-provided references
1. 10.1038/3510464410.1038/35104644 ↗
2. 10.1002/adma.20180056110.1002/adma.201800561 ↗
3. 10.1039/C8TA10513H10.1039/C8TA10513H ↗
4. 10.1016/0079-6786(78)90003-110.1016/0079-6786(78)90003-1 ↗
5. 10.1021/cr500192f10.1021/cr500192f ↗
6. 10.1039/C6EE03367A10.1039/C6EE03367A ↗
7. 10.1149/1.212885910.1149/1.2128859 ↗
8. 10.1149/2.1441707jes10.1149/2.1441707jes ↗
9. 10.1149/1.240747010.1149/1.2407470 ↗
10. 10.1016/0022-0728(87)85045-310.1016/0022-0728(87)85045-3 ↗
11. 10.1016/S0378-7753(96)02555-410.1016/S0378-7753(96)02555-4 ↗
12. 10.1002/admi.20210125810.1002/admi.202101258 ↗
13. 10.1149/1.208685510.1149/1.2086855 ↗
14. 10.1149/1.183842010.1149/1.1838420 ↗
15. 10.1149/1.204865910.1149/1.2048659 ↗
16. 10.1149/1.183730010.1149/1.1837300 ↗
17. 10.1021/cr500003w10.1021/cr500003w ↗
18. 10.1002/adfm.20110085410.1002/adfm.201100854 ↗
19. 10.1016/S0013-4686(99)00276-510.1016/S0013-4686(99)00276-5 ↗
20. 10.1016/j.ensm.2021.07.00510.1016/j.ensm.2021.07.005 ↗
21. 10.1038/nmat348610.1038/nmat3486 ↗
22. 10.1016/j.elecom.2011.12.01910.1016/j.elecom.2011.12.019 ↗
23. 10.1039/c3cp43225d10.1039/c3cp43225d ↗
24. 10.1021/acs.jpcc.5b0918710.1021/acs.jpcc.5b09187 ↗
25. 10.1021/acs.jpcc.3c0272610.1021/acs.jpcc.3c02726 ↗
26. 10.1016/S0013-4686(01)00858-110.1016/S0013-4686(01)00858-1 ↗
27. 10.1149/1.302967410.1149/1.3029674 ↗
28. 10.1002/celc.20230070210.1002/celc.202300702 ↗
29. 10.1039/D1SC04265C10.1039/D1SC04265C ↗
30. 10.3866/PKU.WHXB20200705810.3866/PKU.WHXB202007058 ↗
31. 10.1016/j.electacta.2018.02.15110.1016/j.electacta.2018.02.151 ↗
32. 10.1002/adfm.20160598910.1002/adfm.201605989 ↗
33. 10.3390/batteries701000110.3390/batteries7010001 ↗
34. 10.1002/celc.20160036510.1002/celc.201600365 ↗
35. 10.1021/nl400998t10.1021/nl400998t ↗
36. 10.1021/ja310347x10.1021/ja310347x ↗
37. 10.1039/c2cc32730a10.1039/c2cc32730a ↗
38. 10.1016/j.jelechem.2017.06.00210.1016/j.jelechem.2017.06.002 ↗
39. 10.1149/2.0191510jes10.1149/2.0191510jes ↗
40. 10.1149/2.013404jes10.1149/2.013404jes ↗
41. 10.1149/1.135731610.1149/1.1357316 ↗
42. 10.1039/c0jm04309e10.1039/c0jm04309e ↗
43. 10.1149/1.214215710.1149/1.2142157 ↗
44. 10.1021/jp052474w10.1021/jp052474w ↗
45. 10.1149/1.178579510.1149/1.1785795 ↗
46. 10.1063/1.167475410.1063/1.1674754 ↗
47. 10.1021/acs.chemmater.6b0340310.1021/acs.chemmater.6b03403 ↗
48. 10.1021/acs.jpcc.4c0092710.1021/acs.jpcc.4c00927 ↗
49. 10.1021/acs.jpclett.8b0126110.1021/acs.jpclett.8b01261 ↗
50. 10.1149/1.296994710.1149/1.2969947 ↗
51. 10.1039/C7CP01928A10.1039/C7CP01928A ↗
52. 10.1039/C9EE01453E10.1039/C9EE01453E ↗
53. 10.1002/anie.20180472610.1002/anie.201804726 ↗
54. 10.1021/ja202174710.1021/ja2021747 ↗
55. 10.1021/cm300563410.1021/cm3005634 ↗
56. 10.1149/2.0731412jes10.1149/2.0731412jes ↗
57. 10.1039/C6RA09560G10.1039/C6RA09560G ↗