journal article·2013-06-11

Controlling Electrostatic Charging of Nanocrystalline Diamond at Nanoscale

Elisseos Verveniotis, Alexander Kromka, Bohuslav Rezek

Langmuir· Volume 29· Issue 23
Publisher page

Abstract

Constant electrical current in the range of -1 to -200 pA is applied by an atomic force microscope (AFM) in contact mode regime to induce and study local electrostatic charging of oxygen-terminated nanocrystalline diamond (NCD) thin films. The NCD films are deposited on silicon in 70 nm thickness and with 60% relative sp(2) phase content. Charging current is monitored by conductive AFM. Electric potential contrast induced by the current is evaluated by Kelvin force microscopy (KFM). KFM shows well-defined, homogeneous, and reproducible microscopic patterns that are not influenced by inherent tip-surface junction fluctuations during the charging process. The charged patterns are persistent for at least 72 h due to charge trapping inside the NCD film. The current-induced charging also clearly reveals field-induced detrapping at current amplitudes >-50 pA and tip instability at >-150 pA, both of which limit the achievable potential contrast. In addition, we show that the field also determines the range of electronic states that can trap the charge. We present a model and discuss implications for control of the nanoscale charging process.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Diamond and Carbon-based Materials Research · Force Microscopy Techniques and Applications · Advanced Surface Polishing Techniques

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Institute of Physics ASCR, Cukrovarnicka 10, Prague 6, 16253, Czech Republic

References (20)

Show source-provided references
1. Kawarada H. · Surf. Sci. Rep. · 1996 · 26 · 208
2. Takeuchi D. · J. Appl. Phys. · 2006 · 99 · 08610210.1063/1.2188070 ↗
3. Piantanida G. · J. Appl. Phys. · 2001 · 89 · 825910.1063/1.1368395 ↗
4. Bergonzo P. · Semicond. Sci. Technol. · 2003 · 18 · S10510.1088/0268-1242/18/3/315 ↗
5. Koide Y. · Diamond Relat. Mater. · 2006 · 15 · 196210.1016/j.diamond.2006.08.009 ↗
6. Stallhofer M. · Appl. Phys. Lett. · 2010 · 97 · 11110710.1063/1.3487785 ↗
7. Sumikawa Y. · Appl. Phys. Lett. · 2004 · 85 · 13910.1063/1.1767272 ↗
8. Stehlik Š. · Langmuir · 2013 · 29 · 163410.1021/la304472w ↗
9. Sadewasser S. · 2012 · 710.1007/978-3-642-22566-6_2 ↗
10. Melitz W. · Surf. Sci. Rep. · 2011 · 66 · 110.1016/j.surfrep.2010.10.001 ↗
11. Verveniotis E. · Phys. Status Solidi B · 2009 · 246 · 279810.1002/pssb.200982305 ↗
12. Čermák J. · Phys. Status Solidi A · 2008 · 205 · 213610.1002/pssa.200879712 ↗
13. Verveniotis E. · Phys. Status Solidi A · 2010 · 207 · 279810.1002/pssa.201000014 ↗
14. Verveniotis E. · Nanoscale Res. Lett. · 2011 · 6 · 14410.1186/1556-276X-6-144 ↗
15. Verveniotis E. · Diamond Relat. Mater. · 2012 · 24 · 3910.1016/j.diamond.2011.10.002 ↗
16. Ghodbane S. · Langmuir · 2010 · 26 · 1879810.1021/la1032652 ↗
17. Nonnenmacher M. · Appl. Phys. Lett. · 1991 · 292110.1063/1.105227 ↗
18. Zhang Y. · Langmuir · 2010 · 26 · 1195810.1021/la101290r ↗
19. Charlier J.-C. · Phys. Rev. B · 1992 · 46 · 454010.1103/PhysRevB.46.4540 ↗
20. Rogalla M. · Nucl. Instrum. Methods, A · 1997 · 395 · 4910.1016/S0168-9002(97)00632-3 ↗