journal article·2009-05-05

Influence of Superheated Water on the Hydrogen Bonding and Crystallography of Piperazine-Based (Co)polyamides

Esther Vinken, Ann E. Terry, Anne B. Spoelstra, Cor E. Koning, Sanjay Rastogi

Langmuir· Volume 25· Issue 9
Publisher page

Abstract

Here we demonstrate that superheated water is a solvent for polyamide 2,14 and piperazine-based copolyamides up to a piperazine content of 62 mol %. The incorporation of piperazine allows for a variation of the hydrogen bond density without altering the crystal structure (i.e., the piperazine units cocrystallize with the PA2,14 units (Hoffmann, S.; Vanhaecht, B.; Devroede, J.; Bras, W.; Koning, C. E.; Rastogi, S. Macromolecules 2005, 38, 1797-1803). It is shown that the crystallization of PA2,14 from superheated water greatly influences the crystal structure. Water molecules incorporated in the PA2,14 crystal lattice cause a slip on the hydrogen bonded planes, resulting in a coexistence of a triclinic and a monoclinic crystal structure. On heating above the Brill transition, the water molecules exit from the lattice, restoring the triclinic crystal structure. With increasing piperazine content, and hence decreasing hydrogen bond density, the dissolution temperature decreases. It is only possible to grow single crystals from superheated water up to a piperazine content of 62 mol %. For these single crystals, the incorporation of water molecules in the vicinity of the amide group is seen by the presence of COO- stretch vibrations with FTIR spectroscopy. These vibrations disappear on heating above the Brill transition temperature, and the water molecules leave the amide groups. For copolyamides with more than 62 mol % piperazine, no Brill transition is observed, no single crystals can be grown from water, and no water molecules are observed in the vicinity of the amide groups (Vinken, E.; Terry, A. E.; Hoffmann, S.; Vanhaecht, B.; Koning, C. E.; Rastogi, S. Macromolecules 2006, 39, 2546-2552). The high piperazine content (co)polyamides have fewer hydrogen bond donors and are therefore less likely to have interactions with the water molecules. This work demonstrates the relation among the Brill transition, the dissolution of polyamide in superheated water, and its influence on the hydrogen bonds and the amide groups.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Thermal and Kinetic Analysis · Synthesis and properties of polymers · Epoxy Resin Curing Processes

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Laboratory of Polymer Technology, Department of Chemical Engineering

Dutch Polymer Institute (DPI), P.O. Box 902, 5600AX Eindhoven, The Netherlands

ISIS Facility, Rutherford Appleton Laboratory, Chilton, Didcot, Oxfordshire, OX11 0QX, U.K.

Laboratory of Polymer Chemistry, Department of Chemical Engineering

Physical and Colloid Chemistry, Free University of Brussels, Pleinlaan 2, 1050 Brussels, Belgium

Department of Materials, Loughborough University, Loughborough LE11 3TU, United Kingdom

References (32)

Show source-provided references
1. Hoffmann S. · Macromolecules · 2005 · 38 · 179710.1021/ma048456e ↗
2. Vinken E. · Macromolecules · 2006 · 39 · 254610.1021/ma0526903 ↗
3. Ehrenstein M. · Polymer · 2000 · 41 · 353110.1016/S0032-3861(99)00590-X ↗
4. Brydson J. · 1999
5. Vanhaecht B. · J. Polym. Sci., Part A: Polym. Chem. · 2003 · 41 · 208210.1002/pola.10751 ↗
6. Brill R. · J. Prakt. Chem. · 1942 · 161 · 4910.1002/prac.19421610104 ↗
7. Jones N. A. · Macromolecules · 2000 · 33 · 264210.1021/ma9919559 ↗
8. Rastogi S. · Macromolecules · 2004 · 37 · 882510.1021/ma0483423 ↗
9. Vinken E. · Langmuir · 2008 · 24 · 631310.1021/la800378c ↗
10. Sweeny W. · 1969 · 10
11. Vinken, E.Polyamides: Hydrogen Bonding, the Brill Transition, and Superheated Water. Ph.D. Thesis,Eindhoven University of Technology, Eindhoven, The Netherlands, 2008.
12. Kvick A. · Nucl. Instrum. Methods Phys. Res. B. · 2003 · 199 · 53110.1016/S0168-583X(02)01395-2 ↗
13. Urban V. · J. Appl. Crystallogr. · 2003 · 36 · 80910.1107/S0021889803000554 ↗
14. Wevers M. G. M. · Therm. Acta · 2007 · 453 · 6710.1016/j.tca.2006.10.020 ↗
15. Kilburn D. · Nat. Mater. · 2006 · 5 · 63210.1038/nmat1681 ↗
16. Dill K. A. · Annu. Rev. Biophys. Biomol. Struct. · 2005 · 34 · 17310.1146/annurev.biophys.34.040204.144517 ↗
17. Li Y. · J. Polym. Sci., B: Polym. Phys. · 2002 · 40 · 191310.1002/polb.10251 ↗
18. Jones N. A. · J. Polym. Sci., B: Polym. Phys. · 1997 · 35 · 67510.1002/(SICI)1099-0488(199703)35:4<675::AID-POLB14>3.0.CO;2-D ↗
19. Kraus W. · J. Appl. Crystallogr. · 1996 · 29 · 30110.1107/S0021889895014920 ↗
20. Bunn C. W. · Proc. Roy. Soc. · 1947 · 189 · 39
21. Rotter G. · J. Polym. Sci.: Part B Polym. Phys. · 1992 · 30 · 48910.1002/polb.1992.090300508 ↗
22. Lin-Vien D. · 1991
23. Harings J. A. W. · Cryst. Growth Des. · 2008 · 8 · 246910.1021/cg8001064 ↗
24. Harings J. A. W. · Cryst. Growth Des. · 2008 · 8 · 332310.1021/cg8002405 ↗
25. Cannon C. G. · Spectrochim. Acta · 1960 · 16 · 30210.1016/0371-1951(60)80092-6 ↗
26. Cui X. · J. Polym. Sci., Part B: Polym. Phys. · 2004 · 42 · 401710.1002/polb.20266 ↗
27. Vasanthan N. · Macromolecules · 1998 · 31 · 843310.1021/ma980935o ↗
28. Cooper S. J. · Polymer · 2001 · 42 · 1011910.1016/S0032-3861(01)00566-3 ↗
29. Jakes J. · Spectrochim. Acta · 1971 · 27 · 1910.1016/0584-8539(71)80004-1 ↗
30. Yoshioka Y. · J. Phys. Chem. · 2003 · 107 · 1183510.1021/jp0224160 ↗
31. Yoshioka Y. · Polymer · 2003 · 44 · 640710.1016/S0032-3861(03)00593-7 ↗
32. Atkins E. D. T. · Macromolecules · 1992 · 25 · 91710.1021/ma00028a063 ↗