Source abstract
Abstract
Potassium-ion batteries have emerged as promising next-generation energy storage systems because of the abundance and low cost of potassium. However, achieving high capacity and long-term cycling stability remains challenging, especially for metal/alloy anodes such as antimony (Sb), which suffers from considerable volume changes during charge–discharge cycling. To address this challenge, herein, composite anodes were prepared by combining Sb with rare earth antimonides ( RE Sb x, RE = Y, La, Ce, Sm, or Gd), which are known for their charge–discharge cycling stability. The electrochemical performances of RE Sb x /Sb composite electrodes were systematically evaluated in an ionic liquid electrolyte. Charge–discharge testing revealed that RE Sb x addition, even at 10 wt %, considerably suppressed the rapid capacity fading observed in pure Sb electrodes, leading to excellent cycling stability. Additionally, pure Sb made the highest contribution to the capacity of the composite electrodes, and RE Sb x effectively suppressed electrode degradation. Specifically, the cycle life of the CeSb/Sb electrode was over three times longer than that of the pure Sb electrode. Cross-sectional scanning electron microscopy demonstrated that the RE Sb x phase mitigated electrode expansion and cracking. Further investigation showed that the high K + diffusion coefficient of CeSb, larger lattice parameters of CeSb, and mechanical softness (lower breaking strength) of CeSb played key roles in increasing the cycle life of the CeSb/Sb electrode. These properties facilitated uniform K + distribution and reduced mechanical stress in the CeSb/Sb electrode. Our findings help advance high-performance, resource-efficient energy storage technologies.
Source: openalex_inverted_index · Quality: baseline
Affiliations
Department of Chemistry and Biotechnology, Graduate School of Engineering, Tottori University, Minami 4−101, Koyama−cho, Tottori 680−8552, Japan
Center for Research on Green Sustainable Chemistry, Tottori University, Minami 4−101, Koyama−cho, Tottori 680−8552, Japan
Course of Chemistry and Biotechnology, Department of Engineering, Graduate School of Sustainability Science, Tottori University, Minami 4−101, Koyama−cho, Tottori 680−8552, Japan
Institute of Advanced Energy
Kyoto University
International Center of Young Scientists, National Institute for Materials Science, 1−1 Namiki, Tsukuba 305−0044, Japan
Funding
Institute of Advanced Energy, Kyoto University · National Institute for Materials Science