journal article·2026-06-08

Enhancing Proton Conductivity and Structural Stability of CsH 2 PO 4 Composites with Acid-Treated Zeolite as Solid Acid Electrolyte Materials

Sanghwa Jeong, Jungseub Ha, Sehun Choi, Junbeom Maeng, Won Bae Kim

Publisher page

Abstract

Solid acid electrochemical cells operating at intermediate temperatures are promising for efficient hydrogen-energy conversion, but their practical application is limited by the dehydration-driven degradation of CsH 2 PO 4 (CDP), a representative solid acid electrolyte. In this study, a composite electrolyte based on CDP and phosphoric acid-treated ZSM-5 (ZSM-5(A)) is developed to improve proton-conduction behavior and dehydration tolerance under humidified intermediate-temperature conditions. Structural and spectroscopic analyses indicate that phosphoric acid treatment introduces phosphate-derived local chemical environments into the zeolite while preserving the ZSM-5 framework, thereby altering the interfacial environment surrounding the CDP phase. Proton-conductivity measurements show that CDP/ZSM-5(A) exhibits higher conductivity than pristine CDP and CDP/ZSM-5, including enhanced conductivity below the superprotonic transition with an earlier onset of the conductivity increase, approaching 10 −2 S cm −1 at intermediate temperatures. Under humidified operation at 250 °C, pristine CDP and CDP/ZSM-5 show rapid conductivity decay, whereas CDP/ZSM-5(A) maintains substantially more stable proton-conduction behavior over 50 h. Correlated FT-IR, XPS, temperature-resolved XRD, and SEM analyses further indicate that the acid-treated composite undergoes less severe dehydration-associated chemical and structural changes, while preserving a more continuous pellet microstructure. These results support the role of ZSM-5(A) as a phosphoric acid-treated interfacial component in a CDP-dominated proton-conduction network and identify CDP/ZSM-5(A) as a phosphate-modified composite electrolyte for durable intermediate-temperature electrochemical energy systems.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Advanced Battery Materials and Technologies · Thermal Expansion and Ionic Conductivity · Solid-state spectroscopy and crystallography

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Battery Engineering, Graduate Institute of Ferrous and Eco Materials Technology (GIFT), Pohang University of Science and Technology (POSTECH), 77 Cheongam-ro, Nam-gu, Pohang-si, Gyeongsangbuk-do 37673, Republic of Korea

Department of Chemical Engineering, Pohang University of Science and Technology (POSTECH), 77 Cheongam-ro, Nam-gu, Pohang-si, Gyeongsangbuk-do 37673, Republic of Korea

Funding

National Research Foundation of Korea · Korea Institute for Advancement of Technology

References (54)

Show source-provided references
1. 10.1016/j.ijhydene.2019.04.06810.1016/j.ijhydene.2019.04.068 ↗
2. 10.1016/j.ijhydene.2024.10.35010.1016/j.ijhydene.2024.10.350 ↗
3. 10.1038/s41929-020-0455-810.1038/s41929-020-0455-8 ↗
4. 10.1016/j.enpol.2008.09.03610.1016/j.enpol.2008.09.036 ↗
5. 10.1021/acs.chemrev.3c0090410.1021/acs.chemrev.3c00904 ↗
6. 10.1016/j.ijhydene.2016.06.21110.1016/j.ijhydene.2016.06.211 ↗
7. 10.1002/aesr.20240013210.1002/aesr.202400132 ↗
8. 10.1039/D3QI01557B10.1039/D3QI01557B ↗
9. 10.1016/j.rser.2022.11283610.1016/j.rser.2022.112836 ↗
10. 10.1016/j.joule.2020.10.00610.1016/j.joule.2020.10.006 ↗
11. 10.3390/catal1304070710.3390/catal13040707 ↗
12. 10.1016/j.jpowsour.2025.23854010.1016/j.jpowsour.2025.238540 ↗
13. 10.1149/2.F06093IF10.1149/2.F06093IF ↗
14. 10.1039/D4EE01219D10.1039/D4EE01219D ↗
15. 10.1038/3507353610.1038/35073536 ↗
16. 10.1126/science.109092010.1126/science.1090920 ↗
17. 10.1039/b704558c10.1039/b704558c ↗
18. 10.1021/cm020138b10.1021/cm020138b ↗
19. 10.1007/s11581-020-03867-010.1007/s11581-020-03867-0 ↗
20. 10.1039/D4YA00606B10.1039/D4YA00606B ↗
21. 10.1016/j.electacta.2008.06.01810.1016/j.electacta.2008.06.018 ↗
22. 10.1016/j.sajce.2021.06.00610.1016/j.sajce.2021.06.006 ↗
23. 10.1007/s42452-020-04097-910.1007/s42452-020-04097-9 ↗
24. 10.1134/s002016851410012410.1134/s0020168514100124 ↗
25. 10.1016/j.matpr.2019.02.20510.1016/j.matpr.2019.02.205 ↗
26. 10.3390/membranes1307061710.3390/membranes13070617 ↗
27. 10.1016/j.jpowsour.2008.01.00310.1016/j.jpowsour.2008.01.003 ↗
28. 10.1016/j.ssi.2007.09.00510.1016/j.ssi.2007.09.005 ↗
29. 10.1039/C8SE00054A10.1039/C8SE00054A ↗
30. 10.1002/adfm.20251848210.1002/adfm.202518482 ↗
31. 10.1016/j.nanoen.2025.11098010.1016/j.nanoen.2025.110980 ↗
32. 10.1016/j.scitotenv.2024.17109910.1016/j.scitotenv.2024.171099 ↗
33. 10.1016/j.ssi.2011.09.01810.1016/j.ssi.2011.09.018 ↗
34. 10.1038/s41467-021-22936-010.1038/s41467-021-22936-0 ↗
35. 10.1039/d3cs00404j10.1039/d3cs00404j ↗
36. 10.1016/j.cattod.2018.02.05410.1016/j.cattod.2018.02.054 ↗
37. 10.1021/acs.jpcc.3c0361110.1021/acs.jpcc.3c03611 ↗
38. 10.1016/j.apcata.2006.08.01610.1016/j.apcata.2006.08.016 ↗
39. 10.1021/acs.chemmater.0c0341110.1021/acs.chemmater.0c03411 ↗
40. 10.1016/j.jpowsour.2024.23490810.1016/j.jpowsour.2024.234908 ↗
41. 10.1039/D1RA03847H10.1039/D1RA03847H ↗
42. 10.1016/j.cej.2022.14004010.1016/j.cej.2022.140040 ↗
43. 10.3390/app922489710.3390/app9224897 ↗
44. 10.1039/D5RA01413A10.1039/D5RA01413A ↗
45. 10.3390/catal706017110.3390/catal7060171 ↗
46. 10.1016/j.jpowsour.2008.10.08810.1016/j.jpowsour.2008.10.088 ↗
47. 10.1039/C9RA08738A10.1039/C9RA08738A ↗
48. 10.1039/D1MA00612F10.1039/D1MA00612F ↗
49. 10.1016/j.saa.2025.12660310.1016/j.saa.2025.126603 ↗
50. 10.1016/j.joule.2021.05.01610.1016/j.joule.2021.05.016 ↗
51. 10.1021/jp712049c10.1021/jp712049c ↗
52. 10.1016/j.polymer.2007.09.05010.1016/j.polymer.2007.09.050 ↗
53. 10.1063/1.280477410.1063/1.2804774 ↗
54. 10.1021/la960756510.1021/la9607565 ↗