journal article·2009-10-28

Graphite Oxide Flame-Retardant Polymer Nanocomposites

Amanda L. Higginbotham, Jay R. Lomeda, Alexander B. Morgan, James M. Tour

Publisher page

Abstract

Graphite oxide (GO) polymer nanocomposites were developed at 1, 5, and 10 wt % GO with polycarbonate (PC), acrylonitrile butadiene styrene, and high-impact polystyrene for the purpose of evaluating the flammability reduction and material properties of the resulting systems. The overall morphology and dispersion of GO within the polymer nanocomposites were studied by scanning electron microscopy and optical microscopy; GO was found to be well-dispersed throughout the matrix without the formation of large aggregates. Mechanical testing was performed using dynamic mechanical analysis to measure the storage modulus, which increased for all polymer systems with increased GO loading. Microscale oxygen consumption calorimetry revealed that the addition of GO reduced the total heat release and peak heat release rates in all systems, and GO-PC composites demonstrated very fast self-extinguishing times in vertical open flame tests, which are important to some regulatory fire safety applications.
Source: openalex_inverted_index · Quality: baseline

Research context

OpenAlex topics: Flame retardant materials and properties · Polymer Nanocomposites and Properties · Fire dynamics and safety research

SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.

Affiliations

Department of Chemistry, Rice University, 6100 Main Street, MS 222, Houston, Texas 77005, and Multiscale Composites and Polymers Division, University of Dayton Research Institute, 300 College Park, Dayton, Ohio 45469-0160

References (36)

Show source-provided references
1. Beyer, G.InFlame Retardant Polymer Nanocomposites;Morgan, A. B. and Wilkie, C. A., Eds.John Wiley & Sons, Inc.:Hoboken, NJ, 2007; pp163−190.
2. Blomqvist P. · Fire Technol. · 2004 · 40 · 3910.1023/B:FIRE.0000003315.47815.cb ↗
3. Blomqvist P. · Fire Technol. · 2004 · 40 · 5910.1023/B:FIRE.0000003316.63475.16 ↗
4. Levchik S. V. · J. Fire Sci. · 2006 · 24 · 34510.1177/0734904106068426 ↗
5. Vaia R. A. · Chem. Mater. · 2007 · 19 · 273610.1021/cm062693+ ↗
6. Paul D. R. · Polymer · 2008 · 49 · 318710.1016/j.polymer.2008.04.017 ↗
7. Winey K. I. · MRS Bull. · 2007 · 32 · 31410.1557/mrs2007.229 ↗
8. Bredeau S. · Polym. Int. · 2008 · 57 · 54710.1002/pi.2375 ↗
9. Jang B. Z. · J. Mater. Sci. · 2008 · 43 · 509210.1007/s10853-008-2755-2 ↗
10. Modesti M. · Polym. Degrad. Stab. · 2002 · 77 · 19510.1016/S0141-3910(02)00034-4 ↗
11. Shi L. · Polym. Int. · 2006 · 55 · 86210.1002/pi.2021 ↗
12. Kashiwagi T. · Nat. Mater. · 2005 · 4 · 92810.1038/nmat1502 ↗
13. Kashiwagi T. · Polymer · 2005 · 46 · 47110.1016/j.polymer.2004.10.087 ↗
14. Song P. a. · J. Mater. Chem. · 2008 · 18 · 508310.1039/b808309f ↗
15. Wang J. Q. · Polym. Adv. Technol. · 2006 · 17 · 33510.1002/pat.698 ↗
16. Dasari A. · Polymer · 2009 · 50 · 157710.1016/j.polymer.2009.01.050 ↗
17. Lerf A. · J. Phys. Chem. B · 1998 · 102 · 447710.1021/jp9731821 ↗
18. Steurer P. · Macromol. Rapid Commun. · 2009 · 30 · 31610.1002/marc.200800754 ↗
19. McAllister M. J. · Chem. Mater. · 2007 · 19 · 439610.1021/cm0630800 ↗
20. Zhang R. · Polym. Degrad. Stab. · 2004 · 85 · 58310.1016/j.polymdegradstab.2004.01.020 ↗
21. Zhang R. · Macromol. Mater. Eng. · 2004 · 289 · 35510.1002/mame.200300264 ↗
22. Wang, J. Q. and Han, Z. D.InFire and Polymers IV: Materials and Concepts for Hazard Prevention;Wilkie, C. A. and Nelson, G. L., Eds.American Chemical Society:Washington, DC, 2005; Vol. 922, pp172−184.
23. Uhl F. M. · Polym. Degrad. Stab. · 2004 · 84 · 21510.1016/j.polymdegradstab.2003.10.014 ↗
24. Staudenmaier L. · Ber. Dtsch. Chem. Ges. · 1898 · 31 · 148110.1002/cber.18980310237 ↗
25. Lyon R. E. · Polymer · 2009 · 50 · 260810.1016/j.polymer.2009.03.047 ↗
26. Morgan A. B. · Polym. Adv. Technol. · 2008 · 19 · 53010.1002/pat.1100 ↗
27. Lyon R. E. · J. Anal. Appl. Pyrolysis · 2004 · 71 · 2710.1016/S0165-2370(03)00096-2 ↗
28. Grause G. · Polym. Degrad. Stab. · 2009 · 94 · 111910.1016/j.polymdegradstab.2009.03.014 ↗
29. Levchik S. V. · Polym. Int. · 2005 · 54 · 98110.1002/pi.1806 ↗
30. Levchik S. V. · J. Fire Sci. · 2006 · 24 · 13710.1177/0734904106055997 ↗
31. Morgan A. B. · Polym. Adv. Technol. · 2006 · 17 · 20610.1002/pat.685 ↗
32. Costache M. C. · Polymer · 2007 · 48 · 653210.1016/j.polymer.2007.08.059 ↗
33. 1996
34. Bourbigot S. · Mol. Cryst. Liq. Cryst. · 2008 · 486 · 32510.1080/15421400801921983 ↗
35. Morgan A. B. · Fire Mater. · 2007 · 31 · 25710.1002/fam.937 ↗
36. Kashiwagi, T.InFlame Retardant Polymer Nanocomposites;Morgan, A. B. and Wilkie, C. A., Eds.John Wiley & Sons, Inc.:Hoboken, NJ, 2007; pp285−324.