Surface integrity study of WEDM with various wire electrodes: experiments and analysis
Source abstract
Abstract
Wire electrical discharge machining (WEDM) is always significant for its high-precision machining. However, due to the generation of high discharge energy during machining, machined surfaces are often got distorted. These might be upgraded by choosing the correct tool with proper machining condition. The effects of the electrode materials and process parameters on different responses of WEDM like average surface roughness, recast layer thickness, and surface morphology are systematically examined here to enhance the knowledge of WEDM and its correlation with electrode property. The experiments have been carried out on one of the expensive steel namely Maraging steel 300 due to its applicability in tooling and aerospace industries. Plain brass wire, zinc-coated brass wire (ZCB), and silver-coated brass (SCB) wires are used as a tool electrode for analysis. Comparative experimental studies prove that among BW, ZCB, and SCB, the overall performance of SCB is commendable owing to the high-quality surface considering control parameters in low discharge energy level. However, the second-best performance is shown by ZCB.
Source: openalex_inverted_index · Quality: baseline
Research context
OpenAlex topics: Advanced Machining and Optimization Techniques · Advanced Surface Polishing Techniques · Advanced machining processes and optimization
SciVX discovery tags are terminology-based. OpenAlex topics are source-provided classifications.
Affiliations
Mechanical Engineering Department, National Institute of Technology, Agartala, India;
Mechanical Engineering Department, Institute of Engineering and Management, Kolkata, India
References (22)
Show source-provided references
1. 10.1007/s00170-015-6797-810.1007/s00170-015-6797-8 ↗
2. 10.1007/s40430-015-0335-310.1007/s40430-015-0335-3 ↗
3. 10.1016/j.jmapro.2019.05.02610.1016/j.jmapro.2019.05.026 ↗
4. 10.1016/S0007-8506(07)62194-510.1016/S0007-8506(07)62194-5 ↗
5. 10.1016/j.jestch.2014.05.00210.1016/j.jestch.2014.05.002 ↗
6. 10.1080/10426914.2014.94186510.1080/10426914.2014.941865 ↗
7. 10.1016/S0890-6955(03)00162-710.1016/S0890-6955(03)00162-7 ↗
8. 10.1016/j.ijmachtools.2004.04.01710.1016/j.ijmachtools.2004.04.017 ↗
9. 10.1016/j.measurement.2019.04.07610.1016/j.measurement.2019.04.076 ↗
10. 10.1016/j.ijlmm.2019.09.00310.1016/j.ijlmm.2019.09.003 ↗
11. 10.1016/j.jmapro.2015.09.01110.1016/j.jmapro.2015.09.011 ↗
12. 10.1016/j.precisioneng.2015.01.00810.1016/j.precisioneng.2015.01.008 ↗
13. 10.1016/j.measurement.2017.09.04010.1016/j.measurement.2017.09.040 ↗
14. 10.1016/j.measurement.2017.11.05310.1016/j.measurement.2017.11.053 ↗
15. 10.1016/j.heliyon.2019.e0147310.1016/j.heliyon.2019.e01473 ↗
16. 10.1007/s00170-014-6445-810.1007/s00170-014-6445-8 ↗
17. 10.1016/j.apsusc.2014.09.07410.1016/j.apsusc.2014.09.074 ↗
18. 10.1016/j.mechrescom.2003.09.00610.1016/j.mechrescom.2003.09.006 ↗
19. 10.1016/j.matdes.2015.09.03610.1016/j.matdes.2015.09.036 ↗
20. 10.1007/s12541-013-0279-410.1007/s12541-013-0279-4 ↗
21. 10.1016/j.precisioneng.2014.10.00110.1016/j.precisioneng.2014.10.001 ↗
22. 10.1016/j.jmatprotec.2004.04.37310.1016/j.jmatprotec.2004.04.373 ↗